| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear |
60.0
-
100
µm/m-°C @Temperature 20.0 °C |
33.3
-
55.6
µin/in-°F @Temperature 68.0 °F |
DN.53752 |
|
Polimersan Plastics POLIPA® (PA 6) Polyamide
POLIPA® PA6 (POLYAMIDE) is produced by poly condensation of e-aminoacid and by the help of d-carbon acid and d-amine poly condensation. Its characteristics depend upon the numbers of the main struc..
|
|||
| CTE, linear | 80.0 - 100 µm/m-°C | 44.4 - 55.6 µin/in-°F | Polykemi |
|
Polykemi AB POLYfill PP CQX10030 R3 Polypropylene, Mineral Reinforced, Scratch Resistant
Information provided by Polykemi AB
|
|||
| CTE, linear | 80.0 - 100 µm/m-°C | 44.4 - 55.6 µin/in-°F | Polykemi |
|
Polykemi AB POLYfill PP CQX8025 R2 Polypropylene, Mineral Reinforced, Scratch Resistant
Information provided by Polykemi AB
|
|||
| CTE, linear |
50.0
-
100
µm/m-°C @Temperature 20.0 °C |
27.8
-
55.6
µin/in-°F @Temperature 68.0 °F |
Cured |
|
Resin Technology Group EN 239-2 Cationic UV Cure Epoxy Adhesive
EN 239-2 is an epoxy-based, medium viscosity, cationic- curable adhesive/sealant. This product is activated by exposure to medium intensity UV radiation resulting in a high strength, chemical resist..
|
|||
| CTE, linear |
23.0
-
100
µm/m-°C @Temperature >=162 °C |
12.8
-
55.6
µin/in-°F @Temperature >=324 °F |
Average value: 61.5 µm/m-°C Grade Count:1 |
|
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled". Each property range of values reported i..
|
|||
| CTE, linear | 43.0 - 100 µm/m-°C | 23.9 - 55.6 µin/in-°F | Average value: 67.8 µm/m-°C Grade Count:5 |
|
Overview of materials for PETG Copolyester
This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M..
|
|||
| CTE, linear | 50.0 - 100 µm/m-°C | 27.8 - 55.6 µin/in-°F | Average value: 68.4 µm/m-°C Grade Count:25 |
|
Overview of materials for Polyphenylene Ether, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap..
|
|||
| CTE, linear | 30.0 - 100 µm/m-°C | 16.7 - 55.6 µin/in-°F | Average value: 58.6 µm/m-°C Grade Count:15 |
|
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar..
|
|||
| CTE, linear | 62.0 - 100 µm/m-°C | 34.4 - 55.6 µin/in-°F | Average value: 74.0 µm/m-°C Grade Count:33 |
|
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
|
|||
| CTE, linear | 48.6 - 100 µm/m-°C | 27.0 - 55.6 µin/in-°F | Average value: 77.2 µm/m-°C Grade Count:10 |
|
Overview of materials for Polypropylene with 30% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are..
|
|||
| CTE, linear | 10.0 - 100 µm/m-°C | 5.56 - 55.6 µin/in-°F | Average value: 70.9 µm/m-°C Grade Count:42 |
|
Overview of materials for Nylon 66, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum ..
|
|||
| CTE, linear | 65.0 - 100 µm/m-°C | 36.1 - 55.6 µin/in-°F | ASTM D696 |
|
Guarniflon PTFE G455 Polytetrafluoroethylene 35% Carbographite
PTFE G Special Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high w..
|
|||
| CTE, linear | 80.0 - 100 µm/m-°C | 44.4 - 55.6 µin/in-°F | 25°C to 100°C; ASTM D696 |
|
Guarniflon FEP Fluorinated Ethylene Propylene
Fluorinated thermoplastic material with excellent thermal, electrical and chemical inertness properties. Widely used for different industrial applications for its excellent chemical resistance up t..
|
|||
| CTE, linear |
70.0
-
100
µm/m-°C @Temperature 20.0 - 100 °C |
38.9
-
55.6
µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
|
Schwartz Technical Plastics LAMIGAMID® 100 Polyamide 6, Extruded, Conditioned
Application: machine parts under 80 mm diameter, hammer-heads, cup-shaped bearing shellsInformation provided by Schwartz Technical Plastics GmbH
|
|||
| CTE, linear |
70.0
-
100
µm/m-°C @Temperature 20.0 - 100 °C |
38.9
-
55.6
µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
|
Schwartz Technical Plastics LAMIGAMID® 100 Polyamide 6, Extruded, Dry
Application: machine parts under 80 mm diameter, hammer-heads, cup-shaped bearing shellsInformation provided by Schwartz Technical Plastics GmbH
|
|||
| CTE, linear |
80.0
-
100
µm/m-°C @Temperature 20.0 - 100 °C |
44.4
-
55.6
µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
|
Schwartz Technical Plastics LAMIGAMID® 1200 Cast Polyamide 12, Dry
Application: sprockets, chain-wheels, pulleys, wheels, slide and seal rings, curve disks, etc.Information provided by Schwartz Technical Plastics GmbH
|
|||
| CTE, linear | 80.0 - 100 µm/m-°C | 44.4 - 55.6 µin/in-°F | ISO 11359 |
|
Styrolution Novodur® BX13036 ABS + PMMA
Novodur BX13036 is a new PMMA/ABS blend with high surface quality, enhanced scratch resistance and balanced mechanical propertiesInformation provided by Styrolution
|
|||
| CTE, linear |
80.0
-
100
µm/m-°C @Temperature -30.0 - 30.0 °C |
44.4
-
55.6
µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
|
SABIC Innovative Plastics NORYL GTX GTX6011 PPE+PA6 (Asia Pacific)
PA6 based unfilled GTX. High impact.
|
|||
| CTE, linear |
70.0
-
100
µm/m-°C @Temperature 20.0 °C |
38.9
-
55.6
µin/in-°F @Temperature 68.0 °F |
DIN 53752 |
|
Zell-Metall Engineering Plastics Zellamid 202 (PA 6)
Zellamid® 202 is a tough material with high resistance to abrasion and impact. It features good mechanical properties. By water absorption the excellent shock and vibration resistance is increased...
|
|||
| CTE, linear |
70.0
-
100
µm/m-°C @Temperature 20.0 °C |
38.9
-
55.6
µin/in-°F @Temperature 68.0 °F |
DIN 53752 |
|
Zell-Metall Engineering Plastics Zellamid 250 (PA6.6)
Zellamid® 250 is noted for its high temperature resistance and high tensile strength. It is the hardest and most rigid type of extruded Nylon. Main characteristics are high resistance to fuels, oil..
|
|||
| CTE, linear |
95.0
-
100
µm/m-°C @Temperature 20.0 °C |
52.8
-
55.6
µin/in-°F @Temperature 68.0 °F |
|
|
Abatron AboCast/AboCure 8109-4
Safety hardener (minimum toxicity) version of 8109-3.Processing: 100/10 pbw; Potlife: 2.5 h/20°C (68°F), 30 min/40°C (105°F), 15 min/60°C (140°F); mix at RT; cures in: 24 h/20°C (68°F), 2-3 ..
|
|||
| CTE, linear | 30.0 - 100 µm/m-°C | 16.7 - 55.6 µin/in-°F | Average value: 73.7 µm/m-°C Grade Count:34 |
|
Overview of materials for Nylon 6, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v..
|
|||
| CTE, linear | 80.0 - 100 µm/m-°C | 44.4 - 55.6 µin/in-°F | Average value: 85.0 µm/m-°C Grade Count:14 |
|
Overview of materials for Nylon 6, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat..
|
|||
| CTE, linear | 52.2 - 100 µm/m-°C | 29.0 - 55.6 µin/in-°F | Average value: 70.1 µm/m-°C Grade Count:4 |
|
Overview of materials for Nylon 66, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu..
|
|||
| CTE, linear |
100
-
100
µm/m-°C @Temperature -90.0 - -30.0 °C |
55.6
-
55.6
µin/in-°F @Temperature -130 - -22.0 °F |
Average value: 100 µm/m-°C Grade Count:1 |
|
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Crosslinkable". Each property range of values reported is minimum and ..
|
|||
| CTE, linear | 70.0 - 100 µm/m-°C | 38.9 - 55.6 µin/in-°F | Average value: 81.3 µm/m-°C Grade Count:16 |
|
Overview of materials for Nylon 6, MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria..
|
|||
| CTE, linear | 50.0 - 100 µm/m-°C | 27.8 - 55.6 µin/in-°F | Average value: 79.7 µm/m-°C Grade Count:13 |
|
Overview of materials for Polystyrene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a..
|
|||
| CTE, linear |
10.0
-
100
µm/m-°C @Temperature -100 - 250 °C |
5.56
-
55.6
µin/in-°F @Temperature -148 - 482 °F |
Average value: 21.2 µm/m-°C Grade Count:23 |
|
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a..
|
|||
| CTE, linear |
7.00
-
100
µm/m-°C @Temperature 55.0 - 250 °C |
3.89
-
55.6
µin/in-°F @Temperature 131 - 482 °F |
Average value: 20.4 µm/m-°C Grade Count:19 |
|
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are..
|
|||
| CTE, linear |
100
-
100
µm/m-°C @Temperature 100 - 100 °C |
55.6
-
55.6
µin/in-°F @Temperature 212 - 212 °F |
Average value: 100 µm/m-°C Grade Count:1 |
|
Overview of materials for Polypropylene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of..
|
|||