Polymer Property : Thermal Conductivity = 0.160 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.160 W/m-K
1.11 BTU-in/hr-ft²-°F
DIN 52612
Polycasa PS
QUINN PS sheets have good optical properties and a brilliant surface. The QUINN PS range contains sheets that are easy to fabricate, to vacuum form, and show a high light transmission (min 88% wavel..
Thermal Conductivity 0.160 W/m-K
1.11 BTU-in/hr-ft²-°F
DIN 52612
Ineos Nova S-3400 Medium Impact Compact Polystyrene  (discontinued **)
Impact polystyrene with good flow characteristics and a high elongation. Generally used for applications where a tough material is required. For injection molding generally a lubricated type is us..
Thermal Conductivity 0.160 W/m-K
1.11 BTU-in/hr-ft²-°F
DIN 52612
Ineos Nova S-3500MG Compact Polystyrene Microgranulates  (discontinued **)
Very easy flowing medium impact polystyrene Microgranulates, having a diameter of 0.8 - 1.0 mm and a very large specific surface areas. This grade is especially designed for use in compounding and ..
Thermal Conductivity 0.160 W/m-K
1.11 BTU-in/hr-ft²-°F
DIN 52612
Ineos Nova S-4400 High Impact Compact Polystyrene  (discontinued **)
Impact polystyrene which combines excellent flow characteristics with a good dimensional stability under heat and a high stiffness. This grade is designed for injection molding of technical parts o..
Thermal Conductivity 0.160 W/m-K
1.11 BTU-in/hr-ft²-°F
DIN 52612
Ineos Nova S-5400 High Impact Compact Polystyrene  (discontinued **)
Impact polystyrene with high dimensional stability under heat, particularly suitable fore extrusion and thermoforming of technical parts or packaging applications but also used for injection molding..
Thermal Conductivity 0.160 W/m-K
1.11 BTU-in/hr-ft²-°F
ASTM C177
SABIC Innovative Plastics Lexan® FL930 PC (Asia Pacific)
Various weight reductions at 0.250"" (6.35 mm) wall, 30% GR. Superior flex strength/modulus, good tensile strength. V-0/5VA at 0.250"" (6.35 mm).
Thermal Conductivity 0.160 W/m-K
1.11 BTU-in/hr-ft²-°F
ASTM C177
SABIC Innovative Plastics Lexan® FL933 PC
Various weight reductions at 0.250"" wall. 30% GR. Superior flexural strength and modulus; good tensile strength. UV-stabilized.
Thermal Conductivity 0.160 - 0.432 W/m-K
1.11 - 3.00 BTU-in/hr-ft²-°F
Average value: 0.342 W/m-K Grade Count:3
Overview of materials for Nylon 12, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. ..
Thermal Conductivity 0.160 W/m-K
1.11 BTU-in/hr-ft²-°F
Through Thickness
GrafTech P2 PET Film
Optional coating for eGRAF® SPREADERSHIELD™ graphite products. Structure: Plastic 0.0014mm - Adhesive 0.008mm - Graphite
Thermal Conductivity 0.160 W/m-K
1.11 BTU-in/hr-ft²-°F
Through Thickness
GrafTech P6A6 Ultra-Thin, Double-Coated Adhesive Tape
Optional coating for eGRAF® SPREADERSHIELD™ graphite products. Structure: 0.01mm Total - Acrylic Adhesive - Polyester Film - Acrylic Adhesive - Release Liner
Thermal Conductivity 0.160 W/m-K
1.11 BTU-in/hr-ft²-°F
LG Chemical Acetone
Overview: Acetone is the raw material of MMA(Methyl Metha Acrylate), BPA, ascorbic acid (Vitamin C), etc. In addition, acetone is widely used as solvents for synthetic resins, rubber, oil paper and ..
Thermal Conductivity 0.160 W/m-K
1.11 BTU-in/hr-ft²-°F
DIN 52612-1
Styrolution PS 116 N/L GPPS
Styrolution PS 116N/L is a general purpose polystyrene grade with excellent flow properties and improved heat resistance.Excellent flow propertiesHigh heat resistanceInformation provided by Styrolut..
Thermal Conductivity 0.160 W/m-K
1.11 BTU-in/hr-ft²-°F
DIN 52612-1
Styrolution PS 124 N/L GPPS
Styrolution PS 124N/L is a general purpose polystyrene grade with a good flow characteristic and an improved heat resistance.Excellent flow propertiesHigh heat resistanceUL 94 HB (Antwerp only)Infor..
Thermal Conductivity 0.160 W/m-K
1.11 BTU-in/hr-ft²-°F
DIN 52612-1
Styrolution PS 153F GPPS
Styrolution PS 153F is general purpose polystyrene with high heat resistance and good flow properties. Styrolution PS 153F is free of internal lubricants, e.g. zinc stearate.Free of internal lubrica..
Thermal Conductivity 0.160 W/m-K
1.11 BTU-in/hr-ft²-°F
Styron Pulse® 830 ABS + Polycarbonate
PULSE® 830 Engineering resin offers excellent processability, high heat resistance, and high impact strength at both room and low temperatures.PULSE 830 Engineering resin has been used in automot..
Thermal Conductivity 0.160 W/m-K
1.11 BTU-in/hr-ft²-°F
ASTM C 177
Borealis Borcoat™ GA700E-7032 Syntactic Polypropylene for Steel Pipe Coating
Borcoat GA700E-7032 is a grey colored syntactic, high impact polypropylene with high thermal insulation capacity and high compressive strength.Borcoat GA700E-7032 is recommended as thermal insulatio..
Thermal Conductivity 0.160 W/m-K
1.11 BTU-in/hr-ft²-°F
Goodfellow Topas® Cyclo-olefin copolymer
Information provided by Goodfellow.
Thermal Conductivity 0.160 W/m-K
1.11 BTU-in/hr-ft²-°F
Melt
Covestro Bayblend® T88 GF-20* Polycarbonate + SAN Glass Filled Impact Grade
Developmental productInjection molding grade20 % GFoptimized heat ageing- and UV-stabilityvery good flowtensile modulus = 7500 MPaVicat/B 120 = 130 °CPreprocessingMax. Water content
Thermal Conductivity 0.160 W/m-K
1.11 BTU-in/hr-ft²-°F
Melt
Covestro Bayblend® T88-4N Polycarbonate + ABS, 20% Glass Filled
Injection molding grade20 % glass fiber filledtensile modulus = 5900 MPaVicat/B 120 temperature = 134 °CPreprocessingMax. Water content
Thermal Conductivity 0.160 W/m-K
1.11 BTU-in/hr-ft²-°F
of melt
DuPont Performance Polymers Zytel® FG408L NC010 Nylon 66  (Unverified Data**)
Unreinforced Toughened Polyamide 66 with Developed for Food Contact Applications Zytel FG408L NC010 is a general purpose lubricated impact modified polyamide 66 resin with superior toughness for inj..
Thermal Conductivity 0.160 W/m-K
1.11 BTU-in/hr-ft²-°F
of melt
DuPont Performance Polymers Zytel® FG42A NC010 Nylon 66  (Unverified Data**)
Unreinforced High Viscosity Polyamide 66 with Developed for Food Contact ApplicationsZytel FG42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion. It has been develop..
Thermal Conductivity 0.160 W/m-K
1.11 BTU-in/hr-ft²-°F
of melt
DuPont Performance Polymers Zytel® FG42L NC010 Nylon 66  (Unverified Data**)
Unreinforced High Viscosity Polyamide 66 with Developed for Food Contact Applications Information provided by DuPont Performance Polymers
Thermal Conductivity 0.160 W/m-K
1.11 BTU-in/hr-ft²-°F
of melt
DuPont Performance Polymers Zytel® 103FHS NC010 Nylon 66  (Unverified Data**)
Unreinforced Heat Stabilized Polyamide 66 Zytel 103FHS NC010 is a heat stabilized internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivi..
Thermal Conductivity 0.160 W/m-K
1.11 BTU-in/hr-ft²-°F
of melt
DuPont Performance Polymers Zytel® FN727 NC010A Nylon 6  (Unverified Data**)
Toughened Polyamide 6Information provided by DuPont Performance Polymers
Thermal Conductivity 0.160 W/m-K

@Temperature 50.0 °C
1.11 BTU-in/hr-ft²-°F

@Temperature 122 °F
Dow VORALUX™ HL 430 Copolymer Polyol
VORALUX™ HL 430 is a unique grafted polyether polyol containing copolymerized styrene and acrylonitrile and filtered to 100 microns. It is used in the manufacture of flexible slabstock polyurethan..
Thermal Conductivity 0.160 W/m-K
1.11 BTU-in/hr-ft²-°F
CENTROPLAST CENTROMID 12 GF 30 Polyamide 12 30% glass fiber
CENTROMID 12 GF 30 is a dimensionally stable and high strength material with good electrical insulating properties. Its applications include levers and valve parts.Information provided by CENTROPLA..
Thermal Conductivity 0.160 W/m-K
1.11 BTU-in/hr-ft²-°F
of melt
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66  (Unverified Data**)
Unreinforced Polyamide 66Zytel 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers
Thermal Conductivity 0.160 W/m-K
1.11 BTU-in/hr-ft²-°F
DIN 52612
Ineos Nova S-3201 Medium Impact Compact Polystyrene  (discontinued **)
Extremely easy flowing medium impact polystyrene, designed for extreme short cycle times for injection molding of household, packaging and toys. The material is provided with external lubricant to ..
Thermal Conductivity 0.160 W/m-K
1.11 BTU-in/hr-ft²-°F
DIN 52612
Ineos Nova S-4122 Medium Impact Compact Polystyrene  (discontinued **)
Low friction, medium impact polystyrene which combines excellent flow characteristics with a good dimensional stability under heat and a high stiffness. This grade is designed for injection moldin..
Thermal Conductivity 0.160 W/m-K
1.11 BTU-in/hr-ft²-°F
DIN 52612
Ineos Nova S-3207 Medium Impact Compact Polystyrene  (discontinued **)
High flow medium impact polystyrene, designed of injection molding of low friction household goods, packaging and toys. It combines low friction properties with excellent (ultrasonic) weldability.A..