Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 10.0 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
CTE, linear 18.0 µm/m-°C

@Temperature 20.0 °C
10.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Covestro Petlon® 7530 Semi-Crystalline PET, 35% Mineral/Glass Fiber  (discontinued **)
Characteristics: Excellent Electrical Properties, High Heat and Chemical ResistanceApplications: Automotive (Under Hood), Appliances, Casings and HousingsProcessing: Injection Molding (Melt Temperat..
CTE, linear 18.0 µm/m-°C
10.0 µin/in-°F
MD, below Tg; ASTM D696
Victrex® APTIV® 1103-050 Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, Mineral Filled  (Unve
Description: APTIV® 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance a..
CTE, linear 18.0 µm/m-°C

@Temperature 20.0 °C
10.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Solvay Specialty Polymers Ixef® 1501/0003 Polyarylamide, 30% Glass Fiber, DAM  (discontinued **)
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
CTE, linear 18.0 µm/m-°C

@Temperature 20.0 °C
10.0 µin/in-°F

@Temperature 68.0 °F
Cookson Group Plaskon® 1002 Conventional Encapsulant  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.A low cost, low stress, conventional molding compound recommended for high volume commodity-type packages that house simple linea..
CTE, linear 18.0 µm/m-°C

@Temperature 20.0 - 200 °C
10.0 µin/in-°F

@Temperature 68.0 - 392 °F
Materion Beryllium Copper Alloy 10 Rod and Bar; HT (TH04) Temper; up to 76 mm (UNS C17500)
Treatment required for max strength: 2 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In..
CTE, linear 18.0 µm/m-°C

@Temperature 20.0 - 200 °C
10.0 µin/in-°F

@Temperature 68.0 - 392 °F
Materion Beryllium Copper Alloy 10 Wire; A (TB00) Temper; 1.3-12.7 mm Diameter (UNS C17500)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
CTE, linear 18.0 µm/m-°C

@Temperature 20.0 - 200 °C
10.0 µin/in-°F

@Temperature 68.0 - 392 °F
Materion Beryllium Copper Alloy 10C Castings (UNS C82000)
Pouring Temperature: 1095-1175°CHeat treatment required for max strength (Annealing): 870-900°C/water quenchHeat treatment required for max strength (Hardening): 870-900°C/water quenchTabul..
CTE, linear 18.0 µm/m-°C

@Temperature 20.0 - 200 °C
10.0 µin/in-°F

@Temperature 68.0 - 392 °F
Materion Beryllium Copper Alloy 3 Plate & Rolled Bar; HT (TH04) Temper; up to 76 mm Thickness (UNS C17510)
Treatment required for max strength: 2 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In..
CTE, linear 18.0 µm/m-°C

@Temperature 20.0 - 200 °C
10.0 µin/in-°F

@Temperature 68.0 - 392 °F
Materion Beryllium Copper Alloy 3 Rod and Bar; A (TB00) Temper; All Sizes (UNS C17510)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
CTE, linear 18.0 µm/m-°C

@Temperature 20.0 - 200 °C
10.0 µin/in-°F

@Temperature 68.0 - 392 °F
Materion Beryllium Copper Alloy 3 Rod and Bar; HT (TH04) Temper; up to 76 mm (UNS C17510)
Treatment required for max strength: 2 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In..
CTE, linear 18.0 µm/m-°C

@Temperature 21.1 - 204 °C
10.0 µin/in-°F

@Temperature 70.0 - 400 °F
Materion BrushCAST® 165C High Strength Casting Alloy (As Cast & Aged)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
CTE, linear 18.0 µm/m-°C

@Temperature 21.1 - 204 °C
10.0 µin/in-°F

@Temperature 70.0 - 400 °F
Materion BrushCAST® 20C High Strength Casting Alloy (As Cast & Aged)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
CTE, linear 18.0 µm/m-°C

@Temperature 21.1 - 204 °C
10.0 µin/in-°F

@Temperature 70.0 - 400 °F
Materion BrushCAST® 275C High Strength Casting Alloy (As Cast & Aged)
Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri..
CTE, linear 18.0 µm/m-°C

@Temperature 21.1 - 204 °C
10.0 µin/in-°F

@Temperature 70.0 - 400 °F
Materion BrushCAST® 3C High Conductivity Casting Alloy (As Cast)
Pouring Temperature: 1095-1175°CHeat treatment required for max strength (Annealing): 870-900°C/water quenchHeat treatment required for max strength (Hardening): 870-900°C/water quenchDescr..
CTE, linear 18.0 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
10.0 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis; IPC-TM 650-2.4.24
Industrial Laminates/Norplex NP329 Cotton Fabric
Description: Bleached linen with melamine resin system. Provides better arc resistance than NP320E. Also, resistant to ammonia based refrigerants. Hard, durable material should be heated to punch, ..
CTE, linear 18.0 µm/m-°C
10.0 µin/in-°F
DIN 53752
Lehmann & Voss LUVOCOM® 1/CF/20/TF/5 Polyamide 66, with carbon fiber and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh..
CTE, linear 18.0 µm/m-°C

@Temperature 20.0 - 200 °C
10.0 µin/in-°F

@Temperature 68.0 - 392 °F
Materion Brush 1915â„¢ AT Temper Wire
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°CBrush 1915™ is Brush Wellman's new heat-treatable leaded copper alloy. Enginee..
CTE, linear 18.0 - 21.6 µm/m-°C

@Temperature 20.0 °C
10.0 - 12.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Techmer ES Electrafil® J-1200/CF/40 NAT ABS
CTE, linear 18.0 µm/m-°C

@Temperature 20.0 - 200 °C
10.0 µin/in-°F

@Temperature 68.0 - 392 °F
ASTM D233
UBE UPILEX VT Polyimide Film
Description: UPILEX, the ultra-high heat-resistant polyimide film, is the product of the polycondensation reaction between biphenyltetracarboxylic dianhydride (BPDA), of which process Ube Industries..
CTE, linear 18.0 µm/m-°C

@Temperature 20.0 - 300 °C
10.0 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 210 Gilding Metal, 3/4 Hard
CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi..
CTE, linear 18.0 µm/m-°C

@Temperature 20.0 - 300 °C
10.0 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 7026 Copper Nickel, 1/2 Hard
7026 is a high performance alloy used in springs, terminals, elevated temperature interconnects and high reliability telecommunication components.Information provided by Eagle Brass Company
CTE, linear 18.0 µm/m-°C

@Temperature 20.0 - 300 °C
10.0 µin/in-°F

@Temperature 68.0 - 572 °F
Eagle Brass 7026 Copper Nickel, Annealed
7026 is a high performance alloy used in springs, terminals, elevated temperature interconnects and high reliability telecommunication components.Information provided by Eagle Brass Company
CTE, linear 18.0 µm/m-°C

@Temperature 20.0 °C
10.0 µin/in-°F

@Temperature 68.0 °F
DuPont™ Nomex® N301 Nomex® Aramid Staple Fiber
General NOMEX Information: Nomex® is a family of aromatic polyamide (aramid) fibers. This family consists of staple fibers, continuous filament yarns, paper, and spunlaced fabrics. Uses for stapl..
CTE, linear 18.0 µm/m-°C

@Temperature 20.0 - 50.0 °C
10.0 µin/in-°F

@Temperature 68.0 - 122 °F
DuPont Teijin Films Melinex® ST504 Polyester Film, 500 Gauge
Melinex® ST504 is a crystal clear, high gloss, heat stabilized polyester film. It can be overprinted with a wide range of solvent-based graphic inks and varnishes, silver conductive and dielectric ..
CTE, linear 18.0 µm/m-°C

@Temperature 20.0 - 50.0 °C
10.0 µin/in-°F

@Temperature 68.0 - 122 °F
DuPont Teijin Films Melinex® ST504 Polyester Film, 700 Gauge
Melinex® ST504 is a crystal clear, high gloss, heat stabilized polyester film. It can be overprinted with a wide range of solvent-based graphic inks and varnishes, silver conductive and dielectric ..
CTE, linear 18.0 µm/m-°C
10.0 µin/in-°F
CLAL-MSX NICLAL 42 Copper Alloy
Description: Niclal 42 is a precision resistance alloy, with moderate Resistivity, low Temperature coefficient of resistance and low thermal EMF versus Copper. With high stability of electrical resi..
CTE, linear 18.0 µm/m-°C

@Temperature 100 °C
10.0 µin/in-°F

@Temperature 212 °F
CMW® ELKALOY D130 Copper Alloy, Aluminum Bronze
ELKALOY® D alloys are aluminum bronze type casting alloys. The sequence, ELKALOY® D, D110, D120, D130 materials represents increasing hardness and abrasion resistance but reduced electrical and th..
CTE, linear 18.0 µm/m-°C

@Temperature 20.0 - 200 °C
10.0 µin/in-°F

@Temperature 68.0 - 392 °F
Materion Beryllium Copper Alloy 3 Tube; AT (TF00) Temper; All Sizes (UNS C17510)
Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc...
Copyright © lookpolymers.com All Rights Reserved