| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | ISO 8302 |
|
SABIC Innovative Plastics Cycolac® S705 ABS (Europe-Africa-Middle East)
CYCOLAC S705 is a new generation ABS plating grade, offering semi high heat with a good property balance for impact and flow. CYCOLAC S705 demonstrates excellent electroplatability and a good therma..
|
|||
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | ISO 8302 |
|
SABIC Innovative Plastics Cycoloy® C2100 PC+ABS (Asia Pacific)
CYCOLOY C2100 is a flame retardant blend, specifically developed to meet the stringent requirements of mains current carrying applications. CYCOLOY C2100 combines
|
|||
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | ASTM C177 |
|
SABIC Innovative Plastics Cycoloy® C2950HF PC+ABS
Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced impact and heat properties plus improved flow for various applications.
|
|||
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | ISO 8302 |
|
SABIC Innovative Plastics Cycoloy® C4210 PC+ABS (Europe-Africa-Middle East)
CYCOLOY C4210 is a 10% glass reinforced, non-FR PC+ABS grade. It shows high heat resistance, excellent strength and rigidity with good cosmetic appearance. It combines a good processabity with a low..
|
|||
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | ISO 8302 |
|
SABIC Innovative Plastics Cycoloy® C4210HF PC+ABS
PC+ABS Blend with 10% Glass Reinforce. High flow, High heat resistance., Excellent balance strength/rigidity. Good impact/appearance.
|
|||
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | ISO 8302 |
|
SABIC Innovative Plastics Cycoloy® C4220K PC+ABS (Asia Pacific)
Cycoloy* C4220K resin is an injection moldable 20% glass reinforced non FR PC-ABS.
Key features include improved Knit Line strength, good flow, excellent strength & rigidity, heat resistance & hyd..
|
|||
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | ISO 8302 |
|
SABIC Innovative Plastics Cycoloy® C6840 PC+ABS (Asia Pacific)
Cycoloy* C6840 resin is an injection moldable, flame retardant PC/ABS blend. It contains non-chlorinated & non-brominated flame retardant systems intended to meet governmental regulations and variou..
|
|||
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | ISO 8302 |
|
SABIC Innovative Plastics Cycoloy® FXC630SK PC+ABS (Europe-Africa-Middle East)
PC+ABS, of non-chlorinated & non-brominated flame retardant with Sparkle effect.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | ISO 8302 |
|
SABIC Innovative Plastics Lexan® AD143 PC
LEXAN AD143 is a medium viscosity, injection molding grade exhibiting low dust attraction. It is designed for applications with high optical requirements in terms of clarity and light transmission ..
|
|||
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | ISO 8302 |
|
SABIC Innovative Plastics Lexan® OQ1028 PC (Europe-Africa-Middle East)
Optical quality, high purity PC resin for CD/DVD and BD applications at short cycle times
|
|||
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | ISO 8302 |
|
SABIC Innovative Plastics Lexan® PC2200R PC (Europe-Africa-Middle East)
PC2200R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
|
|||
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | ASTM C177 |
|
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer (Europe-Africa-Middle East)
XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
|
|||
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | ASTM C 177 |
|
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Europe-Africa-Middle East)
Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties.This ..
|
|||
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | ISO 8302 |
|
SABIC Innovative Plastics Cycoloy® FXC810MA PC+ABS (Europe-Africa-Middle East)
CYCOLOY FXC810MA is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require marble colour effects. The colour package may effect performance.This data was suppl..
|
|||
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | ISO 8302 |
|
SABIC Innovative Plastics Lexan® 144R PC (Europe-Africa-Middle East)
Medium viscosity, multi purpose polycarbonate resin with added release agent. Food contact approved in limited colors. Effective January 15th, 2007 this grade will no longer be supported with bioc..
|
|||
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | DIN 52612 |
|
Lehmann & Voss LUVOCOM® 80/TF/18/SI/2/BK Polyacetal-copolymer, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
|
|||
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | ASTM C 177 |
|
SABIC Innovative Plastics PC0700 PC
PC0700 resin is a low flow (MFR = 7 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T..
|
|||
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | ISO 8302 |
|
SABIC Innovative Plastics PC0700 PC (Europe-Africa-Middle East)
PC0700 resin is a low flow (MFR = 7 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T..
|
|||
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | ASTM C 177 |
|
SABIC Innovative Plastics PC0800 PC
PC0800 resin is a low flow (MFR = 8 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T..
|
|||
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | ISO 8302 |
|
SABIC Innovative Plastics PC1500 PC (Europe-Africa-Middle East)
PC1500 resin is a medium-high flow (MFR = 15 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rel..
|
|||
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | ASTM C 177 |
|
SABIC Innovative Plastics PC1800R PC (Europe-Africa-Middle East)
PC1800R resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was suppli..
|
|||
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | ISO 8302 |
|
SABIC Innovative Plastics PC2200 PC (Europe-Africa-Middle East)
PC2200 resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.
|
|||
| Thermal Conductivity |
0.200
W/m-K @Temperature 40.0 °C |
1.39
BTU-in/hr-ft²-°F @Temperature 104 °F |
ASTM C177 |
|
Solvay Specialty Polymers Hyflon® MFA® F1530 Perfluoropolymer
Hyflon® MFA is a family of perfluoro polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistanc..
|
|||
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | ISO 8302 |
|
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Europe-Africa-Middle East)
Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat ..
|
|||
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | ISO 8302 |
|
SABIC Innovative Plastics Xenoy® X4870HH PC+PET (Europe-Africa-Middle East)
Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st..
|
|||
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | ASTM C177 |
|
Covestro Makrolon® 6485 Polycarbonate, Injection Grade
Medium viscosity, flame retardant injection molding grade with easy mold release, not available in transparent colors.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was ..
|
|||
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | Dry |
|
Asahi Kasei Leona® 1300S Nylon 66
General purpose grade. Good balance of flowability and mechanical properties.Applications:Connectors, washers, cable ties. Information provided by Asahi Kasei
|
|||
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | cross-flow; ISO 8302 |
|
Covestro Makrolon® LQ2647 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Optical lens, safety g..
|
|||
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | ISO 8302 |
|
SABIC Innovative Plastics PC2200 PC
PC2200 resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T..
|
|||
| Thermal Conductivity | 0.200 - 0.340 W/m-K | 1.39 - 2.36 BTU-in/hr-ft²-°F | Average value: 0.306 W/m-K Grade Count:25 |
|
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a..
|
|||