Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 90.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
CTE, linear 80.0 - 90.0 µm/m-°C

@Temperature 20.0 °C
44.4 - 50.0 µin/in-°F

@Temperature 68.0 °F
DN.53752
Polimersan Plastics POLIKES® (PA 6 G) Cast Polyamide
POLIKES® PA6 G (CAST POLYAMIDE) is a plastic with high physical, electrical and chemical resistance. Its resistance is high especially against strokes and loads. Its temperature resistance is high..
CTE, linear 80.0 - 90.0 µm/m-°C

@Temperature 20.0 °C
44.4 - 50.0 µin/in-°F

@Temperature 68.0 °F
ASTM E831
Polimersan Plastics POLITEF® (PTFE) with 60% Bronze
As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv..
CTE, linear 70.0 - 90.0 µm/m-°C
38.9 - 50.0 µin/in-°F
Polykemi
Polykemi AB POLYfill PP CQX10030E10 F Polypropylene, Mineral Reinforced, Elastomer Modified
Information provided by Polykemi AB
CTE, linear 70.0 - 90.0 µm/m-°C
38.9 - 50.0 µin/in-°F
Polykemi
Polykemi AB POLYfill PP CQX10030E10 Polypropylene, Mineral Reinforced, Elastomer Modified
Information provided by Polykemi AB
CTE, linear 70.0 - 90.0 µm/m-°C
38.9 - 50.0 µin/in-°F
Polykemi
Polykemi AB POLYfill PP CQX30030 RTX Polypropylene, Mineral Reinforced, Scratch Resistant
Information provided by Polykemi AB
CTE, linear 70.0 - 90.0 µm/m-°C
38.9 - 50.0 µin/in-°F
Polykemi
Polykemi AB POLYfill PPC TS20020 UV Polypropylene Copolymer, Mineral Reinforced, UV-Stabilized
Information provided by Polykemi AB
CTE, linear 50.0 - 90.0 µm/m-°C
27.8 - 50.0 µin/in-°F
Average value: 76.0 µm/m-°C Grade Count:25
Overview of materials for Polystyrene, Molded, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
CTE, linear 72.0 - 90.0 µm/m-°C

@Temperature 0.000 - 156 °C
40.0 - 50.0 µin/in-°F

@Temperature 32.0 - 312 °F
Average value: 76.5 µm/m-°C Grade Count:4
Overview of materials for Acrylic, Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Heat Resistant, Molded". Each property range of values reported is minimum and maximum values o..
CTE, linear 45.0 - 90.0 µm/m-°C
25.0 - 50.0 µin/in-°F
Average value: 63.7 µm/m-°C Grade Count:46
Overview of materials for PVC, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatW..
CTE, linear 35.0 - 90.0 µm/m-°C
19.4 - 50.0 µin/in-°F
Average value: 45.1 µm/m-°C Grade Count:11
Overview of materials for PVC, Foam Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Foam Grade". Each property range of values reported is minimum and maximum values of appropriate Ma..
CTE, linear 70.0 - 90.0 µm/m-°C

@Temperature 20.0 °C
38.9 - 50.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Solvay Specialty Polymers Solef® 8808/0902 Carbon Fiber Reinforced PVDF Compound  (discontinued **)
Key features of this grade: Carbon Fiber Reinforcement, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinate..
CTE, linear 12.0 - 90.0 µm/m-°C
6.67 - 50.0 µin/in-°F
Average value: 44.3 µm/m-°C Grade Count:14
Overview of materials for Epoxy, Cast, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Unreinforced". Each property range of values reported is minimum and maximum values of appr..
CTE, linear 90.0 - 90.0 µm/m-°C

@Temperature 93.3 - 238 °C
50.0 - 50.0 µin/in-°F

@Temperature 200 - 460 °F
Average value: 90.0 µm/m-°C Grade Count:1
Overview of materials for Nylon 66, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Extruded". Each property range of values reported is minimum and maximum values of appropriate..
CTE, linear 70.0 - 90.0 µm/m-°C
38.9 - 50.0 µin/in-°F
Average value: 80.0 µm/m-°C Grade Count:4
Overview of materials for Nylon 12, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Flame Retardant". Each property range of values reported is minimum and maximum values of appr..
CTE, linear 32.0 - 90.0 µm/m-°C
17.8 - 50.0 µin/in-°F
Average value: 67.0 µm/m-°C Grade Count:6
Overview of materials for Nylon, Amorphous Transparent Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Amorphous Transparent Alloy". Each property range of values reported is minimum and maximum value..
CTE, linear 80.0 - 90.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
44.4 - 50.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics NORYL GTX6601 PPE+PA66 (Asia Pacific)
PPE+PA Unfilled GTX
CTE, linear 80.0 - 90.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
44.4 - 50.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics Noryl GTX GTX6601 PPE+PA66 (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear 80.0 - 90.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
44.4 - 50.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics NORYL GTX GTX6601 PPE+PA66 (Asia Pacific)
CTE, linear 50.0 - 90.0 µm/m-°C

@Temperature 20.0 °C
27.8 - 50.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Zeus EFEP Tubing
CTE, linear 50.0 - 90.0 µm/m-°C

@Temperature 20.0 °C
27.8 - 50.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Zeus ETFE Tubing
ETFE (Ethylenetetrafluoroethylene), a copolymer of ethylene and tetrafluoroethylene, is used in applications requiring excellent impact, abrasion and stress cracking resistance. This polymer possess..
CTE, linear 50.0 - 90.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
27.8 - 50.0 µin/in-°F

@Temperature 73.4 - 140 °F
ASTM D696
Daikin NEOFLON EP-610 ETFE Pellets
Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl..
CTE, linear 50.0 - 90.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
27.8 - 50.0 µin/in-°F

@Temperature 73.4 - 140 °F
ASTM D696
Daikin NEOFLON EP-610AS ETFE Pellets
Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl..
CTE, linear 50.0 - 90.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
27.8 - 50.0 µin/in-°F

@Temperature 73.4 - 140 °F
ASTM D696
Daikin NEOFLON RP-4040 EFEP Pellets
NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop..
CTE, linear 50.0 - 90.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
27.8 - 50.0 µin/in-°F

@Temperature 73.4 - 140 °F
ASTM D696
Daikin NEOFLON RP-5000AS EFEP Pellets
NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop..
CTE, linear 50.0 - 90.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
27.8 - 50.0 µin/in-°F

@Temperature 73.4 - 140 °F
ASTM D696
Daikin NEOFLON EP-620 ETFE Pellets
Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl..
CTE, linear 72.0 - 90.0 µm/m-°C

@Temperature 20.0 °C
40.0 - 50.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Ensinger Tecast Vekton™ 6PALM Premium Bearing Grade cast nylon (PA6)
Tecast 6PALM contains both solid and liquid lubricants dispersed throughout the nylon to provide consistent wear rates and coefficients of friction.Information provided by Ensinger, Inc.
CTE, linear 40.0 - 90.0 µm/m-°C
22.2 - 50.0 µin/in-°F
Average value: 72.0 µm/m-°C Grade Count:5
Overview of materials for Nylon 66/6, Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, Mineral Reinforced". Each property range of values reported is minimum and maximum values of..
CTE, linear 80.0 - 90.0 µm/m-°C
44.4 - 50.0 µin/in-°F
Master Bond EP21TDC-2LO Two component, highly flexibilized epoxy resin compound
Product Description: Master Bond Polymer System EP21TDC-2LO is a two component, highly flexible epoxy resin compound for high performance bonding, sealing, coating, and encapsulation. It is formulat..
CTE, linear 54.0 - 90.0 µm/m-°C
30.0 - 50.0 µin/in-°F
Average value: 72.0 µm/m-°C Grade Count:5
Overview of materials for Acrylic, Impact Modified Sheet
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified Sheet". Each property range of values reported is minimum and maximum values of..
CTE, linear 80.0 - 90.0 µm/m-°C
44.4 - 50.0 µin/in-°F
ASTM D696
Guarniflon PTFE G458 Polytetrafluoroethylene 60% Bronze, 2% Carbon
PTFE G Standard Compound with bronzeProperties: Enhanced compressive strength. Good wear resistance and high thermal conductivity.Application: Unlubricated bearings for high speed excluding hard ..
Copyright © lookpolymers.com All Rights Reserved