| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Thermal Conductivity |
0.900
W/m-K <br>@Pressure 2.07 MPa
|
6.25
BTU-in/hr-ft²-°F <br>@Pressure 300 psi
|
ASTM D5470 |
|
Parker Chomerics CHO-SEAL 1401 Conductive Elastomer
High performance for non-corrosive environments; soft(45 Shore A) for low closure force where gasket geometry cannot be exploited; low tear strength; no fluid resistance. Molded and ExtrudedRoHS Com..
|
|||
| Thermal Conductivity | 0.900 W/m-K | 6.25 BTU-in/hr-ft²-°F | ASTM D5470 |
|
Parker Chomerics THERM-A-FORM 1641 Cure-in-Place Potting and Underfill Material
Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co..
|
|||
| Thermal Conductivity | 0.900 - 1.10 W/m-K | 6.25 - 7.63 BTU-in/hr-ft²-°F | ASTM E1461 |
|
Raschig Group 2568 AMC
Glass fiber-reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, heat resistant up to 500°C for short time - usable for s..
|
|||
| Thermal Conductivity | 0.900 - 1.10 W/m-K | 6.25 - 7.63 BTU-in/hr-ft²-°F | ASTM E1461 |
|
Raschig Group 2572 AMC
Glass fiber reinforced Polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, good abrasion stability, high flame retardance in combin..
|
|||
| Thermal Conductivity | 0.900 - 1.10 W/m-K | 6.25 - 7.63 BTU-in/hr-ft²-°F | ASTM E1461 |
|
Raschig Group 5562 DAP
Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona..
|
|||
| Thermal Conductivity | 0.900 - 1.00 W/m-K | 6.25 - 6.94 BTU-in/hr-ft²-°F | ASTM E1461 |
|
Raschig Group RALUPOL® 2100 UP Polyester
Organically and inorganically filled polyester molding compound. Low post-shrinkage, very good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy meta..
|
|||
| Thermal Conductivity | 0.900 - 1.10 W/m-K | 6.25 - 7.63 BTU-in/hr-ft²-°F | ASTM E1461 |
|
Raschig Group RALUPOL® 4802 UP Polyester
Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u..
|
|||
| Thermal Conductivity | 0.900 - 1.10 W/m-K | 6.25 - 7.63 BTU-in/hr-ft²-°F | DIN 52 612 |
|
Raschig Group RALUPOL® 4806 UP
Glass-fiber reinforced polyester molding compound. Very low mold shrinkage and post-shrinkage, very good mechanical strength, very good electrical values, better performance values compared to UP 80..
|
|||
| Thermal Conductivity | 0.900 W/m-K | 6.25 BTU-in/hr-ft²-°F | through-plane, ø80*3mm discs; ISO 22007-2 |
|
SABIC Innovative Plastics LNP KONDUIT OX11314 PPS (Asia Pacific)
Thermally conductive mineral filled PPS FR compound
|
|||
| Thermal Conductivity | 0.900 - 1.10 W/m-K | 6.25 - 7.63 BTU-in/hr-ft²-°F | ASTM E1461 |
|
Raschig Group RALUPOL® 804 UP Polyester
Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy m..
|
|||
| Thermal Conductivity | 0.900 - 1.10 W/m-K | 6.25 - 7.63 BTU-in/hr-ft²-°F | ASTM E1461 |
|
Raschig Group SURAPLAST 54 UPA
Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for..
|
|||
| Thermal Conductivity | 0.900 - 1.10 W/m-K | 6.25 - 7.63 BTU-in/hr-ft²-°F | ASTM E1461 |
|
Raschig Group SURAPLAST UPA 63 UP
Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for..
|
|||
| Thermal Conductivity | 0.900 W/m-K | 6.25 BTU-in/hr-ft²-°F | |
|
Cookson Group Plaskon® 2929BNSC Epoxy Molding Compound
(discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound for the encapsulation of semiconductor devices and fiber optics. Excellent moldability (good release, ..
|
|||
| Thermal Conductivity |
0.900
W/m-K <br>@Temperature 90.0 °C
|
6.25
BTU-in/hr-ft²-°F <br>@Temperature 194 °F
|
|
|
Schott Glass 8095 Lead Glass
Lead glass (28% PbO), electrically highly insulating, highly x-ray absorbing General electrotechnical applicationInformation provided by SCHOTT AG.
|
|||
| Thermal Conductivity |
0.900
W/m-K <br>@Temperature 90.0 °C
|
6.25
BTU-in/hr-ft²-°F <br>@Temperature 194 °F
|
|
|
Schott Glass 8652 Sealing Glass
Tungsten sealing glass, lower sealing temperature than glass 8651 Power diodesInformation provided by SCHOTT AG.
|
|||
| Thermal Conductivity | 0.900 W/m-K | 6.25 BTU-in/hr-ft²-°F | |
|
Dow Corning SE 4422 SILICONE RTV
One-part, grey, moisture cure RTV, flowable, thermally conductive, UL V-1.Information provided by Dow Corning
|
|||
| Thermal Conductivity | 0.900 W/m-K | 6.25 BTU-in/hr-ft²-°F | silicone property; Arlon SQA-TMS-022 |
|
Arlon Thermabond® 99180T010 Silicone Rubber/Fiberglass Laminate
Low outgassing, thermally conductive, electrically insulating, Thermabond®. Bonds with primer. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass.
|
|||
| Thermal Conductivity | 0.901 W/m-K | 6.25 BTU-in/hr-ft²-°F | uncured |
|
Atom Adhesives AA-DUCT 2979 Epoxy Adhesive
AA-DUCT 2979 is a fast curing one part epoxy adhesive with superior electrical conductivity and bonding capability. AA-DUCT 2979 has been shown to retain their properties through hundreds of hours o..
|
|||
| Thermal Conductivity | 0.900 - 1.10 W/m-K | 6.25 - 7.63 BTU-in/hr-ft²-°F | ASTM E1461 |
|
Raschig Group 5567 DAP Diallyl Phthalate (DAP), Cast, Mineral Filler
Glass-fiber reinforced diallyl phthalate molding compound free from halogens. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exc..
|
|||
| Thermal Conductivity | 0.900 - 1.10 W/m-K | 6.25 - 7.63 BTU-in/hr-ft²-°F | ASTM E1461 |
|
Raschig Group RALUPOL® 8605 UP Polyester
Glass fiber reinforced polyester molding compound. Resistant to hydrolysis. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU dire..
|
|||