| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 150 °C | 302 °F | Recommended |
|
Nye Lubricants 229 (SO) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Maximum Service Temperature, Air | 150 °C | 302 °F | Recommended |
|
Nye Lubricants 5100 (SVLG) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Maximum Service Temperature, Air | 150 °C | 302 °F | |
|
Precision Polymer Engineering E60D Ethylene Propylene Rubber
Sulphur cured, Ethylene Propylene Terpolymer, 56-65 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Formulated in accordance with BS2494 Type ‘W’. Water Research Council (WRC) teste..
|
|||
| Maximum Service Temperature, Air | 150 °C | 302 °F | |
|
Resinlab® EP965 Clear Unfilled Electronic Grade Epoxy Encapsulant
Resinlab™ EP965 Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting ..
|
|||
| Maximum Service Temperature, Air | 150 °C | 302 °F | short term |
|
Lehmann & Voss LUVOCOM® 1850-7692/BK PBT, with glass spheres and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
|
|||
| Maximum Service Temperature, Air | 150 °C | 302 °F | |
|
Lehmann & Voss LUVOCOM® 19-8250 Polyamide 46, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Reduced moment of inertia compared with metal parts.Highly dimensionally stable at elevated tem..
|
|||
| Maximum Service Temperature, Air | 150 °C | 302 °F | |
|
Lehmann & Voss LUVOCOM® 19-8365 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
|
|||
| Maximum Service Temperature, Air | 150 °C | 302 °F | |
|
Lehmann & Voss LUVOCOM® 46/CF/15 Polyamide 46, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
|
|||
| Maximum Service Temperature, Air | 150 °C | 302 °F | short term |
|
Lehmann & Voss LUVOCOM® 50/TF/15/BK-1 Polycarbonate, with PTFE, easy flowing
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper..
|
|||
| Maximum Service Temperature, Air | 150 °C | 302 °F | short term |
|
Lehmann & Voss LUVOCOM® 50-8479/BL-1 Polycarbonate, unreinforced
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Isotropic shrinkage characteristics.Reduced moment of inertia ..
|
|||
| Maximum Service Temperature, Air | 150 °C | 302 °F | |
|
LATI Laramid G/50 PPA, 50% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
|
|||
| Maximum Service Temperature, Air | 150 °C | 302 °F | short term |
|
Lehmann & Voss LUVOCOM® 1/GF/40/TF/13 Polyamide 66, with glass fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
|
|||
| Maximum Service Temperature, Air | 150 °C | 302 °F | |
|
GrafTech C1 Acrylic Coating
Optional coating for eGRAF® SPREADERSHIELD™ graphite products. Structure: 0.00254mm Acrylic - Graphite
|
|||
| Maximum Service Temperature, Air | 150 °C | 302 °F | |
|
Silikony Polskie Gumosil M Silicone Rubber
Flexible with good tearing resistance
|
|||
| Maximum Service Temperature, Air |
150
°C @Thickness 3.00 mm |
302
°F @Thickness 0.118 in |
UL Temp Index |
|
Sumitomo Bakelite Durez® 23570 Phenolic, Compression Grade
Durez 23570 Black Phenolic is a glass and mineral filled two-stage, special purpose molding material. It is designed for high strength, good dimensional stability, and electrical properties even aft..
|
|||
| Maximum Service Temperature, Air | 150 °C | 302 °F | Intermittent |
|
Tra-Con Tra-Bond 2106T Fast Cure Thixotropic Epoxy Adhesive
TRA-BOND 2106T is an exceptional epoxy formulation recommended for lower temperature or wet industrial bonding applications where FAST CURING is required. This versatile two-part epoxy system contai..
|
|||
| Maximum Service Temperature, Air | 150 °C | 302 °F | short term; EMS |
|
EMS-Grivory Grivory® 1SBVX-30H LDS black PA1010-GF30
Product Description: Grilamid 1SBVX-30H LDS black is a 30% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is specifically optimized for the laser Direct Structuring techno..
|
|||
| Maximum Service Temperature, Air | 150 °C | 302 °F | short term; EMS |
|
EMS-Grivory Grivory® BRZ 347 W PA6
Product description: Grilon BRZ 347 W is a heat stabilized, high viscosity, impact modified and plasticized PA6 extrusion grade. Grilon BRZ 347 W has the following important properties: High flexibi..
|
|||
| Maximum Service Temperature, Air | 150 °C | 302 °F | short term; EMS |
|
EMS-Grivory Grivory® L 20H FWA black 9225 PA12
Product Description Grilamid L 20 H FWA black 9225 is a medium viscosity, unreinforced and heat stabilized Polyamide 12 (PA12). Grilamid L 20 H FWA black 9225 is used for technical injection molded ..
|
|||
| Maximum Service Temperature, Air | 150 °C | 302 °F | short term; EMS |
|
EMS-Grivory Grivory® LBV-30H FWA black 9225 PA12-GF30
Product Description: Grilamid LBV-30H FWA black 9225 is a 30% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: Stiffness combined wit..
|
|||
| Maximum Service Temperature, Air | 150 °C | 302 °F | Continuous |
|
Epoxy Technology EPO-TEK® E4110-PFC Electrically Conductive Epoxy
Product Description: EPO-TEK®E4110-PFC is a two-component, silver filled, electrically conductive adhesive designed for semiconductor IC packaging and general electronic assembly. It is a thixotr..
|
|||
| Maximum Service Temperature, Air | 150 °C | 302 °F | Service |
|
3M FM06P Indoor UL Recognized Brite Silver Polyester Label Products
3M™ Indoor UL Recognized Brite Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize..
|
|||
| Maximum Service Temperature, Air | 150 °C | 302 °F | Service |
|
3M FM283 Indoor UL Recognized White Polyester Label Products
3M™ Indoor UL Recognized White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ A..
|
|||
| Maximum Service Temperature, Air | 150 °C | 302 °F | at 50% loss of tensile strength after 5000h; IEC 216-1 |
|
BASF Ultradur B 4300 G4 20% Glass Filled PBT
Ultradur B4300 G4 is an easy flowing injection molding PBT with 20% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small..
|
|||
| Maximum Service Temperature, Air | 150 °C | 302 °F | Service |
|
3M FM057 Indoor UL Recognized Brite Silver Polyester Label Products
3M™ Indoor UL Recognized Brite Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize..
|
|||
| Maximum Service Temperature, Air | 150 °C | 302 °F | Continuous use |
|
Hippe PVDF
Better mechanical strength compared to other fluorinated polymers. Tough and hard. High-grade electrical feature. Good weathering stability. Physiologically safe. Not as good as fluorinated pol..
|
|||
| Maximum Service Temperature, Air | 150 °C | 302 °F | |
|
Resinlab® EP1200 Black Casting Resin
Resinlab™ EP1200 Black is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity, flexibility and a low CTE. It meets the re..
|
|||
| Maximum Service Temperature, Air | 150 °C | 302 °F | UL Temperature Index; UL 746B |
|
Sumitomo Bakelite North America FM 4005 Fiberglass Reinforced Phenolic Novolac
FM 4005 is a fiberglass reinforced phenolic novolac molding compound, with excellent dimensional stability and good strength at elevated temperatures. This material is compliant with the specificat..
|
|||
| Maximum Service Temperature, Air | 150 °C | 302 °F | short term |
|
Lehmann & Voss PLASLUBE J-50/10/TF/15/BK Polycarbonate, with glass fiber and PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts, even at elevated te..
|
|||