| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 3.60 - 72.0 µm/m-°C | 2.00 - 40.0 µin/in-°F | Average value: 25.9 µm/m-°C Grade Count:38 |
|
Overview of materials for Polycarbonate, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v..
|
|||
| CTE, linear | 50.0 - 72.0 µm/m-°C | 27.8 - 40.0 µin/in-°F | Average value: 63.5 µm/m-°C Grade Count:3 |
|
Overview of materials for Nylon 11 with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are includ..
|
|||
| CTE, linear |
72.0
-
72.0
µm/m-°C @Temperature 0.000 - 156 °C |
40.0
-
40.0
µin/in-°F @Temperature 32.0 - 312 °F |
Average value: 72.0 µm/m-°C Grade Count:1 |
|
Overview of materials for Acrylic, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
|
|||
| CTE, linear |
72.0
-
72.0
µm/m-°C @Temperature 0.000 - 156 °C |
40.0
-
40.0
µin/in-°F @Temperature 32.0 - 312 °F |
Average value: 72.0 µm/m-°C Grade Count:2 |
|
Overview of materials for Acrylic, UV Stabilized, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, UV Stabilized, Molded". Each property range of values reported is minimum and maximum values of..
|
|||
| CTE, linear | 17.0 - 72.0 µm/m-°C | 9.44 - 40.0 µin/in-°F | Average value: 23.9 µm/m-°C Grade Count:24 |
|
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are..
|
|||
| CTE, linear |
72.0
-
72.0
µm/m-°C @Temperature 0.000 - 156 °C |
40.0
-
40.0
µin/in-°F @Temperature 32.0 - 312 °F |
Average value: 72.0 µm/m-°C Grade Count:2 |
|
Overview of materials for Acrylic, Optical Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of..
|
|||