Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 4.40 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
CTE, linear 4.40 µm/m-°C
<br>@Temperature 20.0 °C
2.44 µin/in-°F
<br>@Temperature 68.0 °F
Pyrotek Pinnacle Thermocouple Protection Tubes O&#039;-Sialon (Bonded Silicon Carbide) TCPT
The robust properties of Pinnacle Thermocouple Protection Tubes make it a superior alternative to competitive tubes in temperature measurement, maintenance and product life areas.ApplicationsCrucibl..
CTE, linear 4.40 µm/m-°C
<br>@Temperature 260 °C
2.44 µin/in-°F
<br>@Temperature 500 °F
Ferro CF 7574 Glaze and Sealant Glass
Glass Type: Zn-B-Si Typical Powder Form: VSD Typical Application: Pyrex Silicon Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and ..
CTE, linear 4.40 µm/m-°C
<br>@Temperature 260 °C
2.44 µin/in-°F
<br>@Temperature 500 °F
Ferro IX 2730 Passivation Glasses - High Voltage (Zn-B-Silicates)
Typical Powder Form: TF Zinc-Boro-Silicate passivation glasses are used for hermetic passivation of high voltage diodes, thyristors, and transistors. They provide high junction temperatures and can..
CTE, linear 4.40 µm/m-°C
<br>@Temperature 20.0 - 300 °C
2.44 µin/in-°F
<br>@Temperature 68.0 - 572 °F
ISO 7991
Schott Glass 8651 Sealing Glass
Tungsten sealing glass Power diodesInformation provided by SCHOTT AG.
CTE, linear 4.40 µm/m-°C
<br>@Temperature 25.0 - 100 °C
2.44 µin/in-°F
<br>@Temperature 77.0 - 212 °F
ASTM E831
M Cubed Technologies HSC-702 Aluminum-toughened Reaction Bonded Silicon Carbide
High fracture tougness reaction bonded SiC. Used in applications that require both high wear and high impact resistance. Bullnoses, fan liners, hydrocyclone liners, etc.Information provided by M C..
CTE, linear 4.40 µm/m-°C
<br>@Temperature 20.0 °C
2.44 µin/in-°F
<br>@Temperature 68.0 °F
Zircar Refractory Composites RS-101 Refractory Sheet
ZRCI Refractory Sheet Type RS-101 is a ceramic fiber reinforced structural alumina product with useful properties to 2300°F (1260°C). It retains strength and utility to levels far exceeding maximu..
CTE, linear 4.40 µm/m-°C
<br>@Temperature 25.0 - 1000 °C
2.44 µin/in-°F
<br>@Temperature 77.0 - 1830 °F
ASTM C372
CoorsTek Direct Sintered Silicon Carbide, SC DS (SC-30, UltraSiC™)
Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
CTE, linear 4.40 µm/m-°C
<br>@Temperature 25.0 - 1000 °C
2.44 µin/in-°F
<br>@Temperature 77.0 - 1830 °F
ASTM C372
CoorsTek SC-DSG (SC-35) Graphite Loaded Sintered Silicon Carbide
Thermal Shock Delta Tc = 600°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
CTE, linear 4.40 µm/m-°C
<br>@Temperature 0.000 - 300 °C
2.44 µin/in-°F
<br>@Temperature 32.0 - 572 °F
Corning 1724 Aluminosilicate Crushed/Powdered Glass
Available in mesh sizes 4 through 325 and can be customized. Used for sealing and other applications.Information provided by Corning Incorporated.
CTE, linear 4.40 µm/m-°C
<br>@Temperature 1000 °C
2.44 µin/in-°F
<br>@Temperature 1830 °F
Chosun Refractories SBSN-CT Tube
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 4.40 µm/m-°C
<br>@Temperature 1000 °C
2.44 µin/in-°F
<br>@Temperature 1830 °F
Chosun Refractories SSB-1 Bricks, Reaction Bonded SiC
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).