Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 22.2 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
CTE, linear 40.0 µm/m-°C
<br>@Temperature 23.0 - 100 °C
22.2 µin/in-°F
<br>@Temperature 73.4 - 212 °F
Quadrant EPP Duratron® PAI T4203 PAI, unfilled, extruded (ISO Data)
Duratron T4203 PAI offers the best toughness and impact strength of all Duratron PAI grades. This extruded Duratron PAI grade is very popular for precision parts in high-tech equipment. In addition,..
CTE, linear 40.0 µm/m-°C
22.2 µin/in-°F
Z-Direction; IPC-TM-650 2.4.41
Rogers Corporation LoPro™ RO4730 Antenna Grade Non-PTFE Laminate
RO4730 LoPro Antenna Grade Laminates are fully compatible with conventional FR-4 and high temperature lead-free solder processing. The resin systems of RO4730 dielectric materials are designed to p..
CTE, linear 40.0 µm/m-°C
<br>@Temperature 20.0 °C
22.2 µin/in-°F
<br>@Temperature 68.0 °F
ASTM D696
LATI LARIL 13 G/20 20% Glass Fiber Reinforced Polyphenylene Oxide (PPOm) &nbsp;(Unverified Data**)
Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most ..
CTE, linear 40.0 - 110 µm/m-°C
22.2 - 61.1 µin/in-°F
Average value: 80.3 µm/m-°C Grade Count:13
Overview of materials for Acetal Copolymer, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values ..
CTE, linear 40.0 µm/m-°C
22.2 µin/in-°F
ASTM D696
Kolon KOPET® KP133G15BL G/F Reinforced Polyester Compound Resin (PET)
Dimensionally stable, high elastic, high flowApplications: Ink CartridgeInformation provided by API-Kolon.
CTE, linear 40.0 µm/m-°C
<br>@Temperature 20.0 °C
22.2 µin/in-°F
<br>@Temperature 68.0 °F
DIN 53752; ASTM D696
Kolon SPESIN® KP513G30WBL Multi Reinforced PBT Resin
SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High..
CTE, linear 40.0 µm/m-°C
22.2 µin/in-°F
ASTM D696
Kolon SPESIN® KP515FLBL High Impact PBT Alloy Resin
High elastic, whether resistantApplications: WipersInformation provided by API-Kolon.
CTE, linear 40.0 µm/m-°C
<br>@Temperature 20.0 °C
22.2 µin/in-°F
<br>@Temperature 68.0 °F
DIN 53752; ASTM D696
Kolon KOPA® KN133MT40 M/F Reinforced Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
CTE, linear 40.0 µm/m-°C
<br>@Temperature 20.0 °C
22.2 µin/in-°F
<br>@Temperature 68.0 °F
DIN 53752; ASTM D696
Kolon KOPA® KN163G30 G/F Reinforced Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
CTE, linear 40.0 µm/m-°C
<br>@Temperature 20.0 °C
22.2 µin/in-°F
<br>@Temperature 68.0 °F
DIN 53752; ASTM D696
Kolon KOPA® KN173MC M/F Reinforced Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
CTE, linear 40.0 µm/m-°C
<br>@Temperature 20.0 °C
22.2 µin/in-°F
<br>@Temperature 68.0 °F
ISO 11359
Teijin Panlite® G-3410R Glass Fiber Reinforced Polycarbonate Resin
GF 10% reinforced and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecision machinery components th..
CTE, linear 40.0 - 60.0 µm/m-°C
<br>@Temperature -30.0 - 30.0 °C
22.2 - 33.3 µin/in-°F
<br>@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics Noryl GTX GTX870 PPE+PA6 (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear 40.0 - 60.0 µm/m-°C
<br>@Temperature -30.0 - 30.0 °C
22.2 - 33.3 µin/in-°F
<br>@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics NORYL GTX GTX870 PPE+PA6 (Asia Pacific)
CTE, linear 40.0 - 45.0 µm/m-°C
22.2 - 25.0 µin/in-°F
Master Bond EP41S-1HT Solvent Resistant Adhesive, Sealant and Coating
Description: Master Bond EP41S-1HT is a two component epoxy resin system for high performance bonding, sealing, coating and encapsulating. It has a 100 to 30 mix ratio by weight and is formulated to..
CTE, linear 40.0 - 45.0 µm/m-°C
22.2 - 25.0 µin/in-°F
Master Bond Supreme 3HTND-1SM Fast Curing, One Component, Surface Mount Adhesive
Master Bond Polymer System Supreme 3HTND-1SM is a one component, exceptionally fast curing surface mount adhesive system with exceptional toughness and durability. It has high shear and peel strengt..
CTE, linear 40.0 µm/m-°C
<br>@Temperature 20.0 °C
22.2 µin/in-°F
<br>@Temperature 68.0 °F
Toyobo ECOVYLOPET® EMC2310 PET Bottle Recycling Grade, 10% Glass Reinforced
Features: PET Bottle Recycling Grade, 10% Glass Fiber Reinforced, General PurposeApplications: Automobile engine head coversHot platesVending machine partsUmbrella ribsInformation provided by Toyobo..
CTE, linear 40.0 µm/m-°C
<br>@Temperature 20.0 °C
22.2 µin/in-°F
<br>@Temperature 68.0 °F
ASTM D696
Toyobo VYLOPET® EMC310TU Injection Molding Polyester Resin, Warpageless, High cycles
Applications: Coiled bobbinsMouthpiecesFeatures: High cyclesWarpagelessInformation provided by Toyobo.
CTE, linear 40.0 µm/m-°C
<br>@Temperature 20.0 °C
22.2 µin/in-°F
<br>@Temperature 68.0 °F
ASTM D696
E-Polymers TEKAMID® TB110M40 , 40% Mineral Filled PA6, DAM
40% Mineral filled, Heat resistance, PlatableInformation provided by E-Polymers Co. Ltd.
CTE, linear 40.0 µm/m-°C
<br>@Temperature 20.0 °C
22.2 µin/in-°F
<br>@Temperature 68.0 °F
Armstrong C-7/H20 Epoxy Adhesive
A clear, unfilled, medium viscosity adhesive recommended for use with any Armstrong Activator. Physical property data included covers C-7 used with Activators W and H-20. All other Activators may ..
CTE, linear 40.0 µm/m-°C
22.2 µin/in-°F
ASTM E831
Addiplast Addinyl A2 M20 V10 Nylon 66, Glass/Mineral Filled
Mixed products with improved stiffness and good dimensional stability, low warpage.Information provided by Addiplast.
CTE, linear 40.0 µm/m-°C
<br>@Temperature 20.0 °C
22.2 µin/in-°F
<br>@Temperature 68.0 °F
Dry; ASTM D696
Asahi Kasei Leona® 14G15 15% Glass Filled Nylon 66
15% Glass Fiber Reinforced. Enhanced strength and stiffnessApplications:Heater tanks, fuel injectors, ABS sensors, and other under-the-hood automotive parts Information provided by Asahi Kasei
CTE, linear 40.0 µm/m-°C
<br>@Temperature 20.0 °C
22.2 µin/in-°F
<br>@Temperature 68.0 °F
Dry; ASTM D696
Asahi Kasei Leona® CR301 Nylon 66
Suitable for a switch insulator. Low abrasion and superior electrical properties.Applications:Sliding switch insulators Information provided by Asahi Kasei
CTE, linear 40.0 µm/m-°C
<br>@Temperature 23.0 - 80.0 °C
22.2 µin/in-°F
<br>@Temperature 73.4 - 176 °F
DIN 53752
CP-Polymer-Technik Wellamid® 6600 GS 40 HWCP 40% Glass Sphere Filled Nylon 66, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
CTE, linear 40.0 µm/m-°C
22.2 µin/in-°F
ASTM E831
Addiplast Addinyl C2 M20 V10 Nylon 66/6, Glass/Mineral Filled
Mixed products with improved stiffness and good dimensional stability, low warpage.Information provided by Addiplast.
CTE, linear 40.0 µm/m-°C
<br>@Temperature 20.0 °C
22.2 µin/in-°F
<br>@Temperature 68.0 °F
DIN 53752; ASTM D696
Kolon KOPA® KN135G33HI Multi Reinforced Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubric..
CTE, linear 40.0 µm/m-°C
22.2 µin/in-°F
Product Property; ASTM E 831
Arlon R36601A010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate
Description: Generation II Thermabond® NP electrically insulating electronic adhesive. Bonds without primer.Design/Construction: Liner 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Sty..
CTE, linear 40.0 µm/m-°C
22.2 µin/in-°F
Resinlab® EP1240RC Flame Retardant Epoxy Casting Resin
Resinlab™ EP1240RC is a medium viscosity, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File# E186034, Pro..
CTE, linear 40.0 µm/m-°C
<br>@Temperature -30.0 - 30.0 °C
22.2 µin/in-°F
<br>@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics Valox® VSR4150 PBT (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
Copyright © lookpolymers.com All Rights Reserved