| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 110 °C | 230 °F | |
|
Precision Polymer Engineering N80L Nitrile Rubber
Nitrile Butadiene Rubber, 75-85 °IRHD. Low acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. To meet ASTM D2000 line call-out M6BG814, A14, B14, EO14, EO34, F17.Applications: T..
|
|||
| Maximum Service Temperature, Air | 110 °C | 230 °F | Continuous; FRISETTA Test Method |
|
Nilit FRIANYL A63 W-GV10 Nylon 6.6 for injection molding, 10% glass fiber reinforced
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Maximum Service Temperature, Air | 110 °C | 230 °F | |
|
Abatron 810319 A/B Filled Potting Compound
(discontinued **)
Yellow and colors dielectric casting, adhesive, and resurfacing. 1/1 variable ratio.Information provided by Abatron.
|
|||
| Maximum Service Temperature, Air | 110 °C | 230 °F | Continuous; FRISETTA Test Method |
|
Nilit FRIANYL A63 CV10 Nylon 6.6 for injection molding, 10% carbon fiber reinforced
Nylon 6.6 for injection molding (good conductive and electrostatic properties).Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Maximum Service Temperature, Air | 110 °C | 230 °F | Continuous; FRISETTA Test Method |
|
Nilit FRIANYL B63 GV25 Nylon 6 for injection molding, 25% glass fiber reinforced
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Maximum Service Temperature, Air | 110 °C | 230 °F | |
|
Lehmann & Voss LUVOCOM® 1700-7859 PPO, with carbon fiber, glass fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Improved friction and wear behaviour...
|
|||
| Maximum Service Temperature, Air | 110 °C | 230 °F | |
|
Lehmann & Voss LUVOCOM® 3-7088/GY7012 Polyamide 6, with carbon fiber and glass fiber, low-warpage
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressElectrically conductive, suitable for continuous discharging of staticall..
|
|||
| Maximum Service Temperature, Air | 110 °C | 230 °F | short term |
|
Lehmann & Voss LUVOCOM® TPU-7682 Thermoplastic polyurethane, with carbon fiber
Applications: Electrically conductive, suitable for continuous discharging of statically generated electricity.Improved wear behaviour, low warpage.Bearings, sleeves, sliding elements, chair rollers..
|
|||
| Maximum Service Temperature, Air | 110 °C | 230 °F | |
|
Lehmann & Voss LUVOCOM® 1/GK/30/TF/13/SI/2 Polyamide 66, with glass spheres, PTFE, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage, isotropic shrinka..
|
|||
| Maximum Service Temperature, Air | 110 °C | 230 °F | |
|
LATI Latamid 6 H2 G/30-V2HF PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-2 classified, halogens-based flame retardants and red phosphorous freeAvailability: Africa & Middle East; Asia Pacific; Europe..
|
|||
| Maximum Service Temperature, Air | 110 °C | 230 °F | Continuous Use |
|
Polyram PlusTek PB302G3 Nylon 6, 15% Glass Fiber
15% glass-fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Maximum Service Temperature, Air | 110 °C | 230 °F | Continuous Use |
|
Polyram PlusTek RA846 Nylon 6.6, Impact Modified
Impact modified and heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Maximum Service Temperature, Air | 110 °C | 230 °F | long time operation |
|
Zell-Metall Engineering Plastics Zellamid 1200 G at 50% RH
Zellamid® 1200 G is manufactured by an activated anionic reaction. Finished and semi-finished parts are produced by a static cast process. This process makes it possible to produce a material wit..
|
|||
| Maximum Service Temperature, Air | 110 °C | 230 °F | |
|
Trelleborg B569 Nitrile Rubber
Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi..
|
|||
| Maximum Service Temperature, Air | 110 °C | 230 °F | Continuous Use |
|
Polyram PlusTek PA840G6 Nylon 6.6, 30% Glass Fiber
30% glass fiber reinforced, impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Maximum Service Temperature, Air | 110 °C | 230 °F | Continuous Use |
|
Polyram PlusTek PB310G6 Nylon 6, 33% Glass Fiber
33% glass fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Maximum Service Temperature, Air | 110 °C | 230 °F | Continuous Use |
|
Polyram PlusTek PB321I6 Nylon 6, 30% Glass Fiber and Mineral
30% glass fiber and mineral reinforced polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Maximum Service Temperature, Air | 110 °C | 230 °F | Continuous Use |
|
Polyram PlusTek RA303G4 Nylon 6.6, 20% Glass Fiber
20% glass fiber reinforced, heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Maximum Service Temperature, Air | 110 °C | 230 °F | Continuous Use |
|
Polyram PlusTek RA303G6 Nylon 6.6, 30% Glass Fiber
30% glass fiber reinforced, heat stabilized, and hydrolysis resistant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Maximum Service Temperature, Air | 110 °C | 230 °F | Continuous Use |
|
Polyram RamOfin PPC342M6 Polypropylene, 30% Mineral Filled
30% mineral filled, heat resistant polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Maximum Service Temperature, Air | 110 °C | 230 °F | Continuous Use |
|
Polyram RamOfin PPH300G8 Polypropylene, 40% Glass Fiber
40% glass fiber reinforced polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Maximum Service Temperature, Air | 110 °C | 230 °F | |
|
Chengdu Polyster KLX-G11 PC Film & Sheet
PC film and sheet, high transparency, both sides are polished, both sides with transparent protective films. Is printable, flame-retardant, anti-static, resists ultraviolet decay, scratch resistant,..
|
|||
| Maximum Service Temperature, Air | 110 °C | 230 °F | |
|
Dow Corning MOLYKOTE® LONGTERM 00 GREASE
NLGI 00 mineral oil greaseInformation provided by Dow Corning
|
|||
| Maximum Service Temperature, Air | 110 - 130 °C | 230 - 266 °F | long term; EMS |
|
EMS-Grivory Grivory® BG-40 FC PA6-GF40
Product description: Grilon BG-40 FC is a heat stabilized PA6 injection molding grade with 40% glass fibers. Grilon BG-40 FC has the following important properties: High stiffnessExcellent surface f..
|
|||
| Maximum Service Temperature, Air | 110 - 130 °C | 230 - 266 °F | long term; EMS |
|
EMS-Grivory Grivory® XE 3959 black 9992 PA610
Product description: Grilamid XE 3959 is a high viscosity Polyamide 610 especially suitable for extrusion applications. This PA610 product is to a large extent based on renewable raw materials and i..
|
|||
| Maximum Service Temperature, Air | 110 °C | 230 °F | Deflection temperature; load unknown. |
|
Abatron AboCast/AboCure 8109-9
Minimum toxicity version of 8109-8.Processing: 100/25 ratio; Potlife: 45 min/20°C (68°F), 20 min/40°C (105°F), 10 min /60°C (140°F); mix at RT; cures in: 24 h/20°C (68°F), 2-3 h/60°C (140°..
|
|||
| Maximum Service Temperature, Air | 110 °C | 230 °F | |
|
3M 3350 HVAC Construction
Polypropylene tape for use with flexible ducts. UL 181 B-FX ListedInformation provided by 3M
|
|||
| Maximum Service Temperature, Air | 110 °C | 230 °F | at 50% loss of tensile strength after 20000h; IEC 216-1 |
|
BASF Ultradur® S 4090 G2 10% Glass Filled PBT
Description: Is a PBT + ASA, easy-flowing injection-molding grades with 10% glass fibers; for rigid, tough and dimensionally stable technical parts e. g. housings, consoles, contact carriers, covers..
|
|||
| Maximum Service Temperature, Air | 110 °C | 230 °F | |
|
Lehmann & Voss LUVOCOM® 1-8130 Polyamide 66, with carbon fiber, aramid reinforcement and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved wear behaviour, low warpage.Emergency running property, for highest tribologic needs.R..
|
|||