| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Thermal Conductivity | 0.900 - 1.10 W/m-K | 6.25 - 7.63 BTU-in/hr-ft²-°F | ASTM E1461 |
|
Raschig Group 2557 AMC Polyester
Glass fiber reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, exceptional processability with short cycle time and low ..
|
|||
| Thermal Conductivity | 0.900 - 1.10 W/m-K | 6.25 - 7.63 BTU-in/hr-ft²-°F | ASTM E1461 |
|
Raschig Group 2567 AMC
Glass fiber-reinforced and inorganically filled polyester molding compound (UP) in various colors. Outstanding mechanical strength similar to BMC/SMC, very good electrical isolation properties and ..
|
|||
| Thermal Conductivity | 0.900 - 1.10 W/m-K | 6.25 - 7.63 BTU-in/hr-ft²-°F | ASTM E1461 |
|
Raschig Group 2568 AMC
Glass fiber-reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, heat resistant up to 500°C for short time - usable for s..
|
|||
| Thermal Conductivity | 0.900 - 1.10 W/m-K | 6.25 - 7.63 BTU-in/hr-ft²-°F | ASTM E1461 |
|
Raschig Group 2572 AMC
Glass fiber reinforced Polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, good abrasion stability, high flame retardance in combin..
|
|||
| Thermal Conductivity | 0.900 - 1.10 W/m-K | 6.25 - 7.63 BTU-in/hr-ft²-°F | ASTM E1461 |
|
Raschig Group 5553 DAP
Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona..
|
|||
| Thermal Conductivity | 0.900 - 1.10 W/m-K | 6.25 - 7.63 BTU-in/hr-ft²-°F | ASTM E1461 |
|
Raschig Group 5562 DAP
Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona..
|
|||
| Thermal Conductivity | 0.900 - 1.10 W/m-K | 6.25 - 7.63 BTU-in/hr-ft²-°F | ASTM E1461 |
|
Raschig Group 5563 DAP
Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona..
|
|||
| Thermal Conductivity | 0.900 - 1.10 W/m-K | 6.25 - 7.63 BTU-in/hr-ft²-°F | DIN 52 612 |
|
Raschig Group RALUPOL® 4385 UP
Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very high arc resistance, very high mechanical values. This product meets the allowed upper limits for heavy..
|
|||
| Thermal Conductivity | 0.900 - 1.10 W/m-K | 6.25 - 7.63 BTU-in/hr-ft²-°F | ASTM E1461 |
|
Raschig Group RALUPOL® 4566 UP Polyester
Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u..
|
|||
| Thermal Conductivity | 0.900 - 1.10 W/m-K | 6.25 - 7.63 BTU-in/hr-ft²-°F | ASTM E1461 |
|
Raschig Group RALUPOL® 4802 UP Polyester
Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u..
|
|||
| Thermal Conductivity | 0.900 - 1.10 W/m-K | 6.25 - 7.63 BTU-in/hr-ft²-°F | DIN 52 612 |
|
Raschig Group RALUPOL® 4806 UP
Glass-fiber reinforced polyester molding compound. Very low mold shrinkage and post-shrinkage, very good mechanical strength, very good electrical values, better performance values compared to UP 80..
|
|||
| Thermal Conductivity | 0.280 - 1.10 W/m-K | 1.94 - 7.63 BTU-in/hr-ft²-°F | Average value: 0.500 W/m-K Grade Count:19 |
|
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor..
|
|||
| Thermal Conductivity | 0.900 - 1.10 W/m-K | 6.25 - 7.63 BTU-in/hr-ft²-°F | ASTM E1461 |
|
Raschig Group RALUPOL® 802 UP Polyester
Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength, good heat resistance. This product meets the allowed up..
|
|||
| Thermal Conductivity | 0.900 - 1.10 W/m-K | 6.25 - 7.63 BTU-in/hr-ft²-°F | ASTM E1461 |
|
Raschig Group RALUPOL® 804 UP Polyester
Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy m..
|
|||
| Thermal Conductivity | 0.900 - 1.10 W/m-K | 6.25 - 7.63 BTU-in/hr-ft²-°F | ASTM E1461 |
|
Raschig Group SURAPLAST 54 UPA
Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for..
|
|||
| Thermal Conductivity | 0.900 - 1.10 W/m-K | 6.25 - 7.63 BTU-in/hr-ft²-°F | ASTM E1461 |
|
Raschig Group SURAPLAST UPA 63 UP
Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for..
|
|||
| Thermal Conductivity | 0.146 - 1.10 W/m-K | 1.01 - 7.63 BTU-in/hr-ft²-°F | Average value: 0.334 W/m-K Grade Count:40 |
|
Overview of materials for Silicone, RTV, Encapsulation Grade
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Encapsulation Grade". Each property range of values reported is minimum and maximum value..
|
|||
| Thermal Conductivity | 0.280 - 1.10 W/m-K | 1.94 - 7.63 BTU-in/hr-ft²-°F | Average value: 0.553 W/m-K Grade Count:3 |
|
Overview of materials for Nylon 612, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp..
|
|||
| Thermal Conductivity | 0.900 - 1.10 W/m-K | 6.25 - 7.63 BTU-in/hr-ft²-°F | ASTM E1461 |
|
Raschig Group 5567 DAP Diallyl Phthalate (DAP), Cast, Mineral Filler
Glass-fiber reinforced diallyl phthalate molding compound free from halogens. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exc..
|
|||
| Thermal Conductivity | 0.900 - 1.10 W/m-K | 6.25 - 7.63 BTU-in/hr-ft²-°F | ASTM E1461 |
|
Raschig Group RALUPOL® 8605 UP Polyester
Glass fiber reinforced polyester molding compound. Resistant to hydrolysis. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU dire..
|
|||