| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 105 °C | 221 °F | UL Temperature Rating |
|
PolyOne Geon™ Vinyl Wire & Cable EHA70L Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | UL Temperature Rating |
|
PolyOne Geon™ Vinyl Wire & Cable W1213 Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | UL Temperature Rating |
|
PolyOne Geon™ Vinyl Wire & Cable W3200 Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | UL Temperature Rating; UL 1581 |
|
PolyOne OnFlex™ HFFR 310-01 Thermoplastic Elastomer (TPE)
OnFlex™ HFFR 310-01 is a non-halogen flame retardant material designed for cable jackets. New Product. Commercial specifications have not been established. - Non-halogen flame retardant - UL62 comp..
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous; 5,000 h |
|
Quadrant EPP Ertacetal® H-TF POM-H, PTFE-filled, extruded (ISO Data)
Ertacetal H-TF is a DELRIN® AF Blend, a combination of TEFLON® fibres evenly dispersed in a DELRIN acetal resin. Much of the strength that is inherent in Ertacetal H is retained. Some properties c..
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous; FRISETTA Test Method |
|
Nilit FRIANYL B63 W-SG-GV 2010 Nylon 6 for injection molding, 20% mineral filled, 10% glass fiber reinforced
Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | Softening Point |
|
Huntsman HT 939 Special Hardener
Mix Ratio with GY 6010 is 100 phr 35.Comments/Applications: Latent modified polyamide hardener. Excellent shelf life. Six month latency at RT. Excellent adhesion, good mechanicals, highly reacti..
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | |
|
Styrolution Luran® S KR 2864 C Colored ASA+PC
Description: Easy flowing injection molding grade with heat resistance for parts with thin walls and/or with adverse flowpath/wall thickness ratios.Applications: Mobile phone housings.Information pr..
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous Use; ASTM D794 |
|
Teknor Apex APEX® 7500-80 Polyvinyl Chloride, Flexible
Notes: 105°C General Purpose; RoHS Compliant Features: High Heat Resistance Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL..
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous Use; ASTM D794 |
|
Teknor Apex APEX® 80862 Polyvinyl Chloride, Semi-Rigid
Notes: 105°C Insulation; RoHS Compliant Features: High Heat Resistance; Semi-rigid Uses: Cable Jacketing; Insulation Agency Ratings: UL 1061 Forms: PelletsInformation Provided by Teknor Apex
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous Use; ASTM D794 |
|
Teknor Apex APEX® 92-A2292C-90 Polyvinyl Chloride, Flexible
Notes: 105°C General Purpose; RoHS Compliant Features: Flame Retardant; High Heat Resistance Uses: Cable JacketingForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54..
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous; UL-1581 |
|
Teknor Apex ELEXAR® EL 8421 Thermoplastic Elastomer
Information provided by Teknor Apex Company
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous Use; ASTM D794 |
|
Teknor Apex Flexalloy® 89501-83FR Polyvinyl Chloride, Elastomer
Notes: 105°C Insulation; RoHS Compliant Features: High Heat Resistance; Low Temperature Flexibility Uses Wet Rated Insulation Wire Types: NISPE-1; NISPE-2; SE; SEO; SEOW; SEW; SJE; SJEO; SJEOW; S..
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous Use; ASTM D794 |
|
Teknor Apex Flexalloy® 9602-72 Polyvinyl Chloride, Elastomer
Notes: 105°C Jacket; RoHS Compliant Features: Flame Retardant; High Heat Resistance; Low Temperature Flexibility; Sunlight Resistant (720 hours) Uses Cable Jacketing Wire Types: SEOW; SEW; SJEOW;..
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | Deflection temperature in bending , load unknown |
|
Sibur Discar-SL PC/ABS Compositional Polymer
Composition material PC/ABS with low viscosity of melting with high shock resistance, thermal and atmospheric resistance for large, thin wall structural parts of automobile interiors.
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous Use; ASTM D794 |
|
Teknor Apex APEX® 7500-90 Polyvinyl Chloride, Flexible
Notes: 105°C General Purpose; RoHS Compliant Features: High Heat Resistance Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL..
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | |
|
Trelleborg Emerson & Cuming Eccobond® 23 LV General Purpose Catalyst
Emerson & Cuming 23 LV Eccobond® General Purpose CatalystExcellent low temperature performance properties, excellent thermal shock/cycle and impact resistance. Good hardener for cryogenic applicati..
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | |
|
Trelleborg Emerson & Cuming Eccobond® 24 Two-Component High Strength-Impact Resistant Epoxy Adhesive
Emerson & Cuming 24 Eccobond® Two-Component High Strength-Impact Resistant Epoxy AdhesiveClear, low viscosity, room temperature curing, epoxy adhesive. Exhibits resilient bonds when joining dissimi..
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | |
|
Trelleborg Emerson & Cuming Stycast® E-1030 One-Component Epoxy Low Stress Encapsulant
Emerson & Cuming E-1030 Stycast® One-Component Epoxy Low Stress EncapsulantDesigned for the encapsulation of a wide range of stress sensitive electronics. They offer excellent performance at low te..
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | |
|
Trelleborg Emerson & Cuming Stycast® 2754 Two-Component Epoxy Flexible Low-Stress Encapsulant
Emerson & Cuming 2754 Stycast® Two-Component Epoxy Flexible Low-Stress EncapsulantDescriptionElectronic embedment and sealing of metals, ceramics, and plastics. Protection of stress sensitive compo..
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | |
|
Colorite Polymers Weatherflex™ CS1522WX (NTL01P) Wire and Cable Vinyl Compound
Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai..
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | |
|
Colorite Polymers Weatherflex™ CS1534WX (NTL02P) Wire and Cable Vinyl Compound
Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai..
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | Service |
|
3M FM041909 White Polyester Label Products
3M™ White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ Adhesive P1480, which ..
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous Use; ASTM D794 |
|
Teknor Apex APEX® 04-A0386B-88 Polyvinyl Chloride, Flexible
Notes: 105°C Insulation; RoHS Compliant Uses: Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | |
|
Colorite Polymers Weatherflex™ CS1522WX (NTL70B) Wire and Cable Vinyl Compound
Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai..
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous Use; ASTM D794 |
|
Teknor Apex APEX® 7500-85 Polyvinyl Chloride, Flexible
Notes: 105°C General Purpose; RoHS Compliant Features: High Heat Resistance Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL Q..
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous; UL-1581 |
|
Teknor Apex ELEXAR® EL 8732 Thermoplastic Elastomer
Information provided by Teknor Apex Company
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | |
|
3M Scotch® Super 33+™ Vinyl Electrical Tape
Scotch® Super 33+™ Vinyl Electrical Tape is a premium grade, 7 mil thick, all-weather vinyl-insulating tape. It is designed to perform continuously in ambient temperatures up to 105°C. The tape i..
|
|||
| Maximum Service Temperature, Air | <= 105 °C | <= 221 °F | |
|
Sylvin Technologies 6055 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.
|
|||
| Maximum Service Temperature, Air | <= 105 °C | <= 221 °F | |
|
Sylvin Technologies 6148-90 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.
|
|||