Polymer Property : CTE, linear = 94.4 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
CTE, linear 170 µm/m-°C

@Temperature 23.0 - 60.0 °C
94.4 µin/in-°F

@Temperature 73.4 - 140 °F
Murtfeldt Material ”S”® 8000 Polyethylene
Material ”S”® 8000 improves on the already impressive material properties of Original Material ”S”®. The self lubricating character of this material makes it ideally suited for use in sliding..
CTE, linear 170 µm/m-°C

@Temperature 23.0 - 60.0 °C
94.4 µin/in-°F

@Temperature 73.4 - 140 °F
Murtfeldt Original Material ”S”® plus + GB Polyethylene, Glass Bead Filled
The balanced quantity of micro glass beads in Material ”S”® plus+ GB provides the combined benefits of extremely high molecular weight polyethylene and glass. The glass beads that protrude from ..
CTE, linear 170 µm/m-°C

@Temperature 20.0 °C
94.4 µin/in-°F

@Temperature 68.0 °F
Humiseal 1A27 Urethane Conformal Coating
Humiseal 1A27 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL ApprovedPasses thermal shock test (MIL-I-46058C)Flammabilit..
CTE, linear 170 µm/m-°C

@Temperature 20.0 °C
94.4 µin/in-°F

@Temperature 68.0 °F
Humiseal 1A27LSE Urethane Conformal Coating
Humiseal 1A27LSE Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL Approval PendingPasses thermal shock test (MIL-I-46058C)..
CTE, linear 170 µm/m-°C

@Temperature 20.0 °C
94.4 µin/in-°F

@Temperature 68.0 °F
Humiseal 1A33 Urethane Conformal Coating
Humiseal 1A33 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL ApprovedMIL-I-46058C ApprovedPasses thermal shock test (MIL..
CTE, linear 170 µm/m-°C

@Temperature 20.0 °C
94.4 µin/in-°F

@Temperature 68.0 °F
Humiseal 1C61 UV Cure Conformal Coating
Humiseal 1C61 UV Cure Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock t..
CTE, linear 170 µm/m-°C

@Temperature 20.0 °C
94.4 µin/in-°F

@Temperature 68.0 °F
TMA
Toyobo Pelprene™ P-150M Polyester TPE
Key Feature: Pelprene P typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'P' type is a block..
CTE, linear 170 µm/m-°C

@Temperature 20.0 °C
94.4 µin/in-°F

@Temperature 68.0 °F
TMA
Toyobo PELPRENE™ P40H Polyester TPE
Features: Polyester TPEInformation provided by Toyobo.
CTE, linear 170 µm/m-°C

@Temperature 20.0 °C
94.4 µin/in-°F

@Temperature 68.0 °F
TMA
Toyobo PELPRENE™ P40H-05 Polyester TPE, Non-smell, Non-deposit
Features: Polyester TPE, Non-smell, Non-depositInformation provided by Toyobo.
CTE, linear 170 µm/m-°C

@Temperature 20.0 °C
94.4 µin/in-°F

@Temperature 68.0 °F
TMA
Toyobo PELPRENE™ P55B Polyester TPE
Features: Polyester TPEInformation provided by Toyobo.
CTE, linear 170 µm/m-°C

@Temperature 20.0 °C
94.4 µin/in-°F

@Temperature 68.0 °F
TMA
Toyobo PELPRENE™ P55U Polyester TPE, Weather-resistant
Features: Polyester TPE, Weather-resistantInformation provided by Toyobo.
CTE, linear 170 µm/m-°C

@Temperature 20.0 °C
94.4 µin/in-°F

@Temperature 68.0 °F
TMA
Toyobo PELPRENE™ P80C Polyester TPE, High Flexibility, High Melting Point
Features: Polyester TPE, High Flexibility, High Melting PointInformation provided by Toyobo.
CTE, linear 170 µm/m-°C

@Temperature 20.0 °C
94.4 µin/in-°F

@Temperature 68.0 °F
TMA
Toyobo PELPRENE™ P95C Polyester TPE, High Flexibility, High Melting Point
Features: Polyester TPE, High Flexibility, High Melting PointInformation provided by Toyobo.
CTE, linear 170 µm/m-°C
94.4 µin/in-°F
Above Tg
Tra-Con Tra-Bond 9070D Filled Epoxy Adhesive
TRA-BOND 9070D filled epoxy adhesive exhibits a low coefficient of expansion. Information provided by Tra-Con Inc.
CTE, linear 170 µm/m-°C

@Temperature -20.0 - 32.0 °C
94.4 µin/in-°F

@Temperature -4.00 - 89.6 °F
ASTM D696
DuPont™ Surlyn® 8020 Ionomer Resin, Sodium
Surlyn® 8020 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu..
CTE, linear 170 µm/m-°C

@Temperature -20.0 - 32.0 °C
94.4 µin/in-°F

@Temperature -4.00 - 89.6 °F
ASTM D696
DuPont™ Surlyn® 9020 Ionomer Resin, Zinc
Surlyn® 9020 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The resin contains an addit..
CTE, linear 170 µm/m-°C
94.4 µin/in-°F
Above Tg
Epoxy Technology EPO-TEK® 320-LV Optically Opaque Epoxy
Material Description: A two component, optically opaque epoxy adhesive designed for semiconductor and PCB applications in optoelectronic instrumentation and assemblies. A lower viscosity version of..
CTE, linear 170 µm/m-°C
94.4 µin/in-°F
Above Tg
Epoxy Technology EPO-TEK® OG116-31 UV Cure Optical Epoxy
Product Description: EPO-TEK® OG116-31 is a single component, UV curable epoxy adhesive and encapsulant, designed for PCB and circuit assembly applications found in semiconductor, computer, medical..
CTE, linear 170 µm/m-°C
94.4 µin/in-°F
Hippe PE 1000 Polyethylene
Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall..
CTE, linear 170 µm/m-°C
94.4 µin/in-°F
Hippe PE 500 Polyethylene
Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall..
CTE, linear 170 µm/m-°C

@Temperature -40.0 - 140 °C
94.4 µin/in-°F

@Temperature -40.0 - 284 °F
ASTM D696
Arkema Group Pebax® 5533 Polyether Block Amide (PEBA)
Information provided by Arkema Group
CTE, linear 170 µm/m-°C
94.4 µin/in-°F
Above Tg
3M Scotch-Weld™ DP8005 Black Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl..
CTE, linear 170 µm/m-°C
94.4 µin/in-°F
Above Tg
3M Scotch-Weld™ DP8005 Translucent Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl..
CTE, linear 170 µm/m-°C

@Temperature 20.0 °C
94.4 µin/in-°F

@Temperature 68.0 °F
TMA
Toyobo PELPRENE™ P48U Polyester TPE, Weather-resistant
Features: Polyester TPE, Weather-resistantInformation provided by Toyobo.
CTE, linear 170 µm/m-°C

@Temperature 20.0 - 60.0 °C
94.4 µin/in-°F

@Temperature 68.0 - 140 °F
TMS2 Perkin Elmer
Arkema Group Orgalloy® LT 5050 ES Polyamide Alloy
Polyamide Alloy, Blow Molding of Technical PartsInformation provided by Arkema Group
Copyright © lookpolymers.com All Rights Reserved