Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 °C
300 °F
ND Industries 530 Shaft & Bearing Retainer Retaining Compound
General DescriptionA high strength adhesive for retention of cylindrical components, where disassembly is not required.Typical Usesrotors, shafts, bushings, bearings, and pulleysMeets military spec ..
Maximum Service Temperature, Air 149 °C
300 °F
Quadrant EPP Quadrant PPSU LSG PPSU, Extruded, Unfilled, Polyphenylsulfone (ASTM Product Data Sheet)
Maximum Service Temperature, Air 149 °C
300 °F
Permabond HH167 Anaerobic Retainer
Permabond® HH167 is a high viscosity gap filling silver paste, which can be used for repairing metal machinery parts. It is ideal for repairing worn shafts, broken threads, damaged keyways and spli..
Maximum Service Temperature, Air 149 °C
300 °F
Permabond HL126 Anaerobic Threadlocker
PERMABOND® HL126 Threadlocker is a water thin product for locking pre-assembled parts through wicking action. PERMABOND® HL126 Threadlocker prevents vibration loosening. Because of the low viscosi..
Maximum Service Temperature, Air 149 °C
300 °F
continuous
Lucas-Milhaupt Silvaloy® 6 Brazing Alloy
Silvaloy 6 is used for the brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten and molybdenum. It should not be used on ferrous and nickel metals or copper..
Maximum Service Temperature, Air 149 - 171 °C
300 - 340 °F
UL-746 B
Saint-Gobain Norton® ECTFE Fluoropolymer Film
Features/Benefits:Outstanding release propertiesPerformance from -200°C (-328°F) to 165°C (330°F)High dielectric strengthExcellent chemical, radiation, weather and abrasion resistanceNon..
Maximum Service Temperature, Air 149 °C
300 °F
Hexcel® HexWeb® HRH-10/F50 - 5.0 Nonmetallic Flex-Core Honeycomb
Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo..
Maximum Service Temperature, Air 149 °C
300 °F
Loctite® 3103 Acrylic Light Cure Adhesive
Acrylic Light Cure AdhesivesVersatile Loctite® ultraviolet (UV) and visible light curing adhesives can be used in bonding, encapsulating, coating, tacking, and sealing applications. These single co..
Maximum Service Temperature, Air 149 °C
300 °F
Loctite® 3211 Light Cure Acrylic Adhesive
Medical Grade BondersLoctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant products are designe..
Maximum Service Temperature, Air 149 °C
300 °F
Loctite® 334 Acrylic Bonding Adhesive
Acrylic Bonding AdhesivesLoctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impact, stress and shock resistance. ..
Maximum Service Temperature, Air 149 °C
300 °F
Loctite® 5205 Flexible Cure Flange Sealant
Anaerobic GasketingLoctite® 5205 Flexible Cure Flange SealantFast curing and flexible, good sealing properties against oil and water/glycol particularly at high temperatures. High viscosity. Recom..
Maximum Service Temperature, Air 149 °C
300 °F
Loctite® 638 Maximum Strength Retaining Compound
RetainersLoctite Corporation, the pioneer of anaerobic adhesives, has applied this technology to create retaining compounds that increase the shear strength of cylindrical, non-threaded assemblies. ..
Maximum Service Temperature, Air 149 °C
300 °F
Loctite® Gasket Eliminator® 518 Flange Sealant
Anaerobic GasketingLoctite® 518 Flexible Cure Gasket Eliminator® Flange SealantForms a flexible, solvent-resistance seal that will not tear or decay. Seals to 300ºF and fills gaps to 0.050". Can..
Maximum Service Temperature, Air 149 °C
300 °F
CPC - Vycom FLAMETEC™ HALAR® 901 Opaque Ethylene Chlorotrifluoroethylene (ECTFE)
Flametec™ Halar® ECTFE (Ethylene Chlorotrifluoroethylene) is an ultra-pure fluoropolymer that is a tough engineering thermoplastic with a balance of physical and chemical properties that qualify i..
Maximum Service Temperature, Air 149 °C
300 °F
ChevronTexaco Thread Sealing Compound
FeaturesChevron Thread Sealing Compound is a time-tested aluminum complex grease designed especially for casing and tubing connections in high-pressure oil well service, or wherever unusually severe..
Maximum Service Temperature, Air 149 °C
300 °F
DuPont Teijin Films Mylar® A Polyester Film, 1200 Gauge
Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, ..
Maximum Service Temperature, Air 149 °C
300 °F
DuPont Teijin Films Mylar® A Polyester Film, 200 Gauge
Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, ..
Maximum Service Temperature, Air 149 °C
300 °F
DuPont Teijin Films Mylar® MDA Polyester Film, 1200 Gauge
Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion..
Maximum Service Temperature, Air 149 °C
300 °F
DuPont Teijin Films Mylar® A Polyester Film, 92 Gauge
Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, ..
Maximum Service Temperature, Air 149 °C
300 °F
3M 33315 Copper Foil Tape
"Tinned," corrosion resistant.Information provided by 3M
Maximum Service Temperature, Air 149 °C
300 °F
3M 439 Premium Performance Aluminum Foil Tape
Linered version of 431Information provided by 3M
Maximum Service Temperature, Air 149 °C
300 °F
3M Scotch® 2525 Performance Flatback Tape
Scotch® Performance Flatback Tape 2525 is used in holding, splicing or masking applications where high adhesion strength, high temperature capability and high backing strength are required.Informat..
Maximum Service Temperature, Air 149 °C
300 °F
3M Scotch-Weld™ HP69 Pipe Sealant Anaerobic Adhesives
3M™ Scotch-Weld™ Pipe Sealant Anaerobic Adhesives are one-component anaerobic sealants that cure and seal hydraulic and pneumatic pipes and fittings to withstand high temperatures and pressures. H..
Maximum Service Temperature, Air 149 °C
300 °F
Service
3M 7903 Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti..
Maximum Service Temperature, Air 149 °C
300 °F
Short term
3M 93015LE High Strength Double Coated Tape with Adhesive 300LSE
3M ™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryl..
Maximum Service Temperature, Air 149 °C
300 °F
for up to 30 mins
3M Scotch® 4737T High Temperature Fine Line Tape
Scotch® High Temperature Fine Line Tape 4737 is a vinyl paint masking tape for fascia, rocker panels, two-tone and other multiple color applications where critical paint break lines are required.In..
Maximum Service Temperature, Air 149 °C
300 °F
Loctite® 568 Thread Sealant
Thread SealersLoctite® Liquid Thread Sealants seal and secure metal pipes and fittings, filling the space between threaded metal parts, and hardening to prevent leakage. Designed for low and high p..
Maximum Service Temperature, Air 149 °C
300 °F
Loctite® 572 Low Strength Thread Sealant
Thread SealersLoctite® Liquid Thread Sealants seal and secure metal pipes and fittings, filling the space between threaded metal parts, and hardening to prevent leakage. Designed for low and high p..
Maximum Service Temperature, Air 149 °C
300 °F
Loctite® 661 Retaining Compound
RetainersLoctite Corporation, the pioneer of anaerobic adhesives, has applied this technology to create retaining compounds that increase the shear strength of cylindrical, non-threaded assemblies. ..
Maximum Service Temperature, Air 149 °C
300 °F
Henkel Hysol EA 9686 Film Adhesive
Second generation, moisture resistant, toughened 250°F / 121°C curing film with service performance to 300°F / 149°C. Excellent for composite or metal bonding. Data from .060 psf, 300 g / m2.App..
Copyright © lookpolymers.com All Rights Reserved