Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 6.00 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
CTE, linear 6.00 µm/m-°C

@Thickness 1.00 mm,
Temperature -125 - 20.0 °C
3.33 µin/in-°F

@Thickness 0.0394 in,
Temperature -193 - 68.0 °F
ASTM E831-06
NeXolve Novastrat® 800 Polyimide
High temperature polyimide film with low coefficient of thermal expansion.NeXolve Novastrat® 800 is a high temperature polyimide film with low coefficient of thermal expansion (CTE), ~4 ppm/°C fro..
CTE, linear 6.00 - 48.0 µm/m-°C
3.33 - 26.7 µin/in-°F
Average value: 28.7 µm/m-°C Grade Count:3
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. ..
CTE, linear 6.00 µm/m-°C

@Temperature 23.0 °C
3.33 µin/in-°F

@Temperature 73.4 °F
MD; ASTM D696
Mitsui AURUM® JCN6230 Thermoplastic Polyimide Resin, Crystalline  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
CTE, linear 6.00 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
3.33 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis; IPC-TM 650-2.4.24
Industrial Laminates/Norplex NP555 Carbon Fiber  (discontinued **)
Description: NP555 is composed of carbon fiber fabric and a phenolic resin system. It has excellent moisture resistance and physical properties. This material was designed to replace asbestos vane m..
CTE, linear 6.00 - 73.8 µm/m-°C
3.33 - 41.0 µin/in-°F
Average value: 50.9 µm/m-°C Grade Count:41
Overview of materials for Nylon 66, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..
CTE, linear 6.00 - 25.0 µm/m-°C
3.33 - 13.9 µin/in-°F
Average value: 16.4 µm/m-°C Grade Count:8
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in..
CTE, linear 6.00 µm/m-°C

@Temperature 20.0 °C
3.33 µin/in-°F

@Temperature 68.0 °F
MarkeTech Strontium Lanthanum Galate (SrLaGaO3) Single Crystal Substrate
Data provided by the supplier, MarkeTech International.Used as a substrate for deposition of high temperature oxide superconductors.
CTE, linear 6.00 µm/m-°C

@Temperature 30.0 - 300 °C
3.33 µin/in-°F

@Temperature 86.0 - 572 °F
Mo-Sci Corporation GL-0271 E-Glass Spheres
Appearance: Solid low alkali E-glass beads with greenish color.Chemical Durability: Weight loss @ 90°C for 24 hrs in 5% HCl 0.3 mg/cm2Information provided by Mo-Sci Corporation.
CTE, linear 6.00 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.33 µin/in-°F

@Temperature -22.0 - 158 °F
Schott G018-161 Dental Glass
Remarks: Extremely high radioopacity, Zr containingApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Provide..
CTE, linear 6.00 µm/m-°C

@Temperature 20.0 - 400 °C
3.33 µin/in-°F

@Temperature 68.0 - 752 °F
Zircar Refractory Composites RS-100 Refractory Sheet
ZIRCAR Refractory Sheet Type RS-100 is a ceramic fiber reinforced structural alumina composite material with useful properties to 1260°C (2300°F). It has exceptional flexural and compressive stren..
CTE, linear 6.00 µm/m-°C

@Temperature 1000 °C
3.33 µin/in-°F

@Temperature 1830 °F
Chosun Refractories BP-95A Gas Purging Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 6.00 - 7.00 µm/m-°C

@Temperature 1000 °C
3.33 - 3.89 µin/in-°F

@Temperature 1830 °F
Chosun Refractories BPSC-95 Gas Purging Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 6.00 µm/m-°C

@Temperature 1000 °C
3.33 µin/in-°F

@Temperature 1830 °F
Chosun Refractories SF32 Hard Fireclay brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 6.00 µm/m-°C

@Temperature 1000 °C
3.33 µin/in-°F

@Temperature 1830 °F
Chosun Refractories SF-S Hard Fireclay brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 6.00 µm/m-°C
3.33 µin/in-°F
COI Ceramics Nextel™ A-N720 Oxide Ceramic Matrix Composite, Alumina
Description: Oxide ceramic matrix composites products are based upon sol-gel derived matrices and 3M Corporation's Nextel™ fiber products. These materials can be used up to 1200ºC (2200ºF) in air..
CTE, linear 6.00 µm/m-°C

@Temperature 20.0 - 1093 °C
3.33 µin/in-°F

@Temperature 68.0 - 1999 °F
BNZ Materials Zelieblok 1900S Structural Ceramic Insulation
Information provided by BNZ Materials Inc.
CTE, linear 6.00 µm/m-°C

@Temperature 20.0 - 1093 °C
3.33 µin/in-°F

@Temperature 68.0 - 1999 °F
BNZ Materials Zelieblok 2000S Structural Ceramic Insulation
Information provided by BNZ Materials Inc.
CTE, linear 6.00 - 9.00 µm/m-°C
3.33 - 5.00 µin/in-°F
IPC TM-650 2.4.41
Arlon 85NT Polyimide Nonwoven Aramid Laminate and Prepreg
85NT is a pure polyimide laminate and prepreg system (Tg = 250°C), reinforced with a non-woven aramid substrate. This system combines the high-reliability features of polyimide (improved PTH relia..
CTE, linear 6.00 µm/m-°C

@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
3.33 µin/in-°F

@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Dry as Molded
Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent ..
CTE, linear 6.00 µm/m-°C

@Temperature 100 - 1100 °C
3.33 µin/in-°F

@Temperature 212 - 2010 °F
3M Nextel™ XN-625 Woven Fabric 720
Information provided by 3M
CTE, linear 6.00 µm/m-°C

@Temperature 20.0 °C
3.33 µin/in-°F

@Temperature 68.0 °F
ATI Wah Chang Zirconium Alloy Zircaloy-4
Zirconium resists corrosive attack in most organic and mineral acids, strong alkalis, and some molten salts. A tightly adherent and protective oxide film protects the metal-oxide interface to provid..
CTE, linear 6.00 µm/m-°C
3.33 µin/in-°F
at Set Pt.
Ferro EG 2800 Metal Sealing
Glass Type: CA-Si-B Typical Powder Form: VSD Typical Application: TA 23 Battery Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched se..
Copyright © lookpolymers.com All Rights Reserved