Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 15.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
CTE, linear 15.0 µm/m-°C
8.33 µin/in-°F
X-Direction; 10°C/min; ASTM D3386; IPC-TM-650 2.4.41
Rogers Corporation RT/duroid® 6202PR High Frequency Laminate
Features:Low loss for excellent high frequency performanceTight dielectric constant and thickness controlExcellent electrical and mechanical propertiesExtremely low thermal coefficient of dielectric..
CTE, linear 15.0 - 20.0 µm/m-°C

@Temperature 50.0 - 150 °C
8.33 - 11.1 µin/in-°F

@Temperature 122 - 302 °F
ISO 11359-2
Raschig Group 3505 Epoxy
Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed..
CTE, linear 15.0 - 20.0 µm/m-°C

@Temperature 50.0 - 150 °C
8.33 - 11.1 µin/in-°F

@Temperature 122 - 302 °F
ISO 11359-2
Raschig Group 3535 Epoxy
Glass fiber-reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties adn dimensional stability even at high temperatures. Form: Low dust granulate pack..
CTE, linear 15.0 - 20.0 µm/m-°C

@Temperature 50.0 - 150 °C
8.33 - 11.1 µin/in-°F

@Temperature 122 - 302 °F
ISO 11359-2
Raschig Group EPOXIDUR® 3582 EP Epoxy
Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Moldi..
CTE, linear 15.0 - 35.0 µm/m-°C

@Temperature 50.0 - 100 °C
8.33 - 19.4 µin/in-°F

@Temperature 122 - 212 °F
longitudinal; ISO 11359-2
Raschig Group MELOPLAS® 152 MF
Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al..
CTE, linear 15.0 - 35.0 µm/m-°C

@Temperature 50.0 - 100 °C
8.33 - 19.4 µin/in-°F

@Temperature 122 - 212 °F
longitudinal; ISO 11359-2
Raschig Group MELOPLAS® 152.7 MF
Cellulose-reinforced MF molding compound in white and colored shades. High surface hardness, very good UV stability, very good resistance to chemicals also to foodstuff ingredients, physiologically..
CTE, linear 15.0 - 35.0 µm/m-°C

@Temperature 50.0 - 100 °C
8.33 - 19.4 µin/in-°F

@Temperature 122 - 212 °F
ISO 11359-2
Raschig Group MELOPLAS® 181 MF
Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. High surface hardness, good electrical properties, good mechanical strength, high UV and heat resistanc..
CTE, linear 15.0 - 35.0 µm/m-°C

@Temperature 50.0 - 100 °C
8.33 - 19.4 µin/in-°F

@Temperature 122 - 212 °F
ISO 11359-2
Raschig Group MELOPLAS® 182 MF
Wood flour-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in dark colors. Improved dimensional stability and electrical properties as compared with MP 180, high surf..
CTE, linear 15.0 - 35.0 µm/m-°C

@Temperature 50.0 - 100 °C
8.33 - 19.4 µin/in-°F

@Temperature 122 - 212 °F
ISO 11359-2
Raschig Group MELOPLAS® 183 MF
Cellulose-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in white and colored shades. Improved dimensional stability and electrical properties as compared with MP 18..
CTE, linear 15.0 - 35.0 µm/m-°C

@Temperature 50.0 - 100 °C
8.33 - 19.4 µin/in-°F

@Temperature 122 - 212 °F
ISO 11359-2
Raschig Group MELOPLAS® 2500 MF
Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al..
CTE, linear 15.0 µm/m-°C
8.33 µin/in-°F
ISO 11359-2
Solvay Specialty Polymers Ixef® 1022 Polyarylamide (PARA)  (Unverified Data**)
Ixef 1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. Ixef 1022..
CTE, linear 15.0 µm/m-°C
8.33 µin/in-°F
ISO 11359-2
Solvay Specialty Polymers Ixef® GS-1022 Polyarylamide (PARA)  (Unverified Data**)
Ixef GS-1022 is a 50% glass-fiber reinforced grade of polyarylamide (PARA) available in several colors. Parts molded from these colored resins can withstand high-energy gamma radiation without signi..
CTE, linear 15.0 µm/m-°C

@Temperature 20.0 °C
8.33 µin/in-°F

@Temperature 68.0 °F
Cookson Group Plaskon® LS-16S Molding Compound  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.A low stress molding compound specifically formulated for use with conventional molding equipment to increase semiconductor manuf..
CTE, linear 15.0 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
8.33 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis
Industrial Laminates/Norplex NP841 Glass Fabric  (discontinued **)
Description: Woven glass fabric with phenolic resin. Contains Kocite® for controlled conductivity. Acts as static electricity drain to protect electrical and electronic equipment.Thickness Tested: ..
CTE, linear 15.0 µm/m-°C

@Temperature 20.0 °C
8.33 µin/in-°F

@Temperature 68.0 °F
Indium Corp. Indalloy® 281 Bi-Sn Solder Alloy
Good low melting point solder for electronics assembly of for applications where Cd and Pb are to be avoided, and for thermo-electric applications. Shear rate sensitive.Information provided by the m..
CTE, linear 15.0 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
8.33 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis; IPC-TM 650-2.4.24
Industrial Laminates/Norplex NP504 Glass Fabric
Description: Woven glass fabric with high temperature phenolic resin. Good flexural, compressive and impact strengths at elevated temperatures. Capable of continuous operation at 175° C, see note..
CTE, linear 15.0 - 30.0 µm/m-°C

@Temperature 20.0 - 100 °C
8.33 - 16.7 µin/in-°F

@Temperature 68.0 - 212 °F
DIN 53752
Schwartz Technical Plastics LAMINEX® 2140 Cotton Fabric, Phenolic Resin Impregnated, MoS2 Filled
Application: bearing shells and bearing collarsInformation provided by Schwartz Technical Plastics GmbH
CTE, linear 15.0 µm/m-°C

@Temperature 20.0 - 100 °C
8.33 µin/in-°F

@Temperature 68.0 - 212 °F
Special Metals BRIGHTRAY® Alloy F Electrical Resistance Alloy
A nickel-iron-chromium electrical-resistance alloy for use at temperatures up to 1920°F (1050°C) under continuous operating conditions. Its high iron content and relatively low level of nicke..
CTE, linear 15.0 µm/m-°C

@Temperature 20.0 - 100 °C
8.33 µin/in-°F

@Temperature 68.0 - 212 °F
Special Metals INCOLOY® Alloy DS
A nickel-iron-chromium alloy with an addition of silicon. It has good high-temperature strength and excellent resistance to oxidation and carburization. The silicon content makes the alloy resista..
CTE, linear 15.0 µm/m-°C
8.33 µin/in-°F
ISO 11359-2
Unitika RUN35-C25 PA6, Dry
High modulus and low warpage nylonInformation provided by Unitika Ltd.
CTE, linear 15.0 µm/m-°C
8.33 µin/in-°F
x, before Tg; IPC TM-650 2.4.24
Arlon 25N Low-Cost Ceramic Hydrocarbon
High Frequency, Low Loss Thermoset Laminate and Prepreg for Double-sided, Multilayer and Mixed Dielectric Printed Circuit BoardsLow loss ceramic-filled thermoset resinTight dielectric tolerance cont..
CTE, linear 15.0 µm/m-°C
8.33 µin/in-°F
y, before Tg; IPC TM-650 2.4.24
Arlon 25N Low-Cost Ceramic Hydrocarbon
High Frequency, Low Loss Thermoset Laminate and Prepreg for Double-sided, Multilayer and Mixed Dielectric Printed Circuit BoardsLow loss ceramic-filled thermoset resinTight dielectric tolerance cont..
CTE, linear 15.0 µm/m-°C

@Temperature 20.0 °C
8.33 µin/in-°F

@Temperature 68.0 °F
California Fine Wire Nickel 272 Super Alloy
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
CTE, linear 15.0 µm/m-°C

@Temperature 20.0 °C
8.33 µin/in-°F

@Temperature 68.0 °F
California Fine Wire Stablohm 750 Chromium, Aluminum, and Iron Resistance Wire
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
CTE, linear 15.0 - 22.0 µm/m-°C
8.33 - 12.2 µin/in-°F
VDE 0304 T1
Bulk Molding Compounds tetra-DUR N 4111 Bulk Molding Compound
Smooth, high gloss surface. Low profile.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion..
CTE, linear 15.0 µm/m-°C

@Temperature 20.0 °C
8.33 µin/in-°F

@Temperature 68.0 °F
Cosmic Plastics 6120F Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
CTE, linear 15.0 - 224 µm/m-°C
8.33 - 124 µin/in-°F
Average value: 106 µm/m-°C Grade Count:20
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a..
Copyright © lookpolymers.com All Rights Reserved