Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 65.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
CTE, linear 65.0 µm/m-°C

@Temperature 20.0 °C
36.1 µin/in-°F

@Temperature 68.0 °F
DIN 53328
Polycasa PC
QUINN PC sheets have excellent optical properties and a brilliant surface. The QUINN PC range contains sheets that are easy to fabricate and show exceptional performance at both low and high tempera..
CTE, linear 65.0 µm/m-°C
36.1 µin/in-°F
Polykemi
Polykemi AB POLYelast TPE HJ-75 UV Thermoplastic Elastomer, PP/Elastomer/Mineral, UV-Stabilized, Low CLTE
Information provided by Polykemi AB
CTE, linear 65.0 µm/m-°C
36.1 µin/in-°F
Z-Direction; IPC-TM-650 2.4.41
Rogers Corporation RO3730 Antenna Grade Laminate
RO3730™ Laminates have the excellent thermo-mechanical properties and electrical characteristics that antenna designers need. The laminates have a dielectric constant of 3.0 and a loss tangent of..
CTE, linear 65.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
36.1 µin/in-°F

@Temperature -22.0 - 176 °F
ASTM E228
Solvay Engineered Polymers SEQUEL® 1440LS TPO  (discontinued **)
Description: SEQUEL® 1440LS engineered polyolefin material is designed for large automotive exterior applications that require ductile impact properties at low temperatures, excellent processabilit..
CTE, linear 65.0 - 80.0 µm/m-°C
36.1 - 44.4 µin/in-°F
Average value: 73.8 µm/m-°C Grade Count:29
Overview of materials for Polyphenylene Ether, Heat Resistant
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Heat Resistant". Each property range of values reported is minimum and maximum valu..
CTE, linear 65.0 µm/m-°C

@Temperature 23.0 - 100 °C
36.1 µin/in-°F

@Temperature 73.4 - 212 °F
Quadrant EPP Quadrant PC 1000 extruded (ISO Data)
Quadrant Engineering Plastic Products is marketing non-UV-stabilized polycarbonate stock shapes under the trade name Quadrant PC 1000. It is a natural, “non-optical” industrial quality (clear, tra..
CTE, linear 65.0 µm/m-°C
36.1 µin/in-°F
DIN 52328
Isoflon PC Polycarbonate
Good impact resistance among transparent materialsInformation provided by Isoflon.
CTE, linear 65.0 µm/m-°C

@Temperature -40.0 - 35.0 °C
36.1 µin/in-°F

@Temperature -40.0 - 95.0 °F
ASTM D696
MRC Polymers NAXELLâ„¢ PC23MS Polycarbonate, Impact Modified, High MFR, EZ Flow
Economy GradeImpact modifiedCan be UV stabilizedGenerally for black onlyInternal and external lubricant can be addedInformation provided by MRC Polymers Inc.
CTE, linear 65.0 µm/m-°C

@Temperature -40.0 - 35.0 °C
36.1 µin/in-°F

@Temperature -40.0 - 95.0 °F
ASTM D696
MRC Polymers NAXELLâ„¢ PC429HHI Polycarbonate, Impact Modified, High MFR, EZ Flow
Good Property RetentionHeat and Dimensional StabilityHigh Melt Impact ModifiedMFR can be modified between 10 to 26 g/10minsCan be UV stabilizedGenerally for natural, colorable and can go blackIntern..
CTE, linear 65.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
36.1 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics NORYL PX2637 PPE+HIPS (Asia Pacific)
CTE, linear 65.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
36.1 µin/in-°F

@Temperature -22.0 - 176 °F
Borealis Method
Borealis Borcom™ WE007AE Polypropylene
Borcom™ WE007AE is a polypropylene microcomposite intended for injection molding. The product is available in natural color. This material has an excellent balance between impact strength and stif..
CTE, linear 65.0 µm/m-°C
36.1 µin/in-°F
Master Bond EP21LV35Med Two Component, Flexible USP Class VI Epoxy System
Master Bond Polymer System EP21LV3/5Med is a two part, low viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulation and casting that cures flexible. It cures readil..
CTE, linear 65.0 - 70.0 µm/m-°C
36.1 - 38.9 µin/in-°F
Master Bond LED401LV One Component, Moderate Viscosity LED Curable System
Master Bond LED401LV is a very special, one part LED type system that will cure when exposed to a light source emitting 405 nm wavelength and where the presence of any UV light is minimal or inciden..
CTE, linear 65.0 µm/m-°C

@Temperature 40.0 - 130 °C
36.1 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Plenco 1500 Polyester, Granular, Compression Molded
PLENCO 01500 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance, and low post shrinkage characteristics. UL recognized under compon..
CTE, linear 65.0 µm/m-°C
36.1 µin/in-°F
ASTM D696
Unitika C300VN
Characteristics: Flame resistant, transparent (flame resistance: UL94 V0, 0.8 mm) High flowInformation provided by Unitika Ltd.
CTE, linear 65.0 µm/m-°C

@Temperature 20.0 °C
36.1 µin/in-°F

@Temperature 68.0 °F
ASTM D696
A. Schulman POLYTROPE™ TPP 518 Injection Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 518 is an injection grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal expansion i..
CTE, linear 65.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
36.1 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 53752
CP-Polymer-Technik Wellamid® 6000 MR 309 HWCP Mineral Nylon 6, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
CTE, linear 65.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
36.1 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 53752
CP-Polymer-Technik Wellamid® 6600 MR 309 HWCP 30% Mineral Nylon 66, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
CTE, linear 65.0 µm/m-°C

@Temperature 20.0 - 60.0 °C
36.1 µin/in-°F

@Temperature 68.0 - 140 °F
TMS2 Perkin Elmer
Arkema Group Orgalloy® RS 6600 Polyamide 6.6 Alloy
Polyamide Alloy, Rigid grade, Nylon 6.6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group
CTE, linear 65.0 µm/m-°C

@Temperature 20.0 °C
36.1 µin/in-°F

@Temperature 68.0 °F
ASTM E 831
Azoty Tarnow™ TARFLEN SM-B40 PTFE
Reinforced with 40% bronze for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
CTE, linear 65.0 µm/m-°C

@Temperature 20.0 °C
36.1 µin/in-°F

@Temperature 68.0 °F
Armstrong A-7 Epoxy Adhesive
Clear, flexible, 5-minute cure structural bonding plastic adhesive. Develops high performance, high impact durable bonds for operating temperatures from -65° to +250°. Supplied in 1:1 ratio dispe..
CTE, linear 65.0 µm/m-°C

@Temperature -30.0 - 60.0 °C
36.1 µin/in-°F

@Temperature -22.0 - 140 °F
ASTM D696
Asahi Kasei Xyron® SZ800 Modified Polyphenylene Ether
High-Heat ResistantInformation provided by Asahi Kasei
CTE, linear 65.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
36.1 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 53752
CP-Polymer-Technik Wellamid® 6600 MR 409 HWCP 40% Mineral Nylon 66, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
CTE, linear 65.0 µm/m-°C

@Temperature 20.0 °C
36.1 µin/in-°F

@Temperature 68.0 °F
ASTM D696
A. Schulman POLYTROPE™ TPP 518 Injection Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 518 is an injection grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal expansion i..
CTE, linear 65.0 µm/m-°C

@Temperature 20.0 °C
36.1 µin/in-°F

@Temperature 68.0 °F
ASTM E 831
Azoty Tarnow™ TARFLEN SM-B60 PTFE
Tarflen SM1 reinforced with 60% bronze for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
CTE, linear 65.0 µm/m-°C

@Temperature 20.0 °C
36.1 µin/in-°F

@Temperature 68.0 °F
ASTM E 831
Azoty Tarnow™ TARFLEN SM-K22G3 PTFE
Tarflen SM1 reinforced with 22% coke and 3% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
CTE, linear 65.0 µm/m-°C
36.1 µin/in-°F
Average value: 65.0 µm/m-°C Grade Count:9
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether + Styrene-Butadiene Blend". Each property range of values reported is minimum and ma..
CTE, linear 65.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
36.1 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics NORYL 115 PPE+HIPS (Asia Pacific)
PPE+PS, 115 oC HDT
CTE, linear 65.0 µm/m-°C

@Temperature 20.0 °C
36.1 µin/in-°F

@Temperature 68.0 °F
ISO 11359
CENTROPLAST CENTROCARB Polycarbonate
CENTROCARB is a transparent or semi-transparent plastic with high strength and impact resistance. It is dimensionally rigid and has very good electrical insulating properties. It is used in contain..