| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Thermal Conductivity |
27.5
W/m-K @Temperature 1000 °C |
191
BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
|
Outokumpu 4828 High Temperature Austenitic Stainless Steel
Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and ..
|
|||
| Thermal Conductivity |
27.5
W/m-K @Temperature 1000 °C |
191
BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
|
Outokumpu 4833 High Temperature Austenitic Stainless Steel
Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and ..
|
|||
| Thermal Conductivity |
27.5
W/m-K @Temperature 1000 °C |
191
BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
|
Outokumpu 4878 High Temperature Austenitic Stainless Steel
Heat-resistant variant of 1.4541, with a slightly higher max carbon content. Recommended max service temperature for this steel in dry air is 800°C. Applications: Heat and creep resistance. For ..
|
|||
| Thermal Conductivity |
27.5
W/m-K @Temperature 1000 °C |
191
BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
|
Haynes 242® alloy, cold reduced sheet, annealed, 20% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
|
|||
| Thermal Conductivity |
27.5
W/m-K @Temperature 1000 °C |
191
BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
|
Haynes 242® alloy, cold reduced sheet, annealed
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
|
|||
| Thermal Conductivity |
27.5
W/m-K @Temperature 1000 °C |
191
BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
|
Haynes 242® alloy, cold reduced sheet, annealed and 20% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
|
|||
| Thermal Conductivity |
27.5
W/m-K @Temperature 1000 °C |
191
BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
|
Haynes 242® alloy, cold reduced sheet, annealed and 40% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
|
|||
| Thermal Conductivity |
27.5
W/m-K @Temperature 1000 °C |
191
BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
|
Haynes 242® alloy, cold reduced sheet, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
|
|||
| Thermal Conductivity |
27.5
W/m-K @Temperature 1000 °C |
191
BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
|
Haynes Hastelloy® B-3® alloy, 0% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
|
|||
| Thermal Conductivity |
27.5
W/m-K @Temperature 1000 °C |
191
BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
|
Haynes Hastelloy® B-3® alloy, 10% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
|
|||
| Thermal Conductivity |
27.5
W/m-K @Temperature 1000 °C |
191
BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
|
Haynes Hastelloy® B-3® alloy, 20% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
|
|||
| Thermal Conductivity |
27.5
W/m-K @Temperature 1000 °C |
191
BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
|
Haynes Hastelloy® B-3® alloy, 30% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
|
|||
| Thermal Conductivity |
27.5
W/m-K @Temperature 1000 °C |
191
BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
|
Haynes Hastelloy® B-3® alloy, 40% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
|
|||
| Thermal Conductivity |
27.5
W/m-K @Temperature 1000 °C |
191
BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
|
Haynes Hastelloy® B-3® alloy, 50% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
|
|||
| Thermal Conductivity | 27.5 W/m-K | 191 BTU-in/hr-ft²-°F | ASTM-C408 |
|
CoorsTek CAP 4 98.5% Alumina Ceramic Armor Material
CoorsTek CeraShield™ ceramics provide: low weight, high hardness, controlled, uniform microstructure, dimensional stability over wide temperature range, compatibility for use in finished armor sys..
|
|||
| Thermal Conductivity | 27.5 W/m-K | 191 BTU-in/hr-ft²-°F | ASTM-C408 |
|
CoorsTek FG-98 98% Alumina Ceramic Armor Material
CoorsTek CeraShield™ ceramics provide: low weight, high hardness, controlled, uniform microstructure, dimensional stability over wide temperature range, compatibility for use in finished armor sys..
|
|||
| Thermal Conductivity | 27.5 W/m-K | 191 BTU-in/hr-ft²-°F | ASTM C408 |
|
CoorsTek FG-995 Alumina (nom. 98.5% Al2O3)
Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
|
|||
| Thermal Conductivity |
27.5
W/m-K @Temperature 1000 °C |
191
BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
|
Haynes Hastelloy® B-3® alloy, heat treated at 1065°C, rapid quenched
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ea..
|
|||