Polymer Property : CTE, linear = 5.00 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
CTE, linear 5.00 µm/m-°C
2.78 µin/in-°F
Zircar Zirconia Buster M-15 Alumina Boards, Discs & Cylinders Insulation
Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite..
CTE, linear 5.00 µm/m-°C
<br>@Temperature 20.0 °C
2.78 µin/in-°F
<br>@Temperature 68.0 °F
Zircar Zirconia Buster M2-35 Alumina Boards, Discs & Cylinders Insulation
Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite..
CTE, linear 5.00 µm/m-°C
<br>@Temperature 20.0 °C
2.78 µin/in-°F
<br>@Temperature 68.0 °F
Zircar Zirconia M-45 Alumina Boards, Discs & Cylinders Insulation
Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite..
CTE, linear 5.00 µm/m-°C
2.78 µin/in-°F
DIN 53752
Lehmann & Voss LUVOCOM® 1114-8364 PAEK, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Good friction and wear behaviour especially at increased temperatures.Electrically conduct..
CTE, linear 5.00 µm/m-°C
2.78 µin/in-°F
at Set Pt.
Ferro EG 2410 Specialty Glass
Glass Type: Si-MG-Al Typical Powder Form: MVG Typical Application: Sintering Aid / Glaze Ferro offers a wide range of compositions for specialty applications including sintering aids used in the gl..
CTE, linear 5.00 µm/m-°C
<br>@Temperature 20.0 - 300 °C
2.78 µin/in-°F
<br>@Temperature 68.0 - 572 °F
ISO 7991
Schott Glass 8250 Borosilicate Glass
Borosilicate glass for sealing to Kovar metal and molybdenum, electrically highly insulating, low refractive index, good insulator X-ray tubes, transmitting tubes, image amplifier tubes, He-Ne-lase..
CTE, linear 5.00 µm/m-°C
<br>@Temperature 20.0 - 300 °C
2.78 µin/in-°F
<br>@Temperature 68.0 - 572 °F
ISO 7991
Schott Glass 8270 Borosilicate Glass
Borosilicate glass for sealing to Kovar metal and molybdenum, electrically highly insulating, defined UV absorption, stabilized against solarization Backlights The heavy metal content for the elem..
CTE, linear 5.00 µm/m-°C
<br>@Temperature -30.0 - 70.0 °C
2.78 µin/in-°F
<br>@Temperature -22.0 - 158 °F
Schott GM39923 Dental Glass
Remarks: Ba- and F-containing, low refractive glassApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Provide..
CTE, linear 5.00 µm/m-°C
<br>@Temperature 20.0 - 1000 °C
2.78 µin/in-°F
<br>@Temperature 68.0 - 1830 °F
Goodfellow Alumino-silicate Glass Ceramic
SiO2 57/Al2O3 36/CaO/MgO/BaOPorous ceramics can be used as filters and for the controlled release of volatile chemicals. In this material, Alumino-Silicate particles are found in a glassy matrix. Th..
CTE, linear 5.00 µm/m-°C
<br>@Temperature 20.0 - 1000 °C
2.78 µin/in-°F
<br>@Temperature 68.0 - 1830 °F
Zircar Ceramics AL-30 Alumina Insulation
AL-30 and AL-30AA are rigid alumina fiber boards characterized by uniform open porosity and high machinability. Alumina bonded AL-30AA is used in fuel cell reformers.Information provided by Zircar C..
CTE, linear 5.00 µm/m-°C
2.78 µin/in-°F
Zircar Zirconia Buster M-15 Alumina Boards, Discs & Cylinders Insulation
Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite..
CTE, linear 5.00 µm/m-°C
2.78 µin/in-°F
In Plane; ASTM E289-95
Hexcel® HexTOOL™ M81 Multi-Axial High Temperature Epoxy Tooling Compound
HexTOOL™ M81 Tooling Compound is randomly layered strips of uni-directional prepreg which is consolidated into rolled goods. It can be utilized as multi-ply quasi-isotropic hand lay-up, and subsequ..
CTE, linear 5.00 µm/m-°C
<br>@Temperature 20.0 - 1000 °C
2.78 µin/in-°F
<br>@Temperature 68.0 - 1830 °F
Zircar Ceramics ZAL-45 Alumina Insulation
ZAL-45 is an exceptionally strong low density alumina fiber product. Alumina bonded ZAL-45AA is useful in reducing conditions.Information provided by Zircar Ceramics.
CTE, linear 5.00 µm/m-°C
<br>@Temperature 1000 °C
2.78 µin/in-°F
<br>@Temperature 1830 °F
Chosun Refractories AH-3 Acid-Proof and Heat-Resistant Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 5.00 µm/m-°C
<br>@Temperature 1000 °C
2.78 µin/in-°F
<br>@Temperature 1830 °F
Chosun Refractories AH-5 Acid-Proof and Heat-Resistant Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 5.00 µm/m-°C
<br>@Temperature 1000 °C
2.78 µin/in-°F
<br>@Temperature 1830 °F
Chosun Refractories BATN-D2, Lower Gas Purging Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 5.00 µm/m-°C
<br>@Temperature 1000 °C
2.78 µin/in-°F
<br>@Temperature 1830 °F
Chosun Refractories SF31 Hard Fireclay brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 5.00 µm/m-°C
<br>@Temperature 20.0 °C
2.78 µin/in-°F
<br>@Temperature 68.0 °F
Parallel DOM
Alliance N-28EH Neodymium Iron Boron Magnetic Material
CTE, linear 5.00 µm/m-°C
<br>@Temperature 20.0 °C
2.78 µin/in-°F
<br>@Temperature 68.0 °F
Parallel DOM
Alliance N-35 Neodymium Iron Boron Magnetic Material
CTE, linear 5.00 µm/m-°C
<br>@Temperature 20.0 °C
2.78 µin/in-°F
<br>@Temperature 68.0 °F
Parallel DOM
Alliance N-35M Neodymium Iron Boron Magnetic Material
CTE, linear 5.00 µm/m-°C
<br>@Temperature 20.0 °C
2.78 µin/in-°F
<br>@Temperature 68.0 °F
Parallel DOM
Alliance N-35SH Neodymium Iron Boron Magnetic Material
CTE, linear 5.00 µm/m-°C
<br>@Temperature 20.0 °C
2.78 µin/in-°F
<br>@Temperature 68.0 °F
Parallel DOM
Alliance N-50 Neodymium Iron Boron Magnetic Material
CTE, linear 5.00 µm/m-°C
<br>@Temperature 20.0 - 1000 °C
2.78 µin/in-°F
<br>@Temperature 68.0 - 1830 °F
Anderman Ceramics EC70P Mullite-Bonded Porous Silicon Carbide (70%)
Excellent thermal shock properties when in contact with molten metal. Available as tube, sheath, or rod up to 7.2 ft (2.2 m) long with diameters 0.6" to 4.7".Information provided by Anderman Cerami..
CTE, linear 5.00 µm/m-°C
<br>@Temperature 20.0 - 1000 °C
2.78 µin/in-°F
<br>@Temperature 68.0 - 1830 °F
Anderman Ceramics EC90P Mullite-Bonded Porous Silicon Carbide (90%)
Excellent thermal shock properties and thermal conductivity when in contact with molten metal. Available as tube, sheath, or rod up to 6 ft (1.9 m) long with diameters 0.6" to 3.75".Information pro..
CTE, linear 5.00 µm/m-°C
<br>@Temperature 20.0 - 1000 °C
2.78 µin/in-°F
<br>@Temperature 68.0 - 1830 °F
Ceradyne Ceralloy® 137 CA AlN Composite
Applications: cryogenic environment applicationsterminationssever wedgesload pelletsabsorbersFeatures: dielectric loss independent from temperature.Information provided by Ceradyne Company
CTE, linear 5.00 µm/m-°C
<br>@Temperature 20.0 °C
2.78 µin/in-°F
<br>@Temperature 68.0 °F
Parallel DOM
Alliance N-33H Neodymium Iron Boron Magnetic Material
CTE, linear 5.00 µm/m-°C
<br>@Temperature 20.0 °C
2.78 µin/in-°F
<br>@Temperature 68.0 °F
Parallel DOM
Alliance N-42H Neodymium Iron Boron Magnetic Material
CTE, linear 5.00 µm/m-°C
<br>@Temperature 1000 °C
2.78 µin/in-°F
<br>@Temperature 1830 °F
Chosun Refractories H-4S High Alumina brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).