| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear |
170
µm/m-°C @Temperature 23.0 - 60.0 °C |
94.4
µin/in-°F @Temperature 73.4 - 140 °F |
|
|
Murtfeldt Original Material ”S”® plus + GB Polyethylene, Glass Bead Filled
The balanced quantity of micro glass beads in Material ”S”® plus+ GB provides the combined benefits of extremely high molecular weight polyethylene and glass. The glass beads that protrude from ..
|
|||
| CTE, linear |
170
µm/m-°C @Temperature 20.0 °C |
94.4
µin/in-°F @Temperature 68.0 °F |
|
|
Humiseal 1A27 Urethane Conformal Coating
Humiseal 1A27 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL ApprovedPasses thermal shock test (MIL-I-46058C)Flammabilit..
|
|||
| CTE, linear |
170
µm/m-°C @Temperature 20.0 °C |
94.4
µin/in-°F @Temperature 68.0 °F |
|
|
Humiseal 1A27LSE Urethane Conformal Coating
Humiseal 1A27LSE Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL Approval PendingPasses thermal shock test (MIL-I-46058C)..
|
|||
| CTE, linear |
170
µm/m-°C @Temperature 20.0 °C |
94.4
µin/in-°F @Temperature 68.0 °F |
|
|
Humiseal 1A33 Urethane Conformal Coating
Humiseal 1A33 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL ApprovedMIL-I-46058C ApprovedPasses thermal shock test (MIL..
|
|||
| CTE, linear |
170
µm/m-°C @Temperature 20.0 °C |
94.4
µin/in-°F @Temperature 68.0 °F |
|
|
Humiseal 1A33LSE Urethane Conformal Coating
Humiseal 1A33LSE Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses ther..
|
|||
| CTE, linear |
170
µm/m-°C @Temperature 20.0 °C |
94.4
µin/in-°F @Temperature 68.0 °F |
|
|
Humiseal 1C61 UV Cure Conformal Coating
Humiseal 1C61 UV Cure Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock t..
|
|||
| CTE, linear |
170
µm/m-°C @Temperature 20.0 °C |
94.4
µin/in-°F @Temperature 68.0 °F |
|
|
Momentive Performance Materials TSE326 High Temperature, Heat Cured One Component Silicone Adhesive
TSE326 is a one-component, heat curing silicone adhesive which offers extended performance at temperatures exceeding 200C. A flowable material with primerless adhesion to many substrates, it is suit..
|
|||
| CTE, linear |
170
µm/m-°C @Temperature -80.0 - -30.0 °C |
94.4
µin/in-°F @Temperature -112 - -22.0 °F |
ASTM D696 |
|
Lubrizol Pellethane® 2363-80A Thermoplastic Polyurethane Elastomer
Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
|
|||
| CTE, linear |
170
µm/m-°C @Temperature 20.0 °C |
94.4
µin/in-°F @Temperature 68.0 °F |
TMA |
|
Toyobo Pelprene™ P-150M Polyester TPE
Key Feature: Pelprene P typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'P' type is a block..
|
|||
| CTE, linear |
170
µm/m-°C @Temperature 20.0 °C |
94.4
µin/in-°F @Temperature 68.0 °F |
TMA |
|
Toyobo PELPRENE™ P40H Polyester TPE
Features: Polyester TPEInformation provided by Toyobo.
|
|||
| CTE, linear |
170
µm/m-°C @Temperature 20.0 °C |
94.4
µin/in-°F @Temperature 68.0 °F |
TMA |
|
Toyobo PELPRENE™ P40H-05 Polyester TPE, Non-smell, Non-deposit
Features: Polyester TPE, Non-smell, Non-depositInformation provided by Toyobo.
|
|||
| CTE, linear |
170
µm/m-°C @Temperature 20.0 °C |
94.4
µin/in-°F @Temperature 68.0 °F |
TMA |
|
Toyobo PELPRENE™ P40U Polyester TPE, Weather-resistant
Features: Polyester TPE, Weather-resistantInformation provided by Toyobo.
|
|||
| CTE, linear |
170
µm/m-°C @Temperature 20.0 °C |
94.4
µin/in-°F @Temperature 68.0 °F |
TMA |
|
Toyobo PELPRENE™ P46D-01 Polyester TPE, High Viscous, High Durability
Features: Polyester TPE, High Viscous, High DurabilityInformation provided by Toyobo.
|
|||
| CTE, linear |
170
µm/m-°C @Temperature 20.0 °C |
94.4
µin/in-°F @Temperature 68.0 °F |
TMA |
|
Toyobo PELPRENE™ P55U Polyester TPE, Weather-resistant
Features: Polyester TPE, Weather-resistantInformation provided by Toyobo.
|
|||
| CTE, linear |
170
µm/m-°C @Temperature 20.0 °C |
94.4
µin/in-°F @Temperature 68.0 °F |
TMA |
|
Toyobo PELPRENE™ P80C Polyester TPE, High Flexibility, High Melting Point
Features: Polyester TPE, High Flexibility, High Melting PointInformation provided by Toyobo.
|
|||
| CTE, linear |
170
µm/m-°C @Temperature 20.0 °C |
94.4
µin/in-°F @Temperature 68.0 °F |
TMA |
|
Toyobo PELPRENE™ P95C Polyester TPE, High Flexibility, High Melting Point
Features: Polyester TPE, High Flexibility, High Melting PointInformation provided by Toyobo.
|
|||
| CTE, linear | 170 µm/m-°C | 94.4 µin/in-°F | Above Tg |
|
Tra-Con Tra-Bond 9070D Filled Epoxy Adhesive
TRA-BOND 9070D filled epoxy adhesive exhibits a low coefficient of expansion. Information provided by Tra-Con Inc.
|
|||
| CTE, linear |
170
µm/m-°C @Temperature -20.0 - 32.0 °C |
94.4
µin/in-°F @Temperature -4.00 - 89.6 °F |
ASTM D696 |
|
DuPont™ Surlyn® 8020 Ionomer Resin, Sodium
Surlyn® 8020 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu..
|
|||
| CTE, linear |
170
µm/m-°C @Temperature -20.0 - 32.0 °C |
94.4
µin/in-°F @Temperature -4.00 - 89.6 °F |
ASTM D696 |
|
DuPont™ Surlyn® 9020 Ionomer Resin, Zinc
Surlyn® 9020 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The resin contains an addit..
|
|||
| CTE, linear | 170 µm/m-°C | 94.4 µin/in-°F | Above Tg |
|
Epoxy Technology EPO-TEK® OG603 UV Cure Optical Epoxy
Material Description: A single component, low viscosity, UV curable adhesive designed for curing in seconds. It is an all-purpose, general adhesive for optical applications including fiber optic co..
|
|||
| CTE, linear | 170 µm/m-°C | 94.4 µin/in-°F | |
|
Hippe PE 500 Polyethylene
Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall..
|
|||
| CTE, linear | 170 µm/m-°C | 94.4 µin/in-°F | Above Tg |
|
3M Scotch-Weld™ DP8005 Black Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl..
|
|||
| CTE, linear | 170 µm/m-°C | 94.4 µin/in-°F | Above Tg |
|
3M Scotch-Weld™ DP8005 Translucent Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl..
|
|||
| CTE, linear |
170
µm/m-°C @Temperature 20.0 °C |
94.4
µin/in-°F @Temperature 68.0 °F |
TMA |
|
Toyobo PELPRENE™ P48U Polyester TPE, Weather-resistant
Features: Polyester TPE, Weather-resistantInformation provided by Toyobo.
|
|||
| CTE, linear |
170
µm/m-°C @Temperature 20.0 °C |
94.2
µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
|
DSM Biomedical CarboSil® 10 90A Biocompatible Silicone Polycarbonate Urethane
(discontinued **)
Combines the biocompatibility and biostability of conventional silicone elastomers with the processability and toughness of thermoplastic urethane elastomers. Noncytotoxic and nonhemolytic. Low-En..
|
|||
| CTE, linear |
170
µm/m-°C @Temperature 20.0 - 60.0 °C |
94.4
µin/in-°F @Temperature 68.0 - 140 °F |
TMS2 Perkin Elmer |
|
Arkema Group Orgalloy® LT 5050 ES Polyamide Alloy
Polyamide Alloy, Blow Molding of Technical PartsInformation provided by Arkema Group
|
|||