| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear |
12.6
µm/m-°C @Temperature 20.0 °C |
7.00
µin/in-°F @Temperature 68.0 °F |
|
|
Polygon Polylube™ Fiber Series Epoxy Composite Bearings
Low friction coupled with high load carrying capacity are natural benefits. Teflon® superfilaments, which exhibit tensile strength twenty times greater than PTFE resins are integrated into the bea..
|
|||
| CTE, linear | 12.6 - 32.0 µm/m-°C | 7.00 - 17.8 µin/in-°F | Average value: 22.6 µm/m-°C Grade Count:12 |
|
Overview of materials for Epoxy, Encapsulating, Glass or Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Glass or Mineral Filled". Each property range of values reported is minimum and ma..
|
|||
| CTE, linear | 12.6 - 20.0 µm/m-°C | 7.00 - 11.1 µin/in-°F | Average value: 17.1 µm/m-°C Grade Count:5 |
|
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl..
|
|||
| CTE, linear |
12.6
µm/m-°C @Temperature 37.8 - 538 °C |
7.00
µin/in-°F @Temperature 100 - 1000 °F |
|
|
Meehanite HS Heat Resisting Cast Iron
Type HS compares very favorably from a strength standpoint with any heat resisting metal. Compositional adjustments are made to suit the exact service conditions. It machines easily and provides m..
|
|||
| CTE, linear | 12.6 µm/m-°C | 7.00 µin/in-°F | ASTM D696 |
|
Haysite H1000 Polyester Laminate
Haysite Grade 1000 laminate sheet is an outstanding material that is used in applications requiring exceptional weather and corrosion resistance. Grade H1000's unique polyester resin system provide..
|
|||
| CTE, linear |
12.6
µm/m-°C @Temperature 20.0 - 100 °C |
7.00
µin/in-°F @Temperature 68.0 - 212 °F |
|
|
Special Metals INCONEL® Alloy 751
A nickel-chromium alloy similar to INCONEL ALLOY X-750 but with increased aluminum content for greater precipitation hardening. INCONEL alloy 751 was designed for use as exhaust valves in internal-..
|
|||
| CTE, linear |
12.6
µm/m-°C @Temperature 20.0 - 100 °C |
7.00
µin/in-°F @Temperature 68.0 - 212 °F |
|
|
Special Metals INCONEL® Alloy X-750
A nickel-chromium alloy similar to INCONEL alloy 600 but made precipitation hardenable by additions of aluminum and titanium. The alloy has good resistance to corrosion and oxidation along with hig..
|
|||
| CTE, linear |
12.6
µm/m-°C @Temperature 23.0 - 85.0 °C |
7.00
µin/in-°F @Temperature 73.4 - 185 °F |
ISO 11359 |
|
Solvay TECHNYL® A 208F PA66, DRY
Description: Unreinforced polyamide PA66, heat stabilized, high fluidity, fast cycling grade, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 208F offers three main advanta..
|
|||
| CTE, linear |
12.6
µm/m-°C @Temperature 23.0 - 85.0 °C |
7.00
µin/in-°F @Temperature 73.4 - 185 °F |
ASTM D696 |
|
Solvay TECHNYL® 27010ST PA66, DRY
Description: Polyamide 66, with very high impact resistance even at low temperature, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® 2710ST is used in all sector of..
|
|||
| CTE, linear |
12.6
µm/m-°C @Temperature 23.0 - 85.0 °C |
7.00
µin/in-°F @Temperature 73.4 - 185 °F |
ASTM D696 |
|
Solvay TECHNYL® 2710IR PA66, DRY
Description: TECHNYL® 2710 IR is an unfilled polyamide 6.6, impact modified, for injection molding. The product is available in natural color, and in colors on request.Benefits: This product, use..
|
|||
| CTE, linear |
12.6
µm/m-°C @Temperature 20.0 °C |
7.00
µin/in-°F @Temperature 68.0 °F |
|
|
Cotronics Resbond™ 906 High Temperature Ceramic Adhesive, High Expansion |
|||
| CTE, linear |
12.6
µm/m-°C @Temperature 199 °C |
7.00
µin/in-°F @Temperature 390 °F |
hardened to 310 HB |
|
Bohler-Uddeholm P20 PREMIUM MODIFIED Pre-hardened Mold Steel
Cr-Mo alloyed steelP20 Modified offers the following benefits:No hardening risksNo hardening costsTime saving, e.g. no waiting for heat treatmentLower tool cost (e.g. no distortion to rectify)Modifi..
|
|||
| CTE, linear | 12.6 µm/m-°C | 7.00 µin/in-°F | |
|
Accuratus MACOR Machinable Glass Ceramic
Macor is cast as a two phase glass. After casting, it is heat treated causing crystallization of one phase giving rise to its glass-like and ceramic-like characteristics.Key Properties of MACOR: Mac..
|
|||
| CTE, linear |
12.6
µm/m-°C @Temperature 20.0 - 100 °C |
7.00
µin/in-°F @Temperature 68.0 - 212 °F |
|
|
Alloy Wire International RW 122 Hot Cutting Wire - High Strength
Maintains high strength at elevated temperatures. Used for cutting expanded polystyrene (EPS) foam and for the heat sealing of polypropylene bags.Information provided by Alloywire International.
|
|||
| CTE, linear |
12.6
µm/m-°C @Temperature 20.0 °C |
7.00
µin/in-°F @Temperature 68.0 °F |
|
|
Aremco AREMCOLOX™ 502-800 Macor Glass Ceramic
(Unverified Data**)
Recommended for temperatures to 1472°F (800°C) and peaks up to 1832°F (1000°C). Demonstrates low thermal conductivity, high strength, high electrical insulation, zero porosity, non-wetting, and ..
|
|||
| CTE, linear | 12.6 µm/m-°C | 7.00 µin/in-°F | |
|
Aremco Ceramabond™ 571 High Temperature Ceramic Adhesive/Paste, Magnesium Oxide Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
|
|||
| CTE, linear | 12.6 µm/m-°C | 7.00 µin/in-°F | |
|
Saint-Gobain Rulon® FCJ Grade Bearing/Seal PTFE
(discontinued **)
Saint Gobain Rulon® CJ is now produced as a part of the TriStar Plastics Corp. product line under the CJ Bearings trade name.Description: Rulon® is the Saint-Gobain trade name for their family of ..
|
|||
| CTE, linear |
12.6
µm/m-°C @Temperature 27.0 - 600 °C |
7.00
µin/in-°F @Temperature 80.6 - 1110 °F |
|
|
Carpenter Pyrotough® 78 Hot Work Die Steel
Pyrotough® 78 alloy is a premium quality hot work die steel engineered to withstand the operating temperatures and pressures associated with die casting and hot extrusion operations. The patented c..
|
|||
| CTE, linear | 12.6 - 98.0 µm/m-°C | 7.00 - 54.4 µin/in-°F | Average value: 41.5 µm/m-°C Grade Count:12 |
|
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% ..
|
|||
| CTE, linear |
12.6
µm/m-°C @Temperature 23.0 - 85.0 °C |
7.00
µin/in-°F @Temperature 73.4 - 185 °F |
ISO 11359 |
|
Solvay TECHNYL® 1015CR PA6, DRY
Description: Polyamide 6, unfilled, standard for fast injection cycles, for injection molding Available in: Asia Pacific Product Applications: TECHNYL® 1015CR has high fluidity and a good mould re..
|
|||