| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear |
50.0
-
80.0
µm/m-°C @Temperature 23.0 - 55.0 °C |
27.8
-
44.4
µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2:1999 |
|
Nylacast Impact Nylon 6, Impact Grade
Nylacast Impact has been designed for applications that have a high impact resistance and noise reduction capabilities. It works more effectively in applications where there are high stress. It also..
|
|||
| CTE, linear | 60.0 - 80.0 µm/m-°C | 33.3 - 44.4 µin/in-°F | Polykemi |
|
Polykemi AB POLYfill PP CIP15015 UV Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| CTE, linear |
60.0
-
80.0
µm/m-°C @Temperature -30.0 - 30.0 °C |
33.3
-
44.4
µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
|
SABIC Innovative Plastics Cycoloy® MC5300 PC+ABS (Asia Pacific)
Cycoloy MC5300 resin is a high heat, flame retardant PC/ABS blend. MC5300 resin passes UL-94 listing of 1.5mm V0 and 2.5mm 5VB. The balance of good flow, impact performance and heat resistance makes..
|
|||
| CTE, linear |
60.0
-
80.0
µm/m-°C @Temperature -30.0 - 30.0 °C |
33.3
-
44.4
µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
|
SABIC Innovative Plastics Cycoloy® MC5400 PC+ABS (Asia Pacific) |
|||
| CTE, linear |
60.0
-
80.0
µm/m-°C @Temperature -30.0 - 30.0 °C |
33.3
-
44.4
µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
|
SABIC Innovative Plastics Lexan® LCR200 PBT+PC (Asia Pacific) |
|||
| CTE, linear | 60.0 - 80.0 µm/m-°C | 33.3 - 44.4 µin/in-°F | Polykemi |
|
Polykemi AB POLYfill PP EIP8020F Polypropylene/EPDM, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| CTE, linear | 71.0 - 80.0 µm/m-°C | 39.4 - 44.4 µin/in-°F | Average value: 72.5 µm/m-°C Grade Count:6 |
|
Overview of materials for Polystyrene, Transparent Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of..
|
|||
| CTE, linear | 65.0 - 80.0 µm/m-°C | 36.1 - 44.4 µin/in-°F | Average value: 73.8 µm/m-°C Grade Count:29 |
|
Overview of materials for Polyphenylene Ether, Heat Resistant
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Heat Resistant". Each property range of values reported is minimum and maximum valu..
|
|||
| CTE, linear | 0.130 - 80.0 µm/m-°C | 0.0722 - 44.4 µin/in-°F | Average value: 11.2 µm/m-°C Grade Count:11 |
|
Overview of materials for Polycarbonate/ABS Alloy, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Carbon Fiber Filled". Each property range of values reported is minimum and max..
|
|||
| CTE, linear | 30.0 - 80.0 µm/m-°C | 16.7 - 44.4 µin/in-°F | Average value: 53.1 µm/m-°C Grade Count:11 |
|
Overview of materials for Polypropylene with 20% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Mica Filler". Specific grades with primary filler content between 15% and 24% are..
|
|||
| CTE, linear | 24.0 - 80.0 µm/m-°C | 13.3 - 44.4 µin/in-°F | Average value: 52.7 µm/m-°C Grade Count:3 |
|
Overview of materials for Fluorocarbon ETFE, with Glass or Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE, with Glass or Carbon Fiber Filler". Each property range of values reported is minimum..
|
|||
| CTE, linear | 18.0 - 80.0 µm/m-°C | 10.0 - 44.4 µin/in-°F | Average value: 27.3 µm/m-°C Grade Count:19 |
|
Overview of materials for Nylon 6, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a..
|
|||
| CTE, linear | 1.50 - 80.0 µm/m-°C | 0.833 - 44.4 µin/in-°F | Average value: 23.9 µm/m-°C Grade Count:23 |
|
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl..
|
|||
| CTE, linear | 20.0 - 80.0 µm/m-°C | 11.1 - 44.4 µin/in-°F | Average value: 43.3 µm/m-°C Grade Count:21 |
|
Overview of materials for Nylon 12, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. ..
|
|||
| CTE, linear |
70.0
-
80.0
µm/m-°C @Temperature 20.0 - 100 °C |
38.9
-
44.4
µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
|
Schwartz Technical Plastics LAMIGAMID® 200 Polyamide 66, Conditioned
Application: bearing bushes, machine parts, gears, linersInformation provided by Schwartz Technical Plastics GmbH
|
|||
| CTE, linear |
70.0
-
80.0
µm/m-°C @Temperature 20.0 - 100 °C |
38.9
-
44.4
µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
|
Schwartz Technical Plastics LAMIGAMID® 300 Cast Polyamide 6, Conditioned
Application: slippers and center blocks for heavy rolling mills, outrigger floatsInformation provided by Schwartz Technical Plastics GmbH
|
|||
| CTE, linear |
70.0
-
80.0
µm/m-°C @Temperature 20.0 - 100 °C |
38.9
-
44.4
µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
|
Schwartz Technical Plastics LAMIGAMID® 300 Cast Polyamide 6, Dry
Application: slippers and center blocks for heavy rolling mills, outrigger floatsInformation provided by Schwartz Technical Plastics GmbH
|
|||
| CTE, linear |
70.0
-
80.0
µm/m-°C @Temperature 20.0 - 100 °C |
38.9
-
44.4
µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
|
Schwartz Technical Plastics LAMIGAMID® 307 Cast Polyamide 6, Heat Stabilized, Conditioned
Application: slippers, inserts for coupling boxesInformation provided by Schwartz Technical Plastics GmbH
|
|||
| CTE, linear |
70.0
-
80.0
µm/m-°C @Temperature 20.0 - 100 °C |
38.9
-
44.4
µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
|
Schwartz Technical Plastics LAMIGAMID® 307 Cast Polyamide 6, Heat Stabilized, Dry
Application: slippers, inserts for coupling boxesInformation provided by Schwartz Technical Plastics GmbH
|
|||
| CTE, linear |
70.0
-
80.0
µm/m-°C @Temperature 20.0 - 100 °C |
38.9
-
44.4
µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
|
Schwartz Technical Plastics LAMIGAMID® 309 Cast Polyamide 6, Oil Filled, Conditioned
Application: slippers, inserts for coupling boxes, wear linersInformation provided by Schwartz Technical Plastics GmbH
|
|||
| CTE, linear |
70.0
-
80.0
µm/m-°C @Temperature 20.0 - 100 °C |
38.9
-
44.4
µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
|
Schwartz Technical Plastics LAMIGAMID® 309 Cast Polyamide 6, Oil Filled, Dry
Application: slippers, inserts for coupling boxes, wear linersInformation provided by Schwartz Technical Plastics GmbH
|
|||
| CTE, linear |
70.0
-
80.0
µm/m-°C @Temperature 20.0 - 100 °C |
38.9
-
44.4
µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
|
Schwartz Technical Plastics LAMIGAMID® 310 Cast Polyamide 6, Conditioned
Application: sheaves, wheels, rollers, mandrell segments, coupling parts, vibrator parts etc.Information provided by Schwartz Technical Plastics GmbH
|
|||
| CTE, linear |
70.0
-
80.0
µm/m-°C @Temperature 20.0 - 100 °C |
38.9
-
44.4
µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
|
Schwartz Technical Plastics LAMIGAMID® 310 Cast Polyamide 6, Dry
Application: sheaves, wheels, rollers, mandrell segments, coupling parts, vibrator parts etc.Information provided by Schwartz Technical Plastics GmbH
|
|||
| CTE, linear |
70.0
-
80.0
µm/m-°C @Temperature 20.0 - 100 °C |
38.9
-
44.4
µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
|
Schwartz Technical Plastics LAMIGAMID® 324 Cast Polyamide 6, MoS2, Heat Stabilized, Dry
Application: heavy-duty wheels, running speed up to 3m/sInformation provided by Schwartz Technical Plastics GmbH
|
|||
| CTE, linear |
75.0
-
80.0
µm/m-°C @Temperature 0.000 - 80.0 °C |
41.7
-
44.4
µin/in-°F @Temperature 32.0 - 176 °F |
ASTM D696 |
|
Styron Pulse® A35-105 PC/ABS
PULSEâ„¢ A35-105 engineering resins give exceptional impact strength even at low temperatures and have high heat distortion temperature.Information provided by DowThis product line was spun off f..
|
|||
| CTE, linear |
75.0
-
80.0
µm/m-°C @Temperature 0.000 - 80.0 °C |
41.7
-
44.4
µin/in-°F @Temperature 32.0 - 176 °F |
ASTM D696 |
|
Styron Pulse® A35-110 PC/ABS
PULSEâ„¢ A35-110 engineering resins give exceptional impact strength even at low temperatures and have high heat distortion temperature. The proprietary mass ABS technology of Dow allows these p..
|
|||
| CTE, linear |
70.0
-
80.0
µm/m-°C @Temperature 20.0 - 100 °C |
38.9
-
44.4
µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
|
Schwartz Technical Plastics OPTAMID® Cast Polyamide 6, Conditioned
Application: deflection rope sheaves for elevatorsInformation provided by Schwartz Technical Plastics GmbH
|
|||
| CTE, linear |
60.0
-
80.0
µm/m-°C @Temperature 20.0 °C |
33.3
-
44.4
µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
|
Alliance BIN-72 Bonded (Composite) Magnetic Material |
|||
| CTE, linear | 10.0 - 80.0 µm/m-°C | 5.56 - 44.4 µin/in-°F | Average value: 57.5 µm/m-°C Grade Count:7 |
|
Overview of materials for Nylon 66, Nucleated
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Nucleated". Each property range of values reported is minimum and maximum values of appropriat..
|
|||
| CTE, linear | 70.0 - 80.0 µm/m-°C | 38.9 - 44.4 µin/in-°F | |
|
Hippe PVC-U Polyvinyl Chloride
Material at reasonable price, high strength. Used in machine construction as covers, pipes, section, façade elements.Information provided by Hippe.
|
|||