| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear |
7.00
µm/m-°C @Temperature 20.0 °C |
3.89
µin/in-°F @Temperature 68.0 °F |
|
|
Pyrotek Pyrite N-14 Refractory Board
Pyrotek N-14 is a fiberglass reinforced calcium silicate board specifically developed for the non-ferrous industry. The superior strength and unique formulation of Pyrotek N-14 makes it the preferr..
|
|||
| CTE, linear |
7.00
µm/m-°C @Temperature 20.0 - 30.0 °C |
3.89
µin/in-°F @Temperature 68.0 - 86.0 °F |
|
|
PCC-Advanced Forming Technology 70% AlSiC Metal Matrix Composite
AlSiC metal matrix composites are formed by pressure infiltrating molten aluminum into silicon carbide preforms. This method of casting is typically used in applications where solution requirements ..
|
|||
| CTE, linear | 7.00 - 25.0 µm/m-°C | 3.89 - 13.9 µin/in-°F | Average value: 15.7 µm/m-°C Grade Count:3 |
|
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%..
|
|||
| CTE, linear | 7.00 µm/m-°C | 3.89 µin/in-°F | DIN 53752 |
|
Lehmann & Voss LUVOCOM® 1105-7751 PEEK, with carbon fiber, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
|
|||
| CTE, linear |
7.00
µm/m-°C @Temperature 20.0 °C |
3.89
µin/in-°F @Temperature 68.0 °F |
|
|
MarkeTech WCu15 Tungsten Copper Alloy
Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st..
|
|||
| CTE, linear |
7.00
µm/m-°C @Temperature 20.0 °C |
3.89
µin/in-°F @Temperature 68.0 °F |
|
|
MMCC Cu/B4C Particulate Copper Matrix Composite
Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC).
|
|||
| CTE, linear |
7.00
µm/m-°C @Temperature 25.0 - 600 °C |
3.89
µin/in-°F @Temperature 77.0 - 1110 °F |
|
|
ICE Steatite L-5
Data provided by the manufacturer, International Ceramic Engineering.
|
|||
| CTE, linear |
7.00
µm/m-°C @Temperature 20.0 °C |
3.89
µin/in-°F @Temperature 68.0 °F |
|
|
Momentive Performance Materials Niobium Carbide (NbC) Coating
High temperature protective coating for graphite.TaC, NbC, and ZrC coatings resist chemical attack by corrosive liquids and gases at very high temperatures. They are finding increasing acceptance i..
|
|||
| CTE, linear |
7.00
µm/m-°C @Temperature 20.0 °C |
3.89
µin/in-°F @Temperature 68.0 °F |
|
|
Momentive Performance Materials Titanium Diboride/Boron Nitride Composite Vacuum Metallizing Boat
Intermetallic composites from Advanced Ceramics are used vacuum metallizing industry. These ceramics withstand higher operating temperatures, have lower moisture sensitivity, low thermal expansion..
|
|||
| CTE, linear | 7.00 µm/m-°C | 3.89 µin/in-°F | DIN 53752 |
|
Lehmann & Voss LUVOCOM® 1105-7041 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
|
|||
| CTE, linear |
7.00
µm/m-°C @Temperature 20.0 °C |
3.89
µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
|
Glastic Laminates/Shapes SG-200 Fiberglass-Reinforced Polyester Rod
Data provided by Glastic Corporation.A continuous-filament fiberglass-roving provides superior strength. Excellent thermal endurance - used to replace silicone rod.
|
|||
| CTE, linear | 7.00 µm/m-°C | 3.89 µin/in-°F | ISO 11359-2 |
|
Menzolit Menzolit® HPC 1200 Unsaturated Polyester UP
HPC 1200 is a special SMC for high strength applications. The glass level has been selected to combine mouldability with high strength and stiffness properties in orientation direction. The reinforc..
|
|||
| CTE, linear | 7.00 µm/m-°C | 3.89 µin/in-°F | ISO 11359-2 |
|
Menzolit Menzolit® HPC 1300 Unsaturated Polyester UP
HPC 1300 is a special SMC for high strength applications. The glass level has been selected to combine mouldability with high strength and stiffness properties in orientation direction. The reinforc..
|
|||
| CTE, linear |
7.00
µm/m-°C @Temperature 20.0 °C |
3.89
µin/in-°F @Temperature 68.0 °F |
|
|
Sapco C 220 Steatite
Information provided by Sapco.
|
|||
| CTE, linear |
7.00
µm/m-°C @Temperature 20.0 °C |
3.89
µin/in-°F @Temperature 68.0 °F |
|
|
Sapco C 221 Steatite
Information provided by Sapco.
|
|||
| CTE, linear |
7.00
µm/m-°C @Temperature 20.0 - 1000 °C |
3.89
µin/in-°F @Temperature 68.0 - 1830 °F |
|
|
Zircar Refractory Composites RS-99R Refractory Sheet
Type RS-99R boards are prefired and are unaffected by moisture. They stay rigid even if saturated with water.Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)
|
|||
| CTE, linear |
7.00
µm/m-°C @Temperature 20.0 °C |
3.89
µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
|
Eastman TiGlaze SV Copolyester
TiGLAZE SV copolyester is a specialty copolyester for the architectural glazing industry, designed to provide a unique balance of toughness, stiffness and material value. The material has a CC1 Ligh..
|
|||
| CTE, linear |
7.00
µm/m-°C @Temperature 1000 °C |
3.89
µin/in-°F @Temperature 1830 °F |
|
|
Chosun Refractories BPAP Gas Purging Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
|
|||
| CTE, linear |
7.00
µm/m-°C @Temperature 1000 °C |
3.89
µin/in-°F @Temperature 1830 °F |
|
|
Chosun Refractories GPB-2 Special brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
|
|||
| CTE, linear |
7.00
µm/m-°C @Temperature 1000 °C |
3.89
µin/in-°F @Temperature 1830 °F |
|
|
Chosun Refractories SAL90 Special High Alumina brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
|
|||
| CTE, linear |
7.00
µm/m-°C @Temperature 1000 °C |
3.89
µin/in-°F @Temperature 1830 °F |
|
|
Chosun Refractories SAL90C Special High Alumina brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
|
|||
| CTE, linear |
7.00
µm/m-°C @Temperature 1000 °C |
3.89
µin/in-°F @Temperature 1830 °F |
|
|
Chosun Refractories SAL90Z Special High Alumina brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
|
|||
| CTE, linear | 7.00 µm/m-°C | 3.89 µin/in-°F | y direction |
|
Arlon TC350 Glass, PTFE and Micro-Dispersed Ceramic
High Thermal Conductivity, Excellent Dielectric Constant Control and Phase Stability with TemperatureInformation provided by Arlon Materials for Electronics (MED).
|
|||
| CTE, linear |
7.00
µm/m-°C @Temperature 20.0 °C |
3.89
µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
|
Alliance S-20B Samarium Cobalt Magnetic Material |
|||
| CTE, linear |
7.00
µm/m-°C @Temperature 20.0 °C |
3.89
µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
|
Alliance S-22A Samarium Cobalt Magnetic Material |
|||
| CTE, linear |
7.00
µm/m-°C @Temperature 20.0 - 1000 °C |
3.89
µin/in-°F @Temperature 68.0 - 1830 °F |
|
|
Ceradyne Ceralloy® 2710 BeO-SiC
Applications:terminationssever wedgesload pelletsabsorbersFeatures: former industry standard for terminations etc.Information provided by Ceradyne Company
|
|||
| CTE, linear |
7.00
µm/m-°C @Temperature 20.0 °C |
3.89
µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
|
Alliance S-22B Samarium Cobalt Magnetic Material |
|||