Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 4.86 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Thermal Conductivity 0.700 W/m-K

@Temperature 80.0 °C
4.86 BTU-in/hr-ft²-°F

@Temperature 176 °F
ASTM C518
Rogers Corporation TMM® TMM4 Ceramic Thermoset Polymer Composite
TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope..
Thermal Conductivity 0.700 W/m-K
4.86 BTU-in/hr-ft²-°F
ASTM E1225
Proto3000 Duraform® PA Selective Laser Sintering (SLS®) Prototyping Polymer
Description: Durable polyamide (nylon) material for real-world physical testing and functional useFeatures: Excellent surface resolution and feature detailEasy-to-processCompliant with USP Class VI ..
Thermal Conductivity 0.700 W/m-K
4.86 BTU-in/hr-ft²-°F
ASTM D5470
Parker Chomerics PREMIER™ A240-FRHF EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Thermal Conductivity 0.700 - 0.900 W/m-K
4.86 - 6.25 BTU-in/hr-ft²-°F
ASTM E1461
Raschig Group EN 5004 Epoxy Molding Compound
Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo..
Thermal Conductivity 0.700 W/m-K
4.86 BTU-in/hr-ft²-°F
ASTM E1530
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK)  (Unverified Data**)
AV-755 SL45 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like the ot..
Thermal Conductivity 0.700 W/m-K
4.86 BTU-in/hr-ft²-°F
Cookson Group Plaskon® 3100LS Mineral Filled Conventional Encapsulant  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.A semiconductor grade encapsulant suitable for a wide range of applications ranging from small SOICs to moderate lead count DIPs...
Thermal Conductivity 0.700 W/m-K
4.86 BTU-in/hr-ft²-°F
Cookson Group Plaskon® 3300SH Mineral Filled Epoxy Molding Compound  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.Exhibits exceptional reliability, excellent moldability, good release characteristics and low flash. This compound is especially..
Thermal Conductivity 0.700 W/m-K
4.86 BTU-in/hr-ft²-°F
Cookson Group Plaskon® 3400FP Epoxy Molding Compound  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.A fast curing, reduced-stress epoxy molding compound for the encapsulation of semiconductor devices including DIPs, PLCCs, SOICs ..
Thermal Conductivity 0.700 W/m-K
4.86 BTU-in/hr-ft²-°F
Cookson Group Plaskon® SMT-B-1 LAS (146.408) Epoxy Molding Compound for PBGAs  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound optimized specifically for grid arrays (BGA/LGA) requiring low alpha particle count. It is formulated ..
Thermal Conductivity 0.700 W/m-K
4.86 BTU-in/hr-ft²-°F
DIN 52612
Lehmann & Voss LUVOCOM® 50/CF/30 Polycarbonate, with carbon fiber
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi..
Thermal Conductivity 0.700 W/m-K
4.86 BTU-in/hr-ft²-°F
DIN 52612
Fluorseals PTFE 25% carbon filled
Improved compressive strength, wear resistance and thermal conductivity.Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials.
Thermal Conductivity 0.700 W/m-K
4.86 BTU-in/hr-ft²-°F
Menzolit Menzolit® BMC 0900 Unsaturated Polyester UP
BMC 0900 is a special BMC used in a chemically aggressive environment. The glass content is set to a level that combines good mould ability with good strength and stiffness properties. Typical appli..
Thermal Conductivity 0.700 W/m-K
4.86 BTU-in/hr-ft²-°F
Menzolit Menzolit® BMC 1000 Unsaturated Polyester UP
BMC 1000 is a special BMC for hydrolysis resistant applications. The glass content is set to a level that provides sufficient mouldability with high strength and stiffness properties. Typical applic..
Thermal Conductivity 0.700 W/m-K
4.86 BTU-in/hr-ft²-°F
Menzolit Menzolit® MMC 1600 Unsaturated Polyester UP
MMC 1600 is a mineral moulding compound (similar to DMC/BMC) providing of a stone like appearance eg. granite or marble. Chrome plated mould surfaces are required. It is recommended that product thi..
Thermal Conductivity 0.700 W/m-K
4.86 BTU-in/hr-ft²-°F
Menzolit Menzolit® SMC 0390 Unsaturated Polyester UP
SMC 0390 is a standard low profile SMC. Because of its low shrinkage, the material shows good surface quality as well as very low warpage. The product is suitable for applications if a better surfac..
Thermal Conductivity 0.700 W/m-K
4.86 BTU-in/hr-ft²-°F
Menzolit Menzolit® SMC 0400 Unsaturated Polyester UP
SMC 0400 is a Class-A SMC for exterior body applications on cars, LCV´s and trucks. These compounds mould to parts with good up to excellent surface quality for medium bake in-line and off-line p..
Thermal Conductivity 0.700 W/m-K
4.86 BTU-in/hr-ft²-°F
Menzolit Menzolit® SMC 0520 Unsaturated Polyester UP
SMC 0520 is a special SMC with significantly reduced density. The glass level has been selected to combine good moulding with sufficient strength and stiffness properties. Even without a specific fi..
Thermal Conductivity 0.700 W/m-K
4.86 BTU-in/hr-ft²-°F
Menzolit Menzolit® SMC 1100 Unsaturated Polyester UP
SMC 1100 is a special vinylester SMC for high strength applications. The reinforcement has been put to a level that combines mouldability with high strength and stiffness properties. The specific re..
Thermal Conductivity 0.700 W/m-K
4.86 BTU-in/hr-ft²-°F
Menzolit Menzolit® SMC 1400 Unsaturated Polyester UP
SMC 1400 is a special SMC being used in the environment of a combustion engine. The glass level has been selected to combine good mouldability with good stiffness and strength properties. The produc..
Thermal Conductivity 0.700 W/m-K
4.86 BTU-in/hr-ft²-°F
Menzolit Menzolit® SMC 1650 Unsaturated Polyester UP
SMC 1650 is a specially designed anti-microbial polyester moulding compound which incorporates a "germ killer" . It has been tested and found to be compliant for resistance to fungal defacement in ..
Thermal Conductivity 0.700 W/m-K
4.86 BTU-in/hr-ft²-°F
Menzolit Menzolit® BMC 2300 Unsaturated Polyester UP
BMC 2300 is a special BMC with exceptional high fire retardancy. The glass content is set to a level that provides sufficient mouldability with high strength and stiffness properties. Fire retardanc..
Thermal Conductivity 0.700 W/m-K
4.86 BTU-in/hr-ft²-°F
Menzolit Menzolit® BMC 2910 Unsaturated Polyester UP
BMC 2910 incorporates additives which enhance the integral performance of mouldings during and after fire, currently used to mould Boltcaps which are designed to provide protection to the bolted co..
Thermal Conductivity 0.700 W/m-K
4.86 BTU-in/hr-ft²-°F
Menzolit Menzolit® BMC 3100 Unsaturated Polyester UP
BMC 3100 is a special BMC suitable for the use in head lamp reflectors. Because of its high temperature resistance and dimensional stability as well as low coefficient of thermal expansion, complex ..
Thermal Conductivity 0.700 W/m-K
4.86 BTU-in/hr-ft²-°F
Menzolit Menzolit® HPC 1300 Unsaturated Polyester UP
HPC 1300 is a special SMC for high strength applications. The glass level has been selected to combine mouldability with high strength and stiffness properties in orientation direction. The reinforc..
Thermal Conductivity 0.700 W/m-K
4.86 BTU-in/hr-ft²-°F
Menzolit Menzolit® SMC 0160 Unsaturated Polyester UP
SMC 0160 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets ..
Thermal Conductivity 0.700 W/m-K
4.86 BTU-in/hr-ft²-°F
Menzolit Menzolit® SMC 0190 Unsaturated Polyester UP
SMC 0190 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t..
Thermal Conductivity 0.700 W/m-K
4.86 BTU-in/hr-ft²-°F
Cookson Group Plaskon® 3300S Mineral Filled Novolac Epoxy Molding Compound  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.A low stress, flame retardant, novolac hardened epoxy molding compound designed to provide hermeticity protection exceeding that ..
Copyright © lookpolymers.com All Rights Reserved