Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 4.56 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
CTE, linear 8.20 µm/m-°C
4.56 µin/in-°F
at Set Pt. (Fired Thermal Expansion)
Ferro CF 7583 Low-Temperature Sealing
DEVITRIFYING Typical Powder Form: TF Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific t..
CTE, linear 8.20 µm/m-°C

@Temperature 260 °C
4.56 µin/in-°F

@Temperature 500 °F
Fired Thermal Expansion
Ferro CF 7583 Low-Temperature Sealing
DEVITRIFYING Typical Powder Form: TF Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific t..
CTE, linear 8.20 µm/m-°C

@Temperature 260 °C
4.56 µin/in-°F

@Temperature 500 °F
Ferro EG 2927 Metal Sealing
Glass Type: Sr-B-Al Typical Powder Form: VSD Typical Application: Comp. - Battery Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched ..
CTE, linear 8.20 µm/m-°C

@Temperature 20.0 °C
4.56 µin/in-°F

@Temperature 68.0 °F
Sapco 98% Aluminum Oxide
Information provided by Sapco.
CTE, linear 8.20 µm/m-°C

@Temperature 25.0 - 1000 °C
4.56 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM C372
CoorsTek AD-94 Alumina (nom. 94% Al2O3)
Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
CTE, linear 8.20 µm/m-°C

@Temperature 25.0 - 1000 °C
4.56 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM C372
CoorsTek AD-96 Alumina (nom. 96% Al2O3)
Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
CTE, linear 8.20 µm/m-°C

@Temperature 25.0 - 1000 °C
4.56 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM C372
CoorsTek AD-995 Alumina (nom. 99.5% Al2O3)
Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
CTE, linear 8.20 µm/m-°C

@Temperature 25.0 - 1000 °C
4.56 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM-C372
CoorsTek AD-996 99.6% Alumina
CTE, linear 8.20 µm/m-°C

@Temperature 25.0 - 1000 °C
4.56 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM C372
CoorsTek AD-998 Alumina(nom. 99.8% Al2O3)
Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
CTE, linear 8.20 µm/m-°C

@Temperature 25.0 - 1000 °C
4.56 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM-C372
CoorsTek ADD-96 96% Alumina
CTE, linear 8.20 µm/m-°C

@Temperature 25.0 - 1000 °C
4.56 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM-C372
CoorsTek CAP 3 99.5% Alumina Ceramic Armor Material
CoorsTek CeraShield™ ceramics provide: low weight, high hardness, controlled, uniform microstructure, dimensional stability over wide temperature range, compatibility for use in finished armor sys..
CTE, linear 8.20 µm/m-°C

@Temperature 25.0 - 1000 °C
4.56 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM-C372
CoorsTek CAP 4 98.5% Alumina Ceramic Armor Material
CoorsTek CeraShield™ ceramics provide: low weight, high hardness, controlled, uniform microstructure, dimensional stability over wide temperature range, compatibility for use in finished armor sys..
CTE, linear 8.20 µm/m-°C

@Temperature 25.0 - 1000 °C
4.56 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM-C372
CoorsTek FG-98 98% Alumina Ceramic Armor Material
CoorsTek CeraShield™ ceramics provide: low weight, high hardness, controlled, uniform microstructure, dimensional stability over wide temperature range, compatibility for use in finished armor sys..
CTE, linear 8.20 µm/m-°C

@Temperature 25.0 - 1000 °C
4.56 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM C372
CoorsTek FG-995 Alumina (nom. 98.5% Al2O3)
Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
CTE, linear 8.20 µm/m-°C

@Temperature 25.0 - 1000 °C
4.56 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM C372
CoorsTek PlasmaPure™ Alumina (nom. 99.8% Al2O3)
Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
CTE, linear 8.20 µm/m-°C

@Temperature 25.0 - 1000 °C
4.56 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM-C372
CoorsTek PlasmaPure-UC™ 99.9% Alumina
CTE, linear 8.20 µm/m-°C

@Temperature 25.0 - 1000 °C
4.56 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM-C372
CoorsTek Z-PLUS™ 94 Zirconia-Impr. Alumina Ceramic Armor Material
CoorsTek CeraShield™ ceramics provide: low weight, high hardness, controlled, uniform microstructure, dimensional stability over wide temperature range, compatibility for use in finished armor sys..
CTE, linear 8.20 µm/m-°C

@Temperature 20.0 - 650 °C
4.56 µin/in-°F

@Temperature 68.0 - 1200 °F
Du-Co Ceramics DC-10-L-3 Steatite
Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company.
CTE, linear 8.20 µm/m-°C

@Temperature 25.0 - 1000 °C
4.56 µin/in-°F

@Temperature 77.0 - 1830 °F
Astro Met AmAlOx 68 Alumina - Aluminum Oxide
General Description:AmAlOx 68 alumina (Astro Met Aluminum Oxide) is a high purity 99.8% aluminum oxide (alumina) ceramic which has been developed and optimized for maximum wear resistance and corros..
CTE, linear 8.20 µm/m-°C

@Temperature 20.0 - 1000 °C
4.56 µin/in-°F

@Temperature 68.0 - 1830 °F
Ceradyne Ceralloy® 225 Titanium Diboride
Features:electrical conductancewear resistancehardnessApplications:wear componentsballistic armorsputtering targetsInformation provided by Ceradyne Company
CTE, linear 8.20 µm/m-°C
4.56 µin/in-°F
Poco Graphite TM Industrial Grade Graphite
POCO’s specialty graphite materials are used in a wide range of highly technical and industrial applications. Each grade has characteristics and properties that allow the user to match the ideal gr..
Copyright © lookpolymers.com All Rights Reserved