| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Thermal Conductivity | 0.360 - 0.504 W/m-K | 2.50 - 3.50 BTU-in/hr-ft²-°F | ASTM C-177 |
| Technetics Group Texolon™ 9406 PTFE
(Unverified Data**) General purpose 25% glass filled PTFE for applications less demandingPTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surface EnergyLow Diel.. |
|||
| Thermal Conductivity | 0.300 - 0.504 W/m-K | 2.08 - 3.50 BTU-in/hr-ft²-°F | Average value: 0.422 W/m-K Grade Count:11 |
| Overview of materials for Nylon 66, Glass Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum.. |
|||
| Thermal Conductivity | 0.250 - 0.504 W/m-K | 1.74 - 3.50 BTU-in/hr-ft²-°F | Average value: 0.374 W/m-K Grade Count:7 |
| Overview of materials for Nylon 66, Glass/Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of.. |
|||
| Thermal Conductivity | 0.360 - 0.504 W/m-K | 2.50 - 3.50 BTU-in/hr-ft²-°F | ASTM C177 |
| Garlock 9405 PTFE Rubber Sheet, 25% Glass Filled Premium Grade 25% Glass-filled Skived PTFE SheetInformation provided by Garlock Rubber Technologies |
|||