| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear |
13.0
-
95.0
µm/m-°C @Temperature >=162 °C |
7.22
-
52.8
µin/in-°F @Temperature >=324 °F |
Average value: 54.0 µm/m-°C Grade Count:1 |
|
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled". Each property range of values reported ..
|
|||
| CTE, linear |
80.0
-
95.0
µm/m-°C @Temperature 20.0 °C |
44.4
-
52.8
µin/in-°F @Temperature 68.0 °F |
DIN 53752 |
|
GEHR Plastics PA 6.6 Nylon 6.6, Dry
Polyamide shows both a high thermostability and high stiffness, hardness and toughness. These are some of the main characteristics. Due to the fact, that the good mechanical characteristics will be ..
|
|||
| CTE, linear |
90.0
-
95.0
µm/m-°C @Temperature 20.0 °C |
50.0
-
52.8
µin/in-°F @Temperature 68.0 °F |
|
|
Abatron AboCast/AboCure 8109-3
Low viscosity, RT cure. Easy processing.Processing: 100/10 pbw; Potlife: 2.5 h/20°C (68°F), 30 min/40°C (105°F), 15 min/60°C (140°F); mix at RT; cures in: 24 h/20°C (68°F), 2-3 h/60°C (140..
|
|||
| CTE, linear | 43.2 - 95.0 µm/m-°C | 24.0 - 52.8 µin/in-°F | Average value: 58.8 µm/m-°C Grade Count:4 |
|
Overview of materials for Acetal Copolymer + Glass/PTFE
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer + Glass/PTFE". Each property range of values reported is minimum and maximum values of ..
|
|||
| CTE, linear |
17.0
-
95.0
µm/m-°C @Temperature 50.0 - 250 °C |
9.44
-
52.8
µin/in-°F @Temperature 122 - 482 °F |
Average value: 45.7 µm/m-°C Grade Count:6 |
|
Overview of materials for Polyphthalamide (PPA), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o..
|
|||