| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear |
20.0
-
30.0
µm/m-°C @Temperature 50.0 - 100 °C |
11.1
-
16.7
µin/in-°F @Temperature 122 - 212 °F |
ISO 11359-2 |
|
Raschig Group AMPLA® 7250 melamine-modified polyester
Cellulose reinforced melamine-modified Polyester molding compound. Very good electrical values, excellent heat resistance, excellent surface quality, low post shrinkage. This product meets the allow..
|
|||
| CTE, linear |
20.0
µm/m-°C @Temperature 20.0 °C |
11.1
µin/in-°F @Temperature 68.0 °F |
TMA; ASTM E831 |
|
LNP Thermocomp® LF-1006 EM Polyetheretherketone, Glass Fiber Reinforcement
(discontinued **)
Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st..
|
|||
| CTE, linear | 20.0 - 42.2 µm/m-°C | 11.1 - 23.4 µin/in-°F | Average value: 33.6 µm/m-°C Grade Count:4 |
|
Overview of materials for Phenolic, Novolac, Impact Grade, Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Impact Grade, Filled". Each property range of values reported is minimum and maximum ..
|
|||
| CTE, linear | 20.0 µm/m-°C | 11.1 µin/in-°F | Average value: 20.0 µm/m-°C Grade Count:3 |
|
Overview of materials for Nylon 63, 35% Glass-Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 63, 35% Glass-Filled". Each property range of values reported is minimum and maximum values of app..
|
|||
| CTE, linear | 20.0 µm/m-°C | 11.1 µin/in-°F | DIN 53752 |
|
Lehmann & Voss LUVOCOM® 19-7319 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
|
|||
| CTE, linear | 20.0 µm/m-°C | 11.1 µin/in-°F | DIN 53752 |
|
Lehmann & Voss LUVOCOM® 19-7416 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
|
|||
| CTE, linear | 20.0 µm/m-°C | 11.1 µin/in-°F | DIN 53752 |
|
Lehmann & Voss LUVOCOM® 20-0665 Polyphthalamide, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
|
|||
| CTE, linear |
20.0
µm/m-°C @Temperature 20.0 °C |
11.1
µin/in-°F @Temperature 68.0 °F |
DIN 53752; ASTM D696 |
|
Kolon KOPA® KN333G33CR G/F Reinforced Nylon 66
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin..
|
|||
| CTE, linear | 20.0 µm/m-°C | 11.1 µin/in-°F | ASTM D696 |
|
Kolon KOPA® KN333G35CR G/F Reinforced Nylon 66
High thermal resistant, Weather resistant, dimensionally stableApplications Cylinder head coversInformation provided by API-Kolon.
|
|||
| CTE, linear | 20.0 µm/m-°C | 11.1 µin/in-°F | ASTM D696 |
|
Kolon KOPA® KN333G35CRBK G/F Reinforced Nylon 66
EG-resistant, high strength, dimensionally stableApplications Coolant temperature control partsInformation provided by API-Kolon.
|
|||
| CTE, linear | 20.0 µm/m-°C | 11.1 µin/in-°F | ASTM D696 |
|
Gromax CCP PET 9130-104 30% Glass Filled
Product Description: PET glass/mineral 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excell..
|
|||
| CTE, linear |
20.0
µm/m-°C @Temperature 20.0 °C |
11.1
µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
|
Teijin Panlite® GN-3430R Improved Mold Release, Glass Fiber Reinforced, Flame Resistant Polycarbonate Resin
GF 30% reinforced, flame retardant and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecision machin..
|
|||
| CTE, linear |
20.0
µm/m-°C @Temperature 23.0 - 55.0 °C |
11.1
µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
|
Polyplastics Duranex® 330HR Polybutylene Terephthalate (PBT), Hydrolysis resistant, Heat shock resistant, 30% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
|
|||
| CTE, linear |
20.0
µm/m-°C @Temperature 23.0 - 55.0 °C |
11.1
µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
|
Polyplastics Duranex® 531HS Polybutylene Terephthalate (PBT), Hydrolysis resistant, Heat shock resistant, Heat Shock Resistant
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
|
|||
| CTE, linear |
20.0
µm/m-°C @Temperature -30.0 - 30.0 °C |
11.1
µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM E831 |
|
A. Schulman POLYPUR™ FPU 1152C Thermoplastic Polyurethane
Information provided by A. Schulman.
|
|||
| CTE, linear |
20.0
µm/m-°C @Temperature 23.0 - 55.0 °C |
11.1
µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
|
Polyplastics Duranex® 3300H Polybutylene Terephthalate (PBT), Standard, 30% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
|
|||
| CTE, linear |
20.0
µm/m-°C @Temperature 23.0 - 55.0 °C |
11.1
µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
|
Polyplastics Duranex® 3316 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50%, 30% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
|
|||
| CTE, linear |
20.0
µm/m-°C @Temperature 20.0 °C |
11.1
µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
|
DSM Stanyl® TW241F6 Nylon 46-30% Glass Reinforced, Heat Stabilized, Lubricated (Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
|
|||
| CTE, linear |
20.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
11.1
µin/in-°F @Temperature 73.4 - 176 °F |
DIN 53752 |
|
CP-Polymer-Technik Wellamid® 6600 GV 30 HWCP 30% Glass Fiber Nylon 66, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| CTE, linear |
20.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
11.1
µin/in-°F @Temperature 73.4 - 176 °F |
DIN 53752 |
|
CP-Polymer-Technik Wellamid® 6600/58 GV 30 HWCP 30% Glass Fiber Nylon 66, Impact Modified Until -40°C, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| CTE, linear | 20.0 - 30.0 µm/m-°C | 11.1 - 16.7 µin/in-°F | |
|
Hippe PA 66 GF 30 Nylon 66 30% Glass fiber Reinforced
These polyamide components being reinforced with glass fiber up to 30% are not only highly wear-resistant, but also show high mechanical strength, stiffness and dimensional stability. They can also..
|
|||
| CTE, linear | 20.0 - 30.0 µm/m-°C | 11.1 - 16.7 µin/in-°F | |
|
Hippe PBT GF 30 Polybutylene Terephthalate 30% Glass fiber Reinforced
PBT GF is a highly versatile, semi-crystalline structural thermoplastic reinforced with 30% glass fiber, with very high rigidity and strength characteristics and excellent electrical insulation prop..
|
|||
| CTE, linear |
20.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
11.1
µin/in-°F @Temperature 73.4 - 176 °F |
53752-A |
|
BASF Elastollan R 1000 20% Glass Filled TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan..
|
|||
| CTE, linear |
20.0
µm/m-°C @Temperature 20.0 °C |
11.1
µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
|
Teijin Panlite® B-8120R Carbon Fiber Reinforced Polycarbonate Resin
CF 20% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are low molding shrinkage and dimensional accuracy.Applica..
|
|||
| CTE, linear |
20.0
µm/m-°C @Temperature 20.0 °C |
11.1
µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
|
Teijin Panlite® G-3430R Glass Fiber Reinforced Polycarbonate Resin
GF 30% reinforced and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecision machinery components th..
|
|||
| CTE, linear |
20.0
µm/m-°C @Temperature 20.0 °C |
11.1
µin/in-°F @Temperature 68.0 °F |
DN.53752 |
|
Polimersan Plastics POLIPOLEN® (Polyethylene) UHMW-PE 1000