| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 37.8 µm/m-°C @Temperature 20.0 °C |
21.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Ravago Manufacturing Americas Hylon® N2033HL Nylon 6 (DAM) Information provided by Ravago. |
|||
| CTE, linear | 37.8 µm/m-°C @Temperature 20.0 °C |
21.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Ravago Manufacturing Americas Hylon® N2033STHL Nylon 6 (DAM) Information provided by Ravago. |
|||
| CTE, linear | 37.8 µm/m-°C @Temperature -40.0 - 82.2 °C |
21.0 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
| Styron EMERGEâ„¢ 4731-13 Polycarbonate EMERGEâ„¢ PC 4731-13 advanced resin is formulated with 10% glass fiber and has an f1 rating by Underwriters Laboratories Inc. It provides good ignition resistance, rigidity, dimension stability .. |
|||
| CTE, linear | 37.8 µm/m-°C @Temperature -40.0 - 82.2 °C |
21.0 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
| Styron EMERGEâ„¢ 4731-8 Polycarbonate EMERGEâ„¢ PC 4702-15 advanced resin is formulated with 10% glass fiber and has an f1 rating by Underwriters Laboratories Inc. It provides good ignition resistance, rigidity, dimension stability .. |
|||
| CTE, linear | 37.8 µm/m-°C @Temperature -40.0 - 82.2 °C |
21.0 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
| Styron EMERGEâ„¢ 4701-13 Polycarbonate EMERGEâ„¢ PC 4701-13 advanced resin is formulated with 10% glass fiber and a proprietary flame retardant package. It provides good ignition resistance, rigidity, dimension stability and heat res.. |
|||
| CTE, linear | 37.8 µm/m-°C @Temperature 20.0 °C |
21.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
| Axiall Tuf-Stif 2802 Rigid PVC, Extrusion Georgia Gulf Tuf-Stif 2802 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Improved toughness as compared to Tuf-StiffRigidit.. |
|||
| CTE, linear | 37.8 µm/m-°C @Temperature 20.0 °C |
21.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Asahi Kasei Thermylene® P6-30FG-0600R 30% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
| CTE, linear | 37.8 µm/m-°C @Temperature 20.0 °C |
21.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Asahi Kasei Thermylene® P6-30FG-0684 30% Glass Fiber Reinforced, Heat and UV Information provided by Asahi Thermofil |
|||
| CTE, linear | 37.8 µm/m-°C @Temperature 20.0 °C |
21.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Asahi Kasei Thermylene® P6-30FG-0699 30% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
| CTE, linear | 37.8 µm/m-°C @Temperature 20.0 °C |
21.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Asahi Kasei Thermylene® P6-30FG-1734 30% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
| CTE, linear | 37.8 µm/m-°C @Temperature 20.0 °C |
21.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
| Axiall Tuf-Stif 2804 Rigid PVC, Extrusion Georgia Gulf Tuf-Stif 2804 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Improved toughness as compared to Tuf-StiffRigidit.. |
|||
| CTE, linear | 37.8 µm/m-°C @Temperature 20.0 °C |
21.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Asahi Kasei Thermylene® P-30FG-0812 30% Glass Fiber Reinforced, UV Stabilized Information provided by Asahi Thermofil |
|||
| CTE, linear | 37.8 µm/m-°C @Temperature 20.0 °C |
21.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Asahi Kasei Thermylene® P6-30FG-0600 30% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
| CTE, linear | 37.8 µm/m-°C @Temperature 20.0 °C |
21.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Asahi Kasei Thermylene® P6-30FG-0640 30% Glass Fiber Reinforced, Heat and Copper Information provided by Asahi Thermofil |
|||
| CTE, linear | 37.8 µm/m-°C @Temperature 20.0 °C |
21.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Asahi Kasei Thermylene® P6-30FG-0687 30% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
| CTE, linear | 37.8 µm/m-°C @Temperature 20.0 °C |
21.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Asahi Kasei Thermylene® P6-30FG-0860 30% Glass Fiber Reinforced, UV Stabilized Information provided by Asahi Thermofil |
|||
| CTE, linear | 37.8 µm/m-°C | 21.0 µin/in-°F | |
| BCC Products BC 6128 Epoxy, Hi-Heat, Abrasion Resistant BC 6128 is a black, non-staining, silicon carbide filled, “die surface” surfacing resin. This thixotropic resin system provides excellent surface duplication along with good vertical coverage. Ext.. |
|||
| CTE, linear | 37.8 µm/m-°C | 21.0 µin/in-°F | |
| BCC Products EB 6200 Epoxy Tooling Board EB6200 is a “grain-free” elevated temperature epoxy modeling material known for its superior surface finish, dimensional stability and the ability to maintain tolerances even after being subjected.. |
|||
| CTE, linear | 37.8 - 104 µm/m-°C | 21.0 - 57.8 µin/in-°F | Average value: 62.9 µm/m-°C Grade Count:10 |
| Overview of materials for Polypropylene Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o.. |
|||
| CTE, linear | 37.8 - 68.4 µm/m-°C | 21.0 - 38.0 µin/in-°F | Average value: 55.0 µm/m-°C Grade Count:13 |
| Overview of materials for Polypropylene with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in.. |
|||