| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Thermal Conductivity | 0.360 W/m-K | 2.50 BTU-in/hr-ft²-°F | |
|
Premix Premi-Glas® 2206-25 CR-SX Fiberglass Reinforced Thermoset SMC
Premi-Glas® 2206-25 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f..
|
|||
| Thermal Conductivity | 0.360 W/m-K | 2.50 BTU-in/hr-ft²-°F | |
|
Pyrotek Hirolex HG Electrical Insulating Material
Hirolex HG has superior mechanical properties. It is highly resistant to thermal shock, non-flammable and offers good arc resistance.Information provided by Pyrotek.
|
|||
| Thermal Conductivity | 0.360 W/m-K | 2.50 BTU-in/hr-ft²-°F | |
|
Resinlab® EP1320LV Heat Cure Epoxy Conformal Coating
Resinlab™ EP1320 and EP1320LV are one part heat cure epoxy conformal coatings. They can also be used as a small mass potting compounds, structural adhesives, or insulating polymer systems where the..
|
|||
| Thermal Conductivity | 0.360 W/m-K | 2.50 BTU-in/hr-ft²-°F | ASTM E1530 |
|
Solvay Specialty Polymers AvaSpire® AV-651 CF30 Polyaryletherketone (PAEK)
(Unverified Data**)
AvaSpire AV-651 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-651. This formulation offers some advantages relative to 30% carbon fiber reinforced PEEK which include better dimensiona..
|
|||
| Thermal Conductivity | 0.360 W/m-K | 2.50 BTU-in/hr-ft²-°F | ASTM E1530 |
|
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK)
(Unverified Data**)
Ketaspire KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provided.In..
|
|||
| Thermal Conductivity | 0.360 W/m-K | 2.50 BTU-in/hr-ft²-°F | ASTM F433 |
|
Quadrant EPP Duratron® PAI T5030 Polyamide-imide, glass reinforced, extruded (ASTM Product Data Sheet) |
|||
| Thermal Conductivity |
0.360
W/m-K @Temperature 23.9 °C |
2.50
BTU-in/hr-ft²-°F @Temperature 75.0 °F |
ASTM F-433 |
|
PBI Performance Products Celazole® TF-60 V Glass Fiber Reinforced Melt Processable Polybenzimidazole
Celazole® polybenzimidazole (PBI) resin is a unique and highly stable linear hetrocyclic polymer. PBI is characterized by high strength; excellent thermal stability, and broad chemical resistance. ..
|
|||
| Thermal Conductivity | >= 0.360 W/m-K | >= 2.50 BTU-in/hr-ft²-°F | ASTM C177 |
|
PolyOne Edgetek® PF-40GF/000 Polysulfone, Glass Filled
(discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||
| Thermal Conductivity | 0.360 - 0.360 W/m-K | 2.50 - 2.50 BTU-in/hr-ft²-°F | Average value: 0.360 W/m-K Grade Count:4 |
|
Overview of materials for Polyamide-Imide, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Glass Filled". Each property range of values reported is minimum and maximum values of ..
|
|||
| Thermal Conductivity | 0.360 - 1.22 W/m-K | 2.50 - 8.47 BTU-in/hr-ft²-°F | Average value: 0.644 W/m-K Grade Count:14 |
|
Overview of materials for Phenolic, Novolac, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Glass Filled". Each property range of values reported is minimum and maximum values o..
|
|||
| Thermal Conductivity | 0.360 - 0.504 W/m-K | 2.50 - 3.50 BTU-in/hr-ft²-°F | ASTM C-177 |
|
Technetics Group Texolon™ 9406 PTFE
(Unverified Data**)
General purpose 25% glass filled PTFE for applications less demandingPTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surface EnergyLow Diel..
|
|||
| Thermal Conductivity | 0.360 W/m-K | 2.50 BTU-in/hr-ft²-°F | ASTM C177 |
|
Solvay Specialty Polymers AvaSpire® AV-651 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber
AvaSpire® AV-651 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-651. This formulation offers some advantages relative to 30% carbon fiber reinforced PEEK which include better di..
|
|||
| Thermal Conductivity |
<=
0.360
W/m-K @Temperature 500 °C |
<=
2.50
BTU-in/hr-ft²-°F @Temperature 932 °F |
|
|
Sharadaa Ceramics REFINSUL ZAP-017 Insulating Castables
Description: We provide our clients a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for l..
|
|||
| Thermal Conductivity |
0.360
W/m-K @Temperature 100 °C |
2.50
BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1461 |
|
Plenco 2300 Phenolic, Granular, Compression Molded
PLENCO 02300 is a general purpose organic filled molding compound formulated to offer excellent processability while maintaining mechanical strength values. UL recognized under component file E40654..
|
|||
| Thermal Conductivity |
0.360
W/m-K @Temperature 100 °C |
2.50
BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1461 |
|
Plenco 7500 Phenolic, Granular, Compression Molded
PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi..
|
|||
| Thermal Conductivity | 0.360 W/m-K | 2.50 BTU-in/hr-ft²-°F | DIN 52612 |
|
BASF Ultramid® B3EG6 30% Glass Filled PA6 (Conditioned)
Ultramid B3EG6 is a 30% glass fiber reinforced injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500.
|
|||
| Thermal Conductivity | 0.360 W/m-K | 2.50 BTU-in/hr-ft²-°F | DIN 52612 |
|
BASF Ultramid® B3EG6 30% Glass Filled PA6 (Dry)
Ultramid B3EG6 is a 30% glass fiber reinforced injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500.
|
|||
| Thermal Conductivity | 0.360 W/m-K | 2.50 BTU-in/hr-ft²-°F | DIN 52612-1 |
|
BASF Ultramid® B3EG6 LS BK 23189 30% Glass Filled PA6 (Conditioned)
Information provided by BASF
|
|||
| Thermal Conductivity | 0.360 W/m-K | 2.50 BTU-in/hr-ft²-°F | DIN 52612-1 |
|
BASF Ultramid® B3EG7 35% Glass Filled PA6 (Conditioned)
Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF
|
|||
| Thermal Conductivity | 0.360 W/m-K | 2.50 BTU-in/hr-ft²-°F | DIN 52612-1 |
|
BASF Ultramid® B3EG7 35% Glass Filled PA6 (Dry)
Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF
|
|||
| Thermal Conductivity | 0.360 W/m-K | 2.50 BTU-in/hr-ft²-°F | DIN 52612-1 |
|
BASF Ultramid® B3EG7 BK 00564 35% Glass Filled PA6 (Conditioned)
Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF
|
|||
| Thermal Conductivity | 0.360 W/m-K | 2.50 BTU-in/hr-ft²-°F | DIN 52612 |
|
BASF Ultramid® B3WG7 BK 00564 35% Glass Filled PA6 (Conditioned)
Description: 35% glass-fiber reinforced and heat aging resistant injection-molding grade, e.g. for automotive manifolds and pedals.Information provided by BASF
|
|||
| Thermal Conductivity | 0.360 W/m-K | 2.50 BTU-in/hr-ft²-°F | DIN 52612 |
|
BASF Ultramid® B3ZG8 BK 20560 40% Glass Filled PA6-1 (Conditioned)
Description: Impact-modified and 40% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness and toughness, for instance, for vehicle airbag housings and suitcas..
|
|||
| Thermal Conductivity | 0.360 W/m-K | 2.50 BTU-in/hr-ft²-°F | DIN 52612 |
|
BASF Ultramid® B3WG6 BK00564 30% Glass Filled PA6 (Conditioned)
Ultramid B3WG6 BK00564 is a 30% glass fiber reinforced, pigmented black, heat stabilized injection molding PA6 grade.
|
|||
| Thermal Conductivity | 0.360 W/m-K | 2.50 BTU-in/hr-ft²-°F | ASTM C-518 |
|
Sumitomo Bakelite North America FS-10-VO-200-P Short-Glass Reinforced Diallyl Phthalate
Short glass fiber reinforced, flame retardant, diallyl meta-phthalate molding compound with excellent heat resistance.Meets the requirements of ASTM D5948 Type SIG-F.Information provided by Vyncolit..
|
|||
| Thermal Conductivity | 0.360 W/m-K | 2.50 BTU-in/hr-ft²-°F | ASTM C-518 |
|
Sumitomo Bakelite North America FS-5 Short-Glass Reinforced Diallyl Phthalate
Short glass fiber reinforced, non-flame retardant, diallyl meta-phthalate molding compound which meets the requirements of ASTM D5948 TYPE SIG.Information provided by Vyncolit, a Sumitomo Bak Group
|
|||
| Thermal Conductivity | 0.360 W/m-K | 2.50 BTU-in/hr-ft²-°F | Product Property; ASTM E 1530 |
|
Arlon R36601A010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate
Description: Generation II Thermabond® NP electrically insulating electronic adhesive. Bonds without primer.Design/Construction: Liner 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Sty..
|
|||
| Thermal Conductivity | 0.360 W/m-K | 2.50 BTU-in/hr-ft²-°F | DIN 52612 |
|
BASF Ultramid® B3WG6 30% Glass Filled PA6 (Dry)
Ultramid B3WG6 is a 30% glass fiber reinforced, heat stabilized injection molding PA6 grade.
|
|||
| Thermal Conductivity | 0.360 W/m-K | 2.50 BTU-in/hr-ft²-°F | DIN 52612 |
|
BASF Ultramid® B3WG6 BK00564 30% Glass Filled PA6 (Dry)
Ultramid B3WG6 BK00564 is a 30% glass fiber reinforced, pigmented black, heat stabilized injection molding PA6 grade.
|
|||