| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 150 - 180 µm/m-°C @Temperature 20.0 °C |
83.3 - 100 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Solvay Specialty Polymers Solef® 21508 PVDF Copolymer
(discontinued **) Key features of this grade: High Elongation, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® P.. |
|||
| CTE, linear | 18.0 - 180 µm/m-°C | 10.0 - 100 µin/in-°F | Average value: 124 µm/m-°C Grade Count:18 |
| Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum.. |
|||
| CTE, linear | 19.8 - 180 µm/m-°C | 11.0 - 100 µin/in-°F | Average value: 68.4 µm/m-°C Grade Count:29 |
| Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum.. |
|||
| CTE, linear | 75.0 - 180 µm/m-°C @Temperature 60.0 - 60.0 °C |
41.7 - 100 µin/in-°F @Temperature 140 - 140 °F |
Average value: 159 µm/m-°C Grade Count:5 |
| Overview of materials for Epoxy Encapsulant, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Encapsulant, Unreinforced". Each property range of values reported is minimum and maximum values o.. |
|||
| CTE, linear | 98.0 - 180 µm/m-°C @Temperature >=27.0 °C |
54.4 - 100 µin/in-°F @Temperature >=80.6 °F |
Average value: 131 µm/m-°C Grade Count:9 |
| Overview of materials for Epoxy Cure Resin This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
| CTE, linear | 65.0 - 180 µm/m-°C | 36.1 - 100 µin/in-°F | Average value: 103 µm/m-°C Grade Count:13 |
| Overview of materials for Polytetrafluoroethylene (PTFE), Bronze Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Bronze Filled". Each property range of values reported is minimum and ma.. |
|||
| CTE, linear | 180 - 180 µm/m-°C @Temperature 50.0 - 160 °C |
100 - 100 µin/in-°F @Temperature 122 - 320 °F |
Average value: 180 µm/m-°C Grade Count:1 |
| Overview of materials for Nylon 612, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp.. |
|||
| CTE, linear | 100 - 180 µm/m-°C @Temperature 20.0 - 100 °C |
55.6 - 100 µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
| Schwartz Technical Plastics LAMIGAMID® 410 Cast Polyamide 6, Elastomer Modified, Low Temp, Dry Application: outrigger floats, rollersInformation provided by Schwartz Technical Plastics GmbH |
|||
| CTE, linear | 126 - 180 µm/m-°C @Temperature 20.0 °C |
70.0 - 100 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Zeus PTFE Tubing Zeus offers a wide range of standard size products and precision custom PTFE Tubing. PTFE Tubing has become the gold standard in industries requiring the ultimate in lubricity, high temperature use,.. |
|||
| CTE, linear | 72.0 - 180 µm/m-°C | 40.0 - 100 µin/in-°F | |
| TriStar Ultracomp UC-400 Composite Bearing Ultracomp UC-400 - Designed for high loads, low speeds, impact and vibration applications. UC-400 has a MOS2 additive for salt water applications where cathodic reactions could occur. Excellent dry .. |
|||
| CTE, linear | 150 - 180 µm/m-°C @Temperature 20.0 °C |
83.3 - 100 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Solvay Specialty Polymers Solef® 20810 PVDF Copolymer
(discontinued **) Key features of this grade: Li Battery, Virgin. Recommended processing is solution. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta.. |
|||
| CTE, linear | 144 - 180 µm/m-°C @Temperature 25.6 - 204 °C |
80.0 - 100 µin/in-°F @Temperature 78.0 - 400 °F |
ASTM D696 |
| Technetics Group Texolon™ 8534 PTFE
(Unverified Data**) PTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surface EnergyLow Dielectric ConstantHigh Volume and Surface ResistivityFlame ResistanceApp.. |
|||
| CTE, linear | 63.0 - 180 µm/m-°C | 35.0 - 100 µin/in-°F | Average value: 81.9 µm/m-°C Grade Count:62 |
| Overview of materials for Nylon 6, Cast This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||