| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 20.0 - 42.2 µm/m-°C | 11.1 - 23.4 µin/in-°F | Average value: 33.6 µm/m-°C Grade Count:4 |
|
Overview of materials for Phenolic, Novolac, Impact Grade, Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Impact Grade, Filled". Each property range of values reported is minimum and maximum ..
|
|||
| CTE, linear | 20.0 µm/m-°C | 11.1 µin/in-°F | Average value: 20.0 µm/m-°C Grade Count:3 |
|
Overview of materials for Nylon 63, 35% Glass-Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 63, 35% Glass-Filled". Each property range of values reported is minimum and maximum values of app..
|
|||
| CTE, linear | 20.0 µm/m-°C | 11.1 µin/in-°F | DIN 53752 |
|
Lehmann & Voss LUVOCOM® 19-7342 Polyamide 46, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
|
|||
| CTE, linear | 20.0 µm/m-°C | 11.1 µin/in-°F | DIN 53752 |
|
Lehmann & Voss LUVOCOM® 20-0665 Polyphthalamide, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
|
|||
| CTE, linear |
20.0
µm/m-°C <br>@Temperature 20.0 °C
|
11.1
µin/in-°F <br>@Temperature 68.0 °F
|
DIN 53752; ASTM D696 |
|
Kolon KOPA® KN332G30VO G/F Reinforced & Flame Retardant Nylon 66
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin..
|
|||
| CTE, linear | 20.0 µm/m-°C | 11.1 µin/in-°F | ASTM D696 |
|
Kolon KOPA® KN333G25CRBK G/F Reinforced Nylon 66
EG-resistant, high strength, dimensionally stableApplications Cooling water pipesInformation provided by API-Kolon.
|
|||
| CTE, linear | 20.0 µm/m-°C | 11.1 µin/in-°F | ASTM D696 |
|
Kolon KOPA® KN333G30BL G/F Reinforced Nylon 66
G/F 30% reinforcedApplications Engine coversInformation provided by API-Kolon.
|
|||
| CTE, linear |
20.0
µm/m-°C <br>@Temperature 20.0 °C
|
11.1
µin/in-°F <br>@Temperature 68.0 °F
|
DIN 53752; ASTM D696 |
|
Kolon KOPA® KN333G33CR G/F Reinforced Nylon 66
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin..
|
|||
| CTE, linear |
20.0
µm/m-°C <br>@Thickness 1.57 mm,<br> Temperature 20.0 °C
|
11.1
µin/in-°F <br>@Thickness 0.0620 in,<br> Temperature 68.0 °F
|
x-axis; IPC-TM 650-2.4.24 |
|
Industrial Laminates/Norplex NP664 Paper Base Laminate
Description: Low cost room temperature punching grade with mechanical and electrical properties similar to NP612. This version is made with pigment cover plies on the surface.Thickness Tested: 0.062..
|
|||
| CTE, linear |
20.0
µm/m-°C <br>@Temperature 20.0 °C
|
11.1
µin/in-°F <br>@Temperature 68.0 °F
|
ISO 11359 |
|
Teijin Panlite® GV-3430R High Flame Retardancy, Glass Fiber Reinforced Polycarbonate Resin
GF 30% reinforced, improved flame retardance and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecis..
|
|||
| CTE, linear |
20.0
µm/m-°C <br>@Temperature 23.0 - 55.0 °C
|
11.1
µin/in-°F <br>@Temperature 73.4 - 131 °F
|
ISO 11359-2 |
|
Polyplastics Duranex® 303RA Polybutylene Terephthalate (PBT), Resin adhesion improved for multiple injection molding, 30% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
|
|||
| CTE, linear |
20.0
µm/m-°C <br>@Temperature 20.0 °C
|
11.1
µin/in-°F <br>@Temperature 68.0 °F
|
ISO 11359-2 |
|
Polyplastics Freqtis® P0813A (PPS/LCP), Molding Compound
Both base resins (PPS and LCP) exhibit excellent heat resistance, dimensional stability and molding processability. Therefore Freqtis® is widely used for surface mounted electronic components. In ..
|
|||
| CTE, linear |
20.0
µm/m-°C <br>@Temperature 20.0 °C
|
11.1
µin/in-°F <br>@Temperature 68.0 °F
|
ISO 11359-2 |
|
Polyplastics Freqtis® P1210A (PPS/LCP), Molding Compound
Both base resins (PPS and LCP) exhibit excellent heat resistance, dimensional stability and molding processability. Therefore Freqtis® is widely used for surface mounted electronic components. In ..
|
|||
| CTE, linear |
20.0
µm/m-°C <br>@Temperature 23.0 - 55.0 °C
|
11.1
µin/in-°F <br>@Temperature 73.4 - 131 °F
|
ISO 11359-2 |
|
Polyplastics Duranex® 3300 Polybutylene Terephthalate (PBT), Standard, 30% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
|
|||
| CTE, linear |
20.0
µm/m-°C <br>@Temperature 20.0 °C
|
11.1
µin/in-°F <br>@Temperature 68.0 °F
|
ASTM D696 |
|
Toyobo VYLOPET® EMC532 Injection Molding Polyester Resin, Glass Reinforced
Applications: Auto-partsFeatures: Ultrasonic weldabilityGlass fiber reinforcementInformation provided by Toyobo.
|
|||
| CTE, linear |
20.0
µm/m-°C <br>@Temperature 20.0 - 300 °C
|
11.1
µin/in-°F <br>@Temperature 68.0 - 572 °F
|
|
|
Eagle Brass 260 Cartridge Brass, Extra Spring
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul..
|
|||
| CTE, linear |
20.0
µm/m-°C <br>@Temperature 20.0 - 300 °C
|
11.1
µin/in-°F <br>@Temperature 68.0 - 572 °F
|
|
|
Eagle Brass 260 Cartridge Brass, Hard
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul..
|
|||
| CTE, linear |
20.0
µm/m-°C <br>@Temperature 20.0 - 300 °C
|
11.1
µin/in-°F <br>@Temperature 68.0 - 572 °F
|
|
|
Eagle Brass 260 Cartridge Brass, Spring
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul..
|
|||
| CTE, linear |
20.0
µm/m-°C <br>@Temperature 20.0 °C
|
11.1
µin/in-°F <br>@Temperature 68.0 °F
|
ASTM D696 |
|
Covestro Baydur® STR/F-375 Polyurethane Composite SRIM Foam, 20% Glass Filled, MDI-based 2-Component Liquid System
Contains continuous strand fiberglass mat.0.125 in. thickness.Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer ..
|
|||
| CTE, linear |
20.0
µm/m-°C <br>@Temperature 23.0 - 80.0 °C
|
11.1
µin/in-°F <br>@Temperature 73.4 - 176 °F
|
DIN 53752 |
|
CP-Polymer-Technik Wellamid® 6000 GV 30 HW 30% Glass Fiber Nylon 6, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| CTE, linear |
20.0
µm/m-°C <br>@Temperature 20.0 °C
|
11.1
µin/in-°F <br>@Temperature 68.0 °F
|
ISO 11359-1/-2 |
|
DSM Stanyl® TW241F6 Nylon 46-30% Glass Reinforced, Heat Stabilized, Lubricated (Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
|
|||
| CTE, linear |
20.0
µm/m-°C <br>@Temperature 20.0 °C
|
11.1
µin/in-°F <br>@Temperature 68.0 °F
|
ISO 11359-1/-2 |
|
DSM Stanyl® TW241F8 Nylon 46-40% Glass Reinforced, Heat Stabilized, Lubricated (Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
|
|||
| CTE, linear |
20.0
µm/m-°C <br>@Temperature 23.0 - 80.0 °C
|
11.1
µin/in-°F <br>@Temperature 73.4 - 176 °F
|
DIN 53752 |
|
CP-Polymer-Technik Wellamid® 6600 MZ 401 CP Combination Nylon 66, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| CTE, linear |
20.0
µm/m-°C <br>@Temperature 23.0 - 80.0 °C
|
11.1
µin/in-°F <br>@Temperature 73.4 - 176 °F
|
DIN 53752 |
|
CP-Polymer-Technik Wellamid® 6600/58 GV 30 HWCP 30% Glass Fiber Nylon 66, Impact Modified Until -40°C, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| CTE, linear | 20.0 - 30.0 µm/m-°C | 11.1 - 16.7 µin/in-°F | |
|
Hippe PBT GF 30 Polybutylene Terephthalate 30% Glass fiber Reinforced
PBT GF is a highly versatile, semi-crystalline structural thermoplastic reinforced with 30% glass fiber, with very high rigidity and strength characteristics and excellent electrical insulation prop..
|
|||
| CTE, linear |
20.0
µm/m-°C <br>@Thickness 0.0508 mm
|
11.1
µin/in-°F <br>@Thickness 0.00200 in
|
First heat; ASTM-D696 |
|
3M 9673 Adhesive Transfer Tapes with Adhesive 300
3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f..
|
|||
| CTE, linear |
20.0
µm/m-°C <br>@Temperature 20.0 °C
|
11.1
µin/in-°F <br>@Temperature 68.0 °F
|
|
|
AIM 35.7Sn/35.7Pb/28.6Bi Solder for Photonic Packaging
Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials.
|
|||
| CTE, linear |
20.0
µm/m-°C <br>@Temperature 20.0 °C
|
11.1
µin/in-°F <br>@Temperature 68.0 °F
|
Dry; ASTM D696 |
|
Asahi Kasei Leona® 14G33 33% Glass Filled Nylon 66
Enhanced strength and stiffness; with 33% GF. Superior heat aging resistance, fatigue resistance, and creep resistance.Applications:Mechanical and electrical parts, engine mounts and other under-the..
|
|||