| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Thermal Conductivity | 0.400 - 0.500 W/m-K | 2.78 - 3.47 BTU-in/hr-ft²-°F | ASTM E1461 |
|
Raschig Group MELOPAS® 2010 MF Melamine
Organically and inorganically filled Melamine molding compound. Excellent surface hardness, good mechanical strength, good electrical properties. This product meets the allowed upper limits for heav..
|
|||
| Thermal Conductivity | 0.400 - 0.500 W/m-K | 2.78 - 3.47 BTU-in/hr-ft²-°F | ASTM E1461 |
|
Raschig Group MELOPAS® 6605 MP Melamine
Cellulose reinforced Melamine molding compound. Very good electrical properties, excellent surface hardness, good mechanical strength and heat resistance, good wear and UV-stability, good gliding be..
|
|||
| Thermal Conductivity | 0.400 - 0.500 W/m-K | 2.78 - 3.47 BTU-in/hr-ft²-°F | ASTM E1461 |
|
Raschig Group MELOPLAS® 150 MF
Wood flour-reinforced MF molding compound in dark colors. High surface hardness, high mechanical strength, good electrical properties. Self-extinguishing (V-O/1,6 according to UL 94), UL-listed. Fr..
|
|||
| Thermal Conductivity | 0.400 - 0.500 W/m-K | 2.78 - 3.47 BTU-in/hr-ft²-°F | ASTM E1461 |
|
Raschig Group MELOPLAS® 152 MF
Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al..
|
|||
| Thermal Conductivity | 0.400 - 0.500 W/m-K | 2.78 - 3.47 BTU-in/hr-ft²-°F | DIN 52 612 |
|
Raschig Group MELOPLAS® 152.7 MF
Cellulose-reinforced MF molding compound in white and colored shades. High surface hardness, very good UV stability, very good resistance to chemicals also to foodstuff ingredients, physiologically..
|
|||
| Thermal Conductivity | 0.400 - 0.500 W/m-K | 2.78 - 3.47 BTU-in/hr-ft²-°F | ASTM E1461 |
|
Raschig Group MELOPLAS® 181.5 MF
Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. Very good electrical properties, high surface hardness, good mechanical strength, high UV and heat resis..
|
|||
| Thermal Conductivity | 0.400 - 0.500 W/m-K | 2.78 - 3.47 BTU-in/hr-ft²-°F | ASTM E1461 |
|
Raschig Group MELOPLAS® 182 MF
Wood flour-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in dark colors. Improved dimensional stability and electrical properties as compared with MP 180, high surf..
|
|||
| Thermal Conductivity | 0.400 - 0.500 W/m-K | 2.78 - 3.47 BTU-in/hr-ft²-°F | ASTM E1461 |
|
Raschig Group MELOPLAS® 183 MF
Cellulose-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in white and colored shades. Improved dimensional stability and electrical properties as compared with MP 18..
|
|||
| Thermal Conductivity | 0.400 - 0.500 W/m-K | 2.78 - 3.47 BTU-in/hr-ft²-°F | DIN 52 612 |
|
Raschig Group MELOPLAS® 2500 MF
Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al..
|
|||
| Thermal Conductivity | 0.400 - 0.500 W/m-K | 2.78 - 3.47 BTU-in/hr-ft²-°F | ASTM E1461 |
|
Raschig Group MELOPLAS® 3025 MF
Cellulose-reinforced and inorganically filled MF molding compound in white and colored shades. High surface hardness, good UV and heat stability, very good resistance to chemicals - also to foodstu..
|
|||
| Thermal Conductivity | 0.176 - 0.500 W/m-K | 1.22 - 3.47 BTU-in/hr-ft²-°F | Average value: 0.271 W/m-K Grade Count:5 |
|
Overview of materials for Polyetherimide (PEI), 10% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 10% Glass Fiber". Specific grades with glass content between 5% and 14% are included. Ea..
|
|||
| Thermal Conductivity | 0.230 - 0.500 W/m-K | 1.60 - 3.47 BTU-in/hr-ft²-°F | Average value: 0.261 W/m-K Grade Count:39 |
|
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v..
|
|||
| Thermal Conductivity | 0.300 - 0.500 W/m-K | 2.08 - 3.47 BTU-in/hr-ft²-°F | Average value: 0.385 W/m-K Grade Count:6 |
|
Overview of materials for Nylon 6, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a..
|
|||
| Thermal Conductivity | 0.300 - 0.500 W/m-K | 2.08 - 3.47 BTU-in/hr-ft²-°F | ASTM E1461 |
|
Park Electrochemical Nelco® N4000-12 High Speed/Low Loss, CAF Resistant Laminate and Prepreg
The Nelco® N4000-12 series is an enhanced epoxy resin system designed for use in high speed, low loss applications requiring thermal stability, excellent signal speed and CAF resistance.Key Feature..
|
|||