Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Maximum Service Temperature, Air = 140 °C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 140 °C
284 °F
20,000 hr; IEC 216
Nilit Nilitop BT G6 FR C3 is a 30% Glass Fiber Reinforced, Flame Retardant PBT
Description: Nilitop BT G6 FR C3 is a 30% glass fiber reinforced, flame retardant PBT with halogens. The flame retardant does not contain PBB and PBDE, so it is compliant with the WEEE directive. It..
Maximum Service Temperature, Air 140 °C
284 °F
Continuous; FRISETTA Test Method
Nilit FRIANYL A63 TF-GV 1530 Nylon 6.6 for injection molding, 15% PTFE lubricated and 30% glass fiber reinforced
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Maximum Service Temperature, Air 140 °C
284 °F
20,000 h; IEC 216/T1
Raschig Group AMPLA® 2000 melamine-modified polyester
Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Low post-shrinkage, very good electrical values, high heat resistance, very good sliding behavior, ve..
Maximum Service Temperature, Air 140 °C
284 °F
Continuous; FRISETTA Test Method
Nilit FRIANYL A63 TF-KV 1530 Nylon 6.6 for injection molding, 15% PTFE lubricated and 30% glass ball reinforced
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Maximum Service Temperature, Air 140 °C
284 °F
<20000 hours; IEC 60216-P1
Hexion Bakelite™ PF 31.9 Phenolic Formaldehyde Resin, Ammonia Free  (discontinued **)
Phenolic molding compound, mainly organically filled, ammonia free, standardized molding compound.Application areas: Parts for electrical and telecommunications technology, motor vehicle ignition sy..
Maximum Service Temperature, Air 140 °C
284 °F
short term
Lehmann & Voss LUVOCOM® 1-8521 Polyamide 66, with carbon fiber and glass fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Maximum Service Temperature, Air 140 °C
284 °F
short term
Lehmann & Voss LUVOCOM® 6-8159 Polyamide 12, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Especially suitable at dynamic stress situations.Electrically conductive, s..
Maximum Service Temperature, Air 140 °C
284 °F
short term
Lehmann & Voss LUVOCOM® 6-8436 Polyamide 12, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Dynamic stressed parts.Low waterabsorbtion.Isotropic shrinkage characteristics.Bearings, sleeve..
Maximum Service Temperature, Air 140 °C
284 °F
Industrial Laminates/Norplex NP509 Glass Fabric
Description: Woven glass fabric, melamine resin laminate. Very hard, flame resistant, machining grade with excellent electrical properties in high humidity conditions. High physical strength and exc..
Maximum Service Temperature, Air 140 °C
284 °F
Menzolit Menzolit® BMC 0900 Unsaturated Polyester UP
BMC 0900 is a special BMC used in a chemically aggressive environment. The glass content is set to a level that combines good mould ability with good strength and stiffness properties. Typical appli..
Maximum Service Temperature, Air 140 °C
284 °F
Menzolit Menzolit® SMC 0900 Unsaturated Polyester UP
SMC 0900 is a special SMC for use within a chemical aggressive environment. The glass level is selected to combine good mouldability with good strength and stiffness properties. The product is espec..
Maximum Service Temperature, Air 140 °C
284 °F
Continuous; SAE J 2236
Zylog Neoplast® 243 HOFR Thermoplastic Vulcanizate
Neoplast 243 HOFR is a flame retardant thermoplastic vulcanizate (TPV) compound, based on polyolefin chemistry, suitable for Injection Molding and Extrusion applications.RoHS Compliant, UV Stabilize..
Maximum Service Temperature, Air 140 °C
284 °F
Continuous; SAE J 2236
Zylog Neoplast® 250 FT EB Thermoplastic Vulcanizate
Neoplast 250 FT EB is a hard, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding, Blow Molding and Extrusion applications.Ro..
Maximum Service Temperature, Air 140 °C
284 °F
Trelleborg E646 EPDM Rubber
EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and ..
Maximum Service Temperature, Air 140 °C
284 °F
Short peaks operation
Polyram RamOfin PPH300G3 Polypropylene, 15% Glass Fiber
15% Glass fiber reinforced polypropylene for injection molding application.Information provided by Polyram.
Maximum Service Temperature, Air 140 °C
284 °F
Short peaks operation
Polyram RamOfin PPH300G9 Polypropylene, 45% Glass Fiber
45% glass fiber reinforced polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind.
Maximum Service Temperature, Air 140 °C
284 °F
Short peaks operation
Polyram RamOfin PPH301G6NT Polypropylene, 30% Glass Fiber
30% Glass fiber reinforced polypropylene for injection molding applications. Approved and listed by WRAS Potable Water.Information provided by Polyram.
Maximum Service Temperature, Air 140 °C
284 °F
Short peaks operation
Polyram RamOfin PPH353M8 Polypropylene, 40% Mineral Filled
40% mineral filled polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind.
Maximum Service Temperature, Air 140 °C
284 °F
Trelleborg Emerson & Cuming Eccobond® G757 One-Component High Strength-Impact Resistant Epoxy Adhesive
Emerson & Cuming G757 Eccobond® One-Component High Strength-Impact Resistant Epoxy AdhesiveVery flexible, thixotropic, epoxy adhesive. Excellent low temperature resistance. Excellent adhesion to gl..
Maximum Service Temperature, Air 140 °C
284 °F
short term; EMS
EMS-Grivory Grivory® BZ 3 PA6
Information provided by EMS Grivory
Maximum Service Temperature, Air 140 °C
284 °F
long term; EMS
EMS-Grivory Grivory® HT1V-5 FWA nat PA6T/6I-GF50
Product description: Grivory HT1V-5 FWA natural is a 50 wt.-% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6..
Maximum Service Temperature, Air 140 °C
284 °F
at 50% loss of tensile strength after 5000h; IEC 216-1
BASF Ultradur® S 4090 G2 10% Glass Filled PBT
Description: Is a PBT + ASA, easy-flowing injection-molding grades with 10% glass fibers; for rigid, tough and dimensionally stable technical parts e. g. housings, consoles, contact carriers, covers..
Maximum Service Temperature, Air 140 °C
284 °F
ATG s.r.l. EPM Ethylene-Propylene Copolymer
Maximum Service Temperature, Air 140 °C
284 °F
Alliance BCN-14 Bonded (Composite) Magnetic Material
Maximum Service Temperature, Air 140 °C
284 °F
at 50% loss of tensile strength after 5000h; IEC 216-1
BASF Ultradur S 4090 G4 20% Glass Filled PBT
Ultradur S 4090 G4 is a 20% glass reinforced PBT+ASA blend. It produces moldings with good surface finish,is resistant to chemicals and stress cracking, and has low shrinkage and warpage.Applicatio..
Maximum Service Temperature, Air 140 °C
284 °F
RTI
Covestro Petlon® 3530 Semi-Crystalline PET, 30% Glass Fiber  (discontinued **)
Characteristics: Excellent Electrical Properties, High Heat and Chemical ResistanceApplications: Automotive (Underhood), Appliances, Casings and HousingsProcessing: Injection Molding (Melt Temperatu..
Copyright © lookpolymers.com All Rights Reserved