Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 0.250 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Thermal Conductivity 0.240 - 0.250 W/m-K
1.67 - 1.74 BTU-in/hr-ft²-°F
Average value: 0.246 W/m-K Grade Count:5
Overview of materials for Polyetheretherketone, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values..
Thermal Conductivity 0.170 - 0.250 W/m-K
1.18 - 1.74 BTU-in/hr-ft²-°F
Average value: 0.201 W/m-K Grade Count:11
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Thermal Conductivity 0.190 - 0.250 W/m-K
1.32 - 1.74 BTU-in/hr-ft²-°F
Average value: 0.238 W/m-K Grade Count:11
Overview of materials for Fluorinated Ethylene Propylene (FEP), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Fluorinated Ethylene Propylene (FEP), Molded/Extruded". Each property range of values reported is minimu..
Thermal Conductivity 0.150 - 0.250 W/m-K
<br>@Temperature 40.0 °C
1.04 - 1.74 BTU-in/hr-ft²-°F
<br>@Temperature 104 °F
ASTM C177
Solvay Specialty Polymers Hyflon® PFA 125 Perfluoroalkoxy (PFA)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res..
Thermal Conductivity 0.190 - 0.250 W/m-K
1.32 - 1.74 BTU-in/hr-ft²-°F
ASTM C177
Zeus FEP Tubing
FEP, fluorinated ethylene propylene, is a melt processable fluoropolymer that allows for long, continuous lengths and has several distinct advantages over PTFE. Applications where FEP tubing is usua..
Thermal Conductivity 0.150 - 0.250 W/m-K
1.04 - 1.74 BTU-in/hr-ft²-°F
ASTM C177
Zeus PFA Tubing
PFA, or perfluoroalkoxy, is well recognized for its ability to maintain mechanical integrity in extreme temperatures even when exposed to caustic chemicals. PFA comes in high purity versions that ar..
Thermal Conductivity 0.230 - 0.250 W/m-K
1.60 - 1.74 BTU-in/hr-ft²-°F
Average value: 0.244 W/m-K Grade Count:15
Overview of materials for Ionomer, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma..