| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Thermal Conductivity | 0.128 - 0.200 W/m-K | 0.888 - 1.39 BTU-in/hr-ft²-°F | Average value: 0.161 W/m-K Grade Count:5 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i..
|
|||
| Thermal Conductivity | 0.150 - 0.200 W/m-K | 1.04 - 1.39 BTU-in/hr-ft²-°F | Average value: 0.190 W/m-K Grade Count:5 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is ..
|
|||
| Thermal Conductivity | 0.150 - 0.200 W/m-K | 1.04 - 1.39 BTU-in/hr-ft²-°F | Average value: 0.172 W/m-K Grade Count:4 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and ..
|
|||
| Thermal Conductivity | 0.173 - 0.200 W/m-K | 1.20 - 1.39 BTU-in/hr-ft²-°F | Average value: 0.187 W/m-K Grade Count:4 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep..
|
|||
| Thermal Conductivity | 0.173 - 0.200 W/m-K | 1.20 - 1.39 BTU-in/hr-ft²-°F | Average value: 0.191 W/m-K Grade Count:5 |
|
Overview of materials for Polycarbonate, Optical Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a..
|
|||
| Thermal Conductivity | 0.167 - 0.201 W/m-K | 1.16 - 1.39 BTU-in/hr-ft²-°F | |
|
Abatron AboCast/AboCure 50-24/8501-4 High Temperature Resistant Epoxy
Clear amber, low viscosity, structural/dielectric epoxy with high temperature resistance.Suggested Uses: Casting, bonding, potting, encapsulation of electric, structural and industrial components to..
|
|||
| Thermal Conductivity | 0.170 - 0.200 W/m-K | 1.18 - 1.39 BTU-in/hr-ft²-°F | |
|
Abatron AboCast/AboCure 8109-1
High melting point.Processing: 100/30 pbw; mix at 130-140°C (270 °F); cures in 16 h/120°C (250°F), 10 h/140°C (285°F), 8 h/160°C (320°F), 2 h/ 200°C (390°F).Applications: Heavy duty castin..
|
|||
| Thermal Conductivity | 0.167 - 0.201 W/m-K | 1.16 - 1.39 BTU-in/hr-ft²-°F | |
|
Abatron AboCast/AboCure 8502-1 Epoxy
AboCast/AboCure 8502-1 is a solventless clear Epoxy System, used as a casting, adhesive, and impregnating resin for transformers, capacitors, coils, and other electronic components requiring a low-v..
|
|||
| Thermal Conductivity | 0.167 - 0.201 W/m-K | 1.16 - 1.39 BTU-in/hr-ft²-°F | |
|
Abatron AboCast 8103-13 One-Component Epoxy
AboCast 8103-13 is the low-viscosity one-component clear epoxy system with deep impregnation that offers high performance at relatively high temperatures. It is best for thin-wall casting. Suggested..
|
|||
| Thermal Conductivity | 0.167 - 0.201 W/m-K | 1.16 - 1.39 BTU-in/hr-ft²-°F | |
|
Abatron AboCast 8501-6 One-Component Epoxy
AboCast 8501-6 is a clear, high-temperature one-component epoxy system for very high-temperature uses. It offers the highest heat resistance of the clear resins. Suggested Uses: Casting; Potting; E..
|
|||
| Thermal Conductivity | 0.167 - 0.201 W/m-K | 1.16 - 1.39 BTU-in/hr-ft²-°F | |
|
Abatron AboCast 8504-1 One-Component Epoxy
AboCast 8504-1 is a clear, all-purpose one-component epoxy system, with an optimum balance of properties for most casting, adhesive, impregnation, and coating applications.
|
|||
| Thermal Conductivity | 0.167 - 0.201 W/m-K | 1.16 - 1.39 BTU-in/hr-ft²-°F | |
|
Abatron AboCast 8504-5 One-Component Epoxy
AboCast 8504-5 is a clear, plasticized one-component epoxy system with very high strength and impact. It provides exceptional physical properties and thermal shock resistance from sub-zero to modera..
|
|||
| Thermal Conductivity | 0.167 - 0.201 W/m-K | 1.16 - 1.39 BTU-in/hr-ft²-°F | |
|
Abatron AboCast/AboCure 8501-6/8501-4 High Temperature Resistant Epoxy
1-component system. Clear amber, low viscosity, structural/dielectric epoxy.Processing: Pot Life: 5-9 months. Cured 2 hours at 95°C + 15 hour post-cure at 230°C. Information provided by Abatron...
|
|||
| Thermal Conductivity |
0.200
-
0.200
W/m-K @Temperature 150 - 150 °C |
1.39
-
1.39
BTU-in/hr-ft²-°F @Temperature 302 - 302 °F |
Average value: 0.200 W/m-K Grade Count:8 |
|
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max..
|
|||
| Thermal Conductivity | 0.187 - 0.200 W/m-K | 1.30 - 1.39 BTU-in/hr-ft²-°F | Average value: 0.199 W/m-K Grade Count:9 |
|
Overview of materials for Polycarbonate, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app..
|
|||
| Thermal Conductivity | 0.167 - 0.201 W/m-K | 1.16 - 1.39 BTU-in/hr-ft²-°F | |
|
Abatron AboCast/AboCure 50-7/8501-4 High Temperature Resistant Epoxy
Clear amber, high viscosity, structural/dielectric epoxy with high temperature resistance.Suggested Uses: Casting, bonding, potting, encapsulation of electric, structural and industrial components t..
|
|||