Thermal Properties Metric English Comments
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
DIN.52612
Omnia Plastica PTFE Polytetrafluoroethylene
A Fluoropolymer used mainly for its excellent chemical resistance. It has poor mechanical features. The strain, even under low weight, makes it very suitable as a gasket material.Features:Chemical: ..
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
3M Dyneon™ Fluorel™ FC-2180 Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Lower mold shrinkage and excellent co..
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
3M Dyneon™ Fluorel™ FC-2144 Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Higher viscosity version of FC-2123. ..
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
3M Dyneon™ Fluorel™ FC-2120 Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Dipolymer for difficult extrusions. ..
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
3M Dyneon™ Fluorel™ FC-2182 Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Dipolymer for autoclave curing. Used..
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
3M Dyneon™ Fluorel™ FC-2178 Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp..
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
ASTM E1530
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire PEEK is produced to the highest industry standards and is characteriz..
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
ASTM E831
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and pro..
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
ASTM E831
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insulation..
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
ISO 8302
SABIC Innovative Plastics ULTEM 1000R PEI (Europe-Africa-Middle East)
Standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0, V2 and 5VA listing.
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
ISO 8302
SABIC Innovative Plastics Ultem 1010KM PEI (Europe-Africa-Middle East)
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
ASTM C177
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK)
KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha..
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
ISO 8302
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA
NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance.
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
ISO 8302
SABIC Innovative Plastics NORYL HF185 PPE+HIPS (Europe-Africa-Middle East)
NORYL HF185 is an unfilled, halogen free (according VDE/DIN 472 part 815), flame retardant and easy flow NORYL grade.
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
ISO 8302
SABIC Innovative Plastics ULTEM 1000EF PEI
Transparent, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
ISO 8302
SABIC Innovative Plastics ULTEM 1000EF PEI (Asia Pacific)
Transparent, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
DIN 52612 Part 1
Borealis Beta-PPR™ RA7050-GN Polypropylene-Random-Copolymer for Pressure Pipe Systems
Beta-PPR RA7050-GN is a PP-RCT, a Polypropylene-Random-Copolymer with an enhanced Crystalline structure brought about by a special ß-nucleation and with an improved Temperature resistance. Proof o..
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
DIN 52612
Borealis RA130E-1498 Polypropylene Random Copolymer
RA130E-1498 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is white colored. Applications: RA130E-1498 is recommended for the production of PP-R p..
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
Eastman Eastar EN058 PET Copolymer
ISO data as provided by the manufacturer, Eastman Chemical
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
DuPont™ Surlyn® 9020 Ionomer Resin, Zinc
Surlyn® 9020 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The resin contains an addit..
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
Moulding Direction; ASTM C177
Dalau Dalcon 020 Virgin PTFE, Carbon (Anti-Static)
Applications & Industries: General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs. Electrical: Ideal for Anti - Static Applications; Anti -..
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
Hippe PET Polyethylene Terephthalate
Linear, saturated polyesters are thermoplastics which are used where good dimensional accuracy, high creep resistance and good sliding and wear behavior are required. Partially crystallized PET pos..
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
ASTM C 177
Adamas Adalon® 991 PTFE
Information provided by Adamas, HPM
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
ASTM C 177
Adamas Adalon® 998 PTFE, Turquoise
Information provided by Adamas, HPM
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
ASTM C177
Daikin NEOFLON EP-541 ETFE Pellets
Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl..
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
ASTM C177
Solvay Specialty Polymers Algoflon® A.15 PTFE (Polytetrafluoroethylene)  (discontinued **)
Data provided by the manufacturer.Type IV.G.1 Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric p..
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
ASTM C177
Solvay Specialty Polymers Algoflon® A.27 PTFE (Polytetrafluoroethylene)  (discontinued **)
Data provided by the manufacturer.Type IV.G.2 (except elongation at break) Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high iner..
Thermal Conductivity 0.240 W/m-K

@Temperature 280 °C
1.67 BTU-in/hr-ft²-°F

@Temperature 536 °F
Pyrotek ISOCAST Insulating Refractory Castable
Pyrotek's Isocast is a refractory castable based on phosphate bonded calcium silicate material. Isocast exhibits excellent thermal insulation characteristics and very good behavior with respec..
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
ISO 8302
SABIC Innovative Plastics NORYL FN150 PPE+HIPS (Europe-Africa-Middle East)
NORYL FN150 twin wall foam meets UL standard 94 V-0/5V ratings at 4 mm wall thickness. These unique flammability characteristics make FN150 the supreme choice for designing optimum wall thickness in..
Copyright © lookpolymers.com All Rights Reserved