Polymer Property : CTE, linear = 2.78 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
CTE, linear 5.00 - 46.8 µm/m-°C
2.78 - 26.0 µin/in-°F
Average value: 11.6 µm/m-°C Grade Count:8
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and ..
CTE, linear 5.00 µm/m-°C
2.78 µin/in-°F
Zircar Zirconia Buster M-15 Alumina Boards, Discs & Cylinders Insulation
Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite..
CTE, linear 5.00 µm/m-°C

@Temperature 20.0 °C
2.78 µin/in-°F

@Temperature 68.0 °F
Zircar Zirconia Buster M-35 Alumina Board, Disc, and Cylinder Insulation
Zircar alumina insulation Type Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with either a high purity alumina binder in BusterA-30 for use at 1600C or with s..
CTE, linear 5.00 µm/m-°C
2.78 µin/in-°F
DIN 53752
Lehmann & Voss LUVOCOM® 1114-8364 PAEK, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Good friction and wear behaviour especially at increased temperatures.Electrically conduct..
CTE, linear 5.00 µm/m-°C

@Temperature 20.0 °C
2.78 µin/in-°F

@Temperature 68.0 °F
GBC Cerasilâ„¢ 223U Ceramic
Has a lower CTE, better thermal shock resistance, lower firing temperature, and lower consistent shrinkage than steatite.Applications: ideal for volume production of small pressed insulators often r..
CTE, linear 5.00 µm/m-°C

@Temperature -30.0 - 70.0 °C
2.78 µin/in-°F

@Temperature -22.0 - 158 °F
Schott G018-186 Dental Glass
Remarks: Ba- and F-containing, high refractive glassApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Provid..
CTE, linear 5.00 µm/m-°C

@Temperature 20.0 - 300 °C
2.78 µin/in-°F

@Temperature 68.0 - 572 °F
ISO 7991
Schott Glass 8250 Borosilicate Glass
Borosilicate glass for sealing to Kovar metal and molybdenum, electrically highly insulating, low refractive index, good insulator X-ray tubes, transmitting tubes, image amplifier tubes, He-Ne-lase..
CTE, linear 5.00 µm/m-°C

@Temperature 20.0 - 300 °C
2.78 µin/in-°F

@Temperature 68.0 - 572 °F
ISO 7991
Schott Glass 8270 Borosilicate Glass
Borosilicate glass for sealing to Kovar metal and molybdenum, electrically highly insulating, defined UV absorption, stabilized against solarization Backlights The heavy metal content for the elem..
CTE, linear 5.00 µm/m-°C

@Temperature -30.0 - 70.0 °C
2.78 µin/in-°F

@Temperature -22.0 - 158 °F
Schott GM39923 Dental Glass
Remarks: Ba- and F-containing, low refractive glassApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Provide..
CTE, linear 5.00 µm/m-°C

@Temperature 20.0 - 1000 °C
2.78 µin/in-°F

@Temperature 68.0 - 1830 °F
Goodfellow Alumino-silicate Glass Ceramic
SiO2 57/Al2O3 36/CaO/MgO/BaOPorous ceramics can be used as filters and for the controlled release of volatile chemicals. In this material, Alumino-Silicate particles are found in a glassy matrix. Th..
CTE, linear 5.00 µm/m-°C

@Temperature 20.0 - 1000 °C
2.78 µin/in-°F

@Temperature 68.0 - 1830 °F
Zircar Ceramics ZAL-45 Alumina Insulation
ZAL-45 is an exceptionally strong low density alumina fiber product. Alumina bonded ZAL-45AA is useful in reducing conditions.Information provided by Zircar Ceramics.
CTE, linear 5.00 µm/m-°C

@Temperature 25.0 - 1000 °C
2.78 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM C372
CoorsTek Hot Pressed Aluminum Nitride
Aluminum Nitride Advantages: High heat dissipation with thermal conductivity of 170 W/m K Non-toxic alternative to BeO Thermal expansion coefficient similar to Si, GaN, and GaAs semiconductors H..
CTE, linear 5.00 µm/m-°C

@Temperature 1000 °C
2.78 µin/in-°F

@Temperature 1830 °F
Chosun Refractories AH-3 Acid-Proof and Heat-Resistant Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 5.00 µm/m-°C

@Temperature 1000 °C
2.78 µin/in-°F

@Temperature 1830 °F
Chosun Refractories AH-4 Acid-Proof and Heat-Resistant Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 5.00 µm/m-°C

@Temperature 1000 °C
2.78 µin/in-°F

@Temperature 1830 °F
Chosun Refractories BATN-3 Gas Purging Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 5.00 µm/m-°C

@Temperature 1000 °C
2.78 µin/in-°F

@Temperature 1830 °F
Chosun Refractories BATN-8 Gas Purging Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 5.00 - 6.00 µm/m-°C

@Temperature 1000 °C
2.78 - 3.33 µin/in-°F

@Temperature 1830 °F
Chosun Refractories CUN-941 Nozzle Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 5.00 µm/m-°C

@Temperature 20.0 °C
2.78 µin/in-°F

@Temperature 68.0 °F
Parallel DOM
Alliance N-30UH Neodymium Iron Boron Magnetic Material
CTE, linear 5.00 µm/m-°C

@Temperature 20.0 °C
2.78 µin/in-°F

@Temperature 68.0 °F
Parallel DOM
Alliance N-35SH Neodymium Iron Boron Magnetic Material
CTE, linear 5.00 µm/m-°C

@Temperature 20.0 °C
2.78 µin/in-°F

@Temperature 68.0 °F
Parallel DOM
Alliance N-38 Neodymium Iron Boron Magnetic Material
CTE, linear 5.00 µm/m-°C

@Temperature 20.0 °C
2.78 µin/in-°F

@Temperature 68.0 °F
Parallel DOM
Alliance N-40H Neodymium Iron Boron Magnetic Material
CTE, linear 5.00 µm/m-°C

@Temperature 20.0 °C
2.78 µin/in-°F

@Temperature 68.0 °F
Parallel DOM
Alliance N-40SH Neodymium Iron Boron Magnetic Material
CTE, linear 5.00 µm/m-°C

@Temperature 20.0 °C
2.78 µin/in-°F

@Temperature 68.0 °F
Parallel DOM
Alliance N-44H Neodymium Iron Boron Magnetic Material
CTE, linear 5.00 µm/m-°C

@Temperature 20.0 - 1000 °C
2.78 µin/in-°F

@Temperature 68.0 - 1830 °F
Anderman Ceramics EC90P Mullite-Bonded Porous Silicon Carbide (90%)
Excellent thermal shock properties and thermal conductivity when in contact with molten metal. Available as tube, sheath, or rod up to 6 ft (1.9 m) long with diameters 0.6" to 3.75".Information pro..
CTE, linear 5.00 µm/m-°C

@Temperature 20.0 - 1000 °C
2.78 µin/in-°F

@Temperature 68.0 - 1830 °F
Ceradyne Ceralloy® 137 CB AlN Composite
Applications: replacement for Ceralloy® 2710 BeO-SiCterminationssever wedgesload pelletsabsorbersFeatures: higher thermal conductivity then Ceraloy® BeO-SiC at temperatures greater then 150°C, cl..
CTE, linear 5.00 µm/m-°C

@Temperature 20.0 °C
2.78 µin/in-°F

@Temperature 68.0 °F
Parallel DOM
Alliance N-30EZ Neodymium Iron Boron Magnetic Material
CTE, linear 5.00 - 5.50 µm/m-°C

@Temperature 25.0 - 800 °C
2.78 - 3.06 µin/in-°F

@Temperature 77.0 - 1470 °F
China-Yixing Longly Refractories 75 Alumina Ceramic
LONGLY selects high quality ceramic fine powder and micropowder as materials, adopts modern advanced molding technology to produce a multitude of ceramic tubes, rods, beads, balls, columns, plates, ..
CTE, linear 5.00 µm/m-°C

@Temperature 1000 °C
2.78 µin/in-°F

@Temperature 1830 °F
Chosun Refractories H-4S High Alumina brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 5.00 µm/m-°C

@Temperature 20.0 - 1000 °C
2.78 µin/in-°F

@Temperature 68.0 - 1830 °F
Zircar Ceramics ZAL-15 Alumina Insulation
ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics.