Thermal Properties Metric English Comments
Maximum Service Temperature, Air 135 °C
275 °F
Precision Polymer Engineering N75L Nitrile Rubber
Nitrile Butadiene Rubber (NBR), 65-75 °IRHD. Ultra-Low acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. To meet ASTM D2000/SAE J200 line call-out: MBF710, B34, F19.Application..
Maximum Service Temperature, Air 135 °C
275 °F
20,000 h; IEC 60216/T1
Raschig Group MELOPLAS® 152 MF
Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al..
Maximum Service Temperature, Air 135 °C
275 °F
20,000 h; IEC 60216/T1
Raschig Group MELOPLAS® 183 MF
Cellulose-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in white and colored shades. Improved dimensional stability and electrical properties as compared with MP 18..
Maximum Service Temperature, Air 135 °C
275 °F
Resin Technology Group 408 Oxy-Bond™ Electrically Conductive Epoxy Adhesive
Oxy-Bond and Millenium Adhesive SystemsEngineered for strength, durability, lightness, and formability, our Oxy-Bond and Millenium lines offer adhesives with physical and electrical properties to ma..
Maximum Service Temperature, Air 135 °C
275 °F
Lehmann & Voss LUVOCOM® 1t-7370 Polyamide 6/6T, with carbon fiber, toughness-modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
Maximum Service Temperature, Air 135 °C
275 °F
Lehmann & Voss LUVOCOM® 21-7979 Polyamide 6/6T, with glass fiber, 8-mm-granulate
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.High dimensionally stable prec..
Maximum Service Temperature, Air 135 °C
275 °F
Lehmann & Voss LUVOCOM® 21-8115 Polyamide 6/6T, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear..
Maximum Service Temperature, Air 135 °C
275 °F
Greene Tweed WRâ„¢ FP100 Polyketone, Reinforced
Greene Tweed’s WR® FP100, a reinforced compression-molded polyketone, offers excellent wear resistance with FDA compliance. The typical properties and physical characteristics of WR FP100 m..
Maximum Service Temperature, Air 135 °C
275 °F
LATI Latamid 66 H2 G/60 PA 66, 60% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl..
Maximum Service Temperature, Air 135 °C
275 °F
LATI Later 4 G/30-V0HF1 PBT, 30% Glass Fiber Reinforced, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Europe..
Maximum Service Temperature, Air 135 °C
275 °F
LATI Latigloss 66 H2 G/60 PA 66, 60% Glass Fiber Reinforced, Heat Stabilized
Product with high mechanical properties and exceptional surface finish based on Polyamide 66 (PA66). Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am..
Maximum Service Temperature, Air 135 °C
275 °F
Saint-Gobain Norprene® A-60-G Industrial Grade Tubing Formulation
Description: Norprene® Industrial Grade Tubing, Formulation A-60-G: Norprene® Industrial Grade Tubing outperforms neoprene, EPDM and other general-purpose tubings in test after test and appl..
Maximum Service Temperature, Air 135 °C
275 °F
Master Bond EP21TDCN Two Component Nickel Conductive Epoxy Adhesive
Product Description: Master Bond Polymer System EP21TDCN is a two component, nickel filled, electrically conductive, adhesive for high performance bonding, formulated to cure at room temperature or ..
Maximum Service Temperature, Air 135 °C
275 °F
Master Bond EP76M-1R Nickel Conductive Epoxy Adhesive
Description: Master Bond Polymer System EP76M-1R is a two component, nickel filled, electrically conductive adhesive for high performance bonding formulated to cure at room temperature or more rapid..
Maximum Service Temperature, Air 135 °C
275 °F
Tra-Con Tra-Bond 2123 Metal Repair Steel/Epoxy Adhesive
TRA-BOND 2123 is a versatile steel metal/epoxy adhesive formulation developed for modern industrial repair, casting and bonding applications where a steel-like or cast iron finish is required. This ..
Maximum Service Temperature, Air 135 °C
275 °F
Loctite® 3751 Acrylic Light Cure Adhesive
Acrylic Light Cure AdhesivesVersatile Loctite® ultraviolet (UV) and visible light curing adhesives can be used in bonding, encapsulating, coating, tacking, and sealing applications. These single co..
Maximum Service Temperature, Air 135 °C
275 °F
See Note 2.
ChevronTexaco Marfak® Heavy Duty 2
Texaco Marfak grease delivers value through:Good film strengthGood rust and corrosion protection, even in wet conditions.Texaco Marfak greases are fibrous sodium soap greases. It resists oil separat..
Maximum Service Temperature, Air 135 °C
275 °F
few hours; VDE 0304/P2-1, IEC 216
EPICHEM Epilon FR-PC V0 Polycarbonate
Characteristics: self-extinguishing V0 at 1,6 mm
Maximum Service Temperature, Air 135 °C
275 °F
at 50% loss of tensile strength after 20000h; IEC 216-1
BASF Ultradur B 4300 G4 20% Glass Filled PBT
Ultradur B4300 G4 is an easy flowing injection molding PBT with 20% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small..
Maximum Service Temperature, Air 135 °C
275 °F
for 50% loss of tensile strength after 20000hr
BASF Ultramid® B3EG7 35% Glass Filled PA6 (Dry)
Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF
Maximum Service Temperature, Air 135 °C
275 °F
for 50% loss of tensile strength after 20000hr
BASF Ultramid® B3EG7 BK 00564 35% Glass Filled PA6 (Conditioned)
Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF
Maximum Service Temperature, Air 135 °C
275 °F
for 50% loss of tensile strength after 20000hr
BASF Ultramid® KR 4355 G5 25% Glass Filled PA6/6T (Conditioned)
Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r..
Maximum Service Temperature, Air 135 °C
275 °F
for 50% loss of tensile strength after 20000hr
BASF Ultramid® B3EG5 25% Glass Filled PA6 (Conditioned)
Description: 25% glass-fiber reinforced injection-molding grade for industrial articles and electrical insulating partsInformation provided by BASF
Maximum Service Temperature, Air 135 - 190 °C
275 - 374 °F
Average value: 150 °C Grade Count:22
Overview of materials for Melamine-Phenolic Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Melamine-Phenolic Copolymer". Each property range of values reported is minimum and maximum values of ap..
Maximum Service Temperature, Air 135 °C
275 °F
ExxonMobil Santoprene® 111-87 Thermoplastic Elastomer  (discontinued **)
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Maximum Service Temperature, Air 135 °C
275 °F
ExxonMobil Santoprene® 211-87 Thermoplastic Elastomer  (discontinued **)
A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Maximum Service Temperature, Air 135 °C
275 °F
ExxonMobil Santoprene® 221-80 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide..
Maximum Service Temperature, Air 135 °C
275 °F
Resinlab® CYNERGY CA6904 Adhesive
Description: The CYNERGY 6900 SERIES are for use in demanding applications where very fast cure speeds and high temperature resistance are required. These are single component solvent free materials..
Copyright © lookpolymers.com All Rights Reserved