| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear |
54.0
µm/m-°C @Temperature -18.0 - 38.0 °C |
30.0
µin/in-°F @Temperature -0.400 - 100 °F |
ASTM D696 |
|
Plaskolite Optix® PL-25 Acrylic Resin
Extrusion grade pellets. Highest molecular weight and heat resistance of Optix® line.Data provided by the manufacturer, Plaskolite, Inc.
|
|||
| CTE, linear |
54.0
µm/m-°C @Temperature -18.0 - 38.0 °C |
30.0
µin/in-°F @Temperature -0.400 - 100 °F |
ASTM D696 |
|
Plaskolite PETG Mirror Sheet
Versatile fabrication properties with good impact strength, good design flexibility, and speed of fabrication.Data provided by the manufacturer, Plaskolite, Inc.
|
|||
| CTE, linear |
54.0
µm/m-°C @Temperature 17.0 - 37.0 °C |
30.0
µin/in-°F @Temperature 62.6 - 98.6 °F |
ASTM D696 |
|
Plaskolite PL-24 Acrylic Resin
For injection molding. An unlubricated version of PL-25 extrusion grade pellets. Highest molecular weight, maximum heat resistance.Information supplied by the manufacturer.
|
|||
| CTE, linear |
54.0
µm/m-°C @Temperature -18.0 - 38.0 °C |
30.0
µin/in-°F @Temperature -0.400 - 100 °F |
ASTM D696 |
|
Plaskolite Optix® SG Sign Grade Acrylic Sheet
Available in unlimited lengths - no seams in finished products.Data provided by the manufacturer, Plaskolite, Inc.
|
|||
| CTE, linear | 54.0 - 160 µm/m-°C | 30.0 - 88.9 µin/in-°F | Average value: 105 µm/m-°C Grade Count:7 |
|
Overview of materials for Thermoset Polyurethane, Liquid
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid". Each property range of values reported is minimum and maximum values of..
|
|||
| CTE, linear | 54.0 - 340 µm/m-°C | 30.0 - 189 µin/in-°F | Average value: 233 µm/m-°C Grade Count:49 |
|
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Adhesive/Sealant Grade". Each property range of values reported is minimum and maximum va..
|
|||
| CTE, linear |
54.0
µm/m-°C @Temperature -40.0 - 176 °C |
30.0
µin/in-°F @Temperature -40.0 - 349 °F |
ASTM D696 |
|
Ravago Manufacturing Americas Hylac® FR134G10 ABS, 10% Glass Fiber Reinforced
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
|
|||
| CTE, linear |
54.0
µm/m-°C @Temperature -18.0 - 38.0 °C |
30.0
µin/in-°F @Temperature -0.400 - 100 °F |
ASTM D696 |
|
Plaskolite Optix® PL-52 Acrylic Resin
(discontinued **)
Injection/extrusion pellets. High heat resistance/medium flow.Data provided by the manufacturer, Plaskolite, Inc.
|
|||
| CTE, linear | 54.0 - 62.0 µm/m-°C | 30.0 - 34.4 µin/in-°F | Average value: 57.2 µm/m-°C Grade Count:8 |
|
Overview of materials for PVC, Powder
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Powder". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
|
|||
| CTE, linear | 54.0 - 140 µm/m-°C | 30.0 - 77.8 µin/in-°F | Average value: 103 µm/m-°C Grade Count:4 |
|
Overview of materials for Polypropylene, Stainless Fiber, EMI
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum valu..
|
|||
| CTE, linear | 54.0 µm/m-°C | 30.0 µin/in-°F | Average value: 54.0 µm/m-°C Grade Count:3 |
|
Overview of materials for Nylon 6, Stainless Steel Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Stainless Steel Filled". Each property range of values reported is minimum and maximum values o..
|
|||
| CTE, linear |
54.0
µm/m-°C @Temperature 20.0 °C |
30.0
µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
|
LyondellBasell SEQUEL® 1825 Engineered Polyolefin
Description: SEQUEL® 1825 engineered polyolefin is designed for automotive applications that require energy management combined with ductility and a balance of stiffness and impact resistance ove..
|
|||
| CTE, linear |
54.0
-
144
µm/m-°C @Temperature 25.6 - 204 °C |
30.0
-
80.0
µin/in-°F @Temperature 78.0 - 400 °F |
ASTM D696 |
|
Garlock 9405 PTFE Rubber Sheet, 25% Glass Filled
Premium Grade 25% Glass-filled Skived PTFE SheetInformation provided by Garlock Rubber Technologies
|
|||
| CTE, linear | 54.0 µm/m-°C | 30.0 µin/in-°F | Alpha 1 |
|
Lord Adhesives Thermosetâ„¢ MD-150 Conductive Adhesive
LORD Thermosetâ„¢ MD-150 silver-filled conductive adhesive offers excellent electrical and thermal conductivity. It is designed for use with automated dispensing, stamping and screen-printing app..
|
|||
| CTE, linear |
54.0
µm/m-°C @Temperature -30.0 - 30.0 °C |
30.0
µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
|
LyondellBasell Astryn BB73F Polypropylene Copolymer, Mineral Filled
Key Features: high melt flow, high modulus, UV-stabilized, mineral-filled, high rigidity, good impact strength, good dimensional stability, good scratch and mar resistance, excellent processability,..
|
|||
| CTE, linear |
54.0
µm/m-°C @Temperature -30.0 - 30.0 °C |
30.0
µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
|
LyondellBasell Astryn BB77G Polypropylene Copolymer, 15% Talc
Key Features: high melt flow, high modulus, UV-stabilized, mineral-filled polypropylene copolymer, good impact stiffness and balance, good dimensional stability, good colorability, good aesthetics, ..
|
|||
| CTE, linear |
54.0
µm/m-°C @Temperature 20.0 °C |
30.0
µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
|
Saint-Gobain Norton® High Performance Extruded PEI Film
Description: PEI = polyetherimide. Used Primarily for Electrical/Electronics ApplicationsInformation provided by Saint Gobain Performance Products.
|
|||
| CTE, linear |
54.0
µm/m-°C @Temperature -30.0 - 80.0 °C |
30.0
µin/in-°F @Temperature -22.0 - 176 °F |
Borealis Method |
|
Borealis Daplen™ EF341AE Polypropylene TPO Compound
Daplen™ EF341AE is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q..
|
|||
| CTE, linear |
54.0
µm/m-°C @Temperature 40.0 - 130 °C |
30.0
µin/in-°F @Temperature 104 - 266 °F |
TMA; ASTM E831 |
|
Plenco 1501 Polyester, Briquette, Transfer Molded
PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va..
|
|||
| CTE, linear |
54.0
µm/m-°C @Temperature 40.0 - 130 °C |
30.0
µin/in-°F @Temperature 104 - 266 °F |
TMA; ASTM E831 |
|
Plenco 1530 Polyester, Briquette, Transfer Molded
PLENCO 01530 is a glass and mineral reinforced pelletized polyester molding compound, offering improved mechanical strength properties along with excellent electrical properties and dimensional stab..
|
|||
| CTE, linear | 54.0 µm/m-°C | 30.0 µin/in-°F | |
|
Hexcel® HexPly® F593 Epoxy Resin
HexPly® F593 is a modified 350°F (177°C) curing epoxy system with very low flow for carbon fabric and tape applications that provides excellent laminate and honeycomb sandwich properties. As a lo..
|
|||
| CTE, linear | 54.0 µm/m-°C | 30.0 µin/in-°F | Below Tg |
|
Epoxy Technology EPO-TEK® 353ND Black High Temperature Epoxy
Product Description: EPO TEK® 353ND Black is a a two component, high temperature epoxy designed for semiconductor, hybrid, fiber optic, and medical applicationsAdvantages & Application Notes: EPO T..
|
|||
| CTE, linear |
54.0
µm/m-°C @Temperature 20.0 °C |
30.0
µin/in-°F @Temperature 68.0 °F |
|
|
Cotronics Duralco™ 120 500°F Silver Filled Epoxy, Electrically Conductive
Contains over 70% ultra fine silver to provide excellent electrical conductivity. Cures at room temperature.>Applications: ideal for use where maximum conductivity is required.
|
|||
| CTE, linear |
54.0
µm/m-°C @Temperature 20.0 °C |
30.0
µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
|
Asahi Kasei Thermylene® P6-10FG-0600 10% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
|
|||
| CTE, linear |
54.0
µm/m-°C @Temperature 20.0 °C |
30.0
µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
|
Asahi Kasei Thermylene® P6-15FG-1734 15% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
|
|||
| CTE, linear |
54.0
µm/m-°C @Temperature 20.0 °C |
30.0
µin/in-°F @Temperature 68.0 °F |
|
|
Aremco Aremco-Bond™ 657 High Performance Epoxide
Stainless Steel-Filled, High Corrosion Resistance.
|
|||
| CTE, linear |
54.0
µm/m-°C @Temperature 20.0 °C |
30.0
µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
|
Asahi Kasei Thermylene® P1-10FG-8100 10% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
|
|||
| CTE, linear | 54.0 µm/m-°C | 30.0 µin/in-°F | |
|
Resinlab® EP691 Unfilled Electronic Grade Epoxy Encapsulant
Resinlab™ EP691 is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting and ad..
|
|||
| CTE, linear | 54.0 - 90.0 µm/m-°C | 30.0 - 50.0 µin/in-°F | Average value: 72.0 µm/m-°C Grade Count:5 |
|
Overview of materials for Acrylic, Impact Modified Sheet
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified Sheet". Each property range of values reported is minimum and maximum values of..
|
|||
| CTE, linear | 54.0 µm/m-°C | 30.0 µin/in-°F | |
|
Unifrax Fiberfrax® Rigidizer™ W Inorganic Liquid Hardener