Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
CTE, linear 27.0 µm/m-°C

@Temperature -40.0 - 150 °C
15.0 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E831
Quadrant EPP Semitron® MPR-1000 (ASTM Product Data Sheet)
CTE, linear 27.0 µm/m-°C

@Temperature -40.0 - 149 °C
15.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP Duratron® PAI T4503 Compression Molded, Polyamide-imide, Eelectrical Grade (ASTM Product Data Sheet)
CTE, linear 27.0 µm/m-°C

@Temperature -40.0 - 149 °C
15.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP Semitron® 420 ESd V (ASTM Product Data Sheet)
CTE, linear 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
PolyOne Edgetek® AS-30CF/000 UV Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced  (discontinued
Description/Features:Carbon Fiber ReinforcedUV StabilizedUL 94 HB (HEM TEST)PolyOne First ChoiceInformation provided by PolyOne Corporation.
CTE, linear 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Ravago Manufacturing Americas Hylon® N1013L Nylon 6/6 (DAM)  (discontinued **)
Information provided by Ravago.
CTE, linear 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
PolyOne Lubri-Tech™ NL-30GF/15T Nylon 6/12, Glass Filled, PTFE Lubricated  (discontinued **)
Description/Features:Glass Fiber ReinforcedPTFE LubricatedUL 94 HB (HEM TEST)Information provided by PolyOne Corporation.
CTE, linear 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
Indium Corp. Indalloy® 205 In-Pb Solder Alloy
Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics..
CTE, linear 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
Indium Corp. Indalloy® 7 In-Pb Solder Alloy
Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics..
CTE, linear 27.0 µm/m-°C
15.0 µin/in-°F
Through Thickness
GrafTech eGRAF® HITHERM™ HT-2510 Graphite with Polymer Additive
Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat..
CTE, linear 27.0 µm/m-°C
15.0 µin/in-°F
Through Thickness
GrafTech eGRAF® HITHERM™ HT-705 Graphite
Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat..
CTE, linear 27.0 µm/m-°C
15.0 µin/in-°F
Through-Plane
GrafTech eGRAF® SPREADERSHIELD™ SS400 Graphite
Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate..
CTE, linear 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Techmer ES Electrafil® J-1/CF/10 Nylon 66, 10% Carbon Fiber Reinforced
CTE, linear 27.0 µm/m-°C

@Temperature -30.0 - 100 °C
15.0 µin/in-°F

@Temperature -22.0 - 212 °F
ASTM D696
A. Schulman POLYTROPE™ TPP 615 Olefinic Elastomer
DescriptionPolytrope TPP 615 is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 615 is de..
CTE, linear 27.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
15.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
2.7 mm/mm; ASTM D696
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
CTE, linear 27.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
15.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
2.7 mm/mm; ASTM D696
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
CTE, linear 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
Williams Advanced Alloys WS209 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
CTE, linear 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
Longitudinal
Goodfellow Polyaramid/Polyphenylene Sulfide Composite Sheet or Rod
25% Polyaramid fiber - PPS Matrix. Information provided by Goodfellow.
CTE, linear 27.0 µm/m-°C

@Temperature -30.0 - 100 °C
15.0 µin/in-°F

@Temperature -22.0 - 212 °F
ASTM D696
A. Schulman POLYTROPE™ TPP 615 Olefinic Elastomer
DescriptionPolytrope TPP 615 is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 615 is de..
CTE, linear 27.0 µm/m-°C

@Temperature -30.0 - 100 °C
15.0 µin/in-°F

@Temperature -22.0 - 212 °F
ASTM D696
A. Schulman POLYTROPE™ TPP 615 Olefinic Elastomer
DescriptionPolytrope TPP 615 is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 615 is de..
CTE, linear 27.0 µm/m-°C

@Temperature -30.0 - 100 °C
15.0 µin/in-°F

@Temperature -22.0 - 212 °F
ASTM D696
A. Schulman POLYTROPE™ TPP 615 Olefinic Elastomer
DescriptionPolytrope TPP 615 is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 615 is de..
CTE, linear 27.0 µm/m-°C
15.0 µin/in-°F
ASTM C531
Chesterton ARC 791 Composite
Description: A quartz reinforced composite designed to resurface and restore concrete surfaces, to protect new concrete, and to repair concrete damaged by chemical and physical abuse. ARC 791 has ex..
CTE, linear 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Ensinger Tecanat™ GF20 20% Glass Reinforced Polycarbonate (PC)
Tenacat™ GF20 is typically used in business equipment where gears, rollers, interlam mechanical parts, connectors and relays are required. The automotive industry uses polycarbonate materials for ..
CTE, linear 27.0 µm/m-°C
15.0 µin/in-°F
Below Tg
Epoxy Technology EPO-TEK® N20E Electrically Conductive Paste
Product Description: EPO-TEK® N20E is a two component, electrically and thermally conductive, epoxy adhesive designed for semiconductor and electronics assembly. Its applications and field conditi..
CTE, linear 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
AIM 62Sn/Pb36/Ag2 Solder for Photonic Packaging
Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials.
CTE, linear 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Techmer ES Plaslube® J-50/30/TF/15 Polycarbonate, 30% Glass Reinforced, PTFE Lubricated
30% Glass Reinforced, PTFE Lubricated
CTE, linear 27.0 - 93.6 µm/m-°C
15.0 - 52.0 µin/in-°F
Average value: 70.3 µm/m-°C Grade Count:12
Overview of materials for Nylon 6, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, PTFE Filled". Each property range of values reported is minimum and maximum values of appropria..
CTE, linear 27.0 µm/m-°C
15.0 µin/in-°F
ASTM D696
Quantum Nylon 6/6 30% Glass Fiber Filled
Information provided by Quantum Advanced Engineering Plastics
CTE, linear 27.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
15.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
3.45 mm/mm; ASTM D696
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
CTE, linear 27.0 - 68.0 µm/m-°C

@Temperature 125 - 175 °C
15.0 - 37.8 µin/in-°F

@Temperature 257 - 347 °F
Average value: 37.4 µm/m-°C Grade Count:5
Overview of materials for Polyimide, Thermoset Film
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Thermoset Film". Each property range of values reported is minimum and maximum values of appr..