| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air |
80.0
°C <br>@Time 1.80e+7 sec
|
176
°F <br>@Time 5000 hour
|
|
|
Murtfeldt Original Material ”S”® plus + Bright ESD Polyethylene, Conductive
Material ”S”® plus+ Bright ESD is a light plastic with high conductivity and a voltage-dissipating effect on earthed components. This material is ideal for use in applications where a high value..
|
|||
| Maximum Service Temperature, Air | 80.0 °C | 176 °F | |
|
Okulen® 500 PE-HMW, AST
OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel..
|
|||
| Maximum Service Temperature, Air | 80.0 °C | 176 °F | continuous |
|
Orbilan RubberLen® R55 HMW-PE, dark blue
ORBILAN RUBBERLEN® is a two-layered laminated panel made from Thermoplastic Elastomer (TPE) and low-pressure Polyethylene of High Molecular Weight (HMW-PE). RUBBERLEN® distinguishes itself by very..
|
|||
| Maximum Service Temperature, Air | 80.0 °C | 176 °F | continuous |
|
P & P Technology Chloroprene Neoprene Sponge
Good resistance to heat and moderate chemicals and moderate resistance to oils. Has good characteristics to resist sea water, acids, fats, greases and many solvents. Neoprene has good ozone resistan..
|
|||
| Maximum Service Temperature, Air | 80.0 °C | 176 °F | Continuous; FRISETTA Test Method |
|
Nilit FRIANYL B63 S20 Nylon 6 for injection molding
Nylon 6 for injection molding, impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Maximum Service Temperature, Air | 80.0 °C | 176 °F | Continuous |
|
Quadrant EPP Borotron® UH PE-UHMW + boron based additive (ISO Data)
Borotron UH and Borotron HM are boron loaded PE-(U)HMW grades, specifically developed for neutron shielding purposes in nuclear installations. The high hydrogen content of PE-(U)HMW makes it very su..
|
|||
| Maximum Service Temperature, Air | 80.0 °C | 176 °F | Glass |
|
Parker Chomerics Tecknit Teckshield®-F 100 OPI 0.0022" Diameter Wire, High Performance EMC Window
Description: TECKSHIELD-F high-performance fully laminated flat windows are specially designed to provide optimum optical transmission and EMI shielding in severe interference environments. TECKSHIE..
|
|||
| Maximum Service Temperature, Air | 80.0 °C | 176 °F | Glass |
|
Parker Chomerics Tecknit Teckshield®-F 145 OPI 0.0022" Diameter Wire, High Performance EMC Window
Description: TECKSHIELD-F high-performance fully laminated flat windows are specially designed to provide optimum optical transmission and EMI shielding in severe interference environments. TECKSHIE..
|
|||
| Maximum Service Temperature, Air | 80.0 - 150 °C | 176 - 302 °F | Average value: 131 °C Grade Count:8 |
|
Overview of materials for Polycarbonate, 10% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea..
|
|||
| Maximum Service Temperature, Air | 80.0 °C | 176 °F | short term |
|
Lehmann & Voss LUVOCOM® 1200-8493 ABS, with steel fiber
Applications: Office communication.Electrically conductive, suitable for continuous discharging of statically generated electricity.Isotropic shrinkage characteristics.Information provided by Lehman..
|
|||
| Maximum Service Temperature, Air | 80.0 °C | 176 °F | Continuous |
|
Schwartz Technical Plastics LAMIGAMID® 710 High Density Polyethylene
Application: chain-guides, cutting plates, linersInformation provided by Schwartz Technical Plastics GmbH
|
|||
| Maximum Service Temperature, Air | 80.0 °C | 176 °F | Continuous Use; ASTM D794 |
|
Teknor Apex APEX® 155 Polyvinyl Chloride, Flexible
Notes: 80°C Jacket; RoHS CompliantFeatures: Sunlight Resistant (720 hours); Good UV Resistance Uses: Building Wire Jacketing; Wire and Cable Applications Agency Ratings: UL QMTT2 .E73402Forms: Pe..
|
|||
| Maximum Service Temperature, Air | 80.0 °C | 176 °F | |
|
Styrolution Terluran® EGP-7 ABS
Terluran EGP-7 is an extrusion grade with well balanced properties.UL 94 HBInformation provided by Styrolution
|
|||
| Maximum Service Temperature, Air | 80.0 °C | 176 °F | Continuous Use; ASTM D794 |
|
Teknor Apex APEX® 82-E211-B Polyvinyl Chloride, Flexible
Notes: 80°C Insulation; RoHS Compliant Uses: Transportation Wire Insulation Agency Ratings: SAE J1128 Automotive Specifications: Chrysler MS-DC16 Type A Processing Method: Extrusion Forms: Pell..
|
|||
| Maximum Service Temperature, Air | 80.0 °C | 176 °F | Continuous Use; ASTM D794 |
|
Teknor Apex APEX® 01-A0303E-95 Polyvinyl Chloride, Flexible
Notes: 105°C Insulation; RoHS Compliant Uses: Automotive Electronics; Insulation; Wire and Cable Applications Wire Types: GPT Agency Ratings: SAE J1128 Forms: PelletsInformation Provided by Tekno..
|
|||
| Maximum Service Temperature, Air | 80.0 °C | 176 °F | Continuous use |
|
Polyram PlusTek PA108 Nylon6/6.6 Alloy for Injection Molding
Good surface finish Nylon 6/6.6 alloy for injection molding.Information provided by Polyram.
|
|||
| Maximum Service Temperature, Air | 80.0 °C | 176 °F | Continuous Use |
|
Polyram PlusTek RA845 Nylon 6.6, Impact Modified
Improved impact polyamide 6.6 for good resistance to low temp for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Maximum Service Temperature, Air | 80.0 °C | 176 °F | |
|
Trelleborg R642 Commercial Natural Rubber Polyisoprene
All information provided by Trelleborg
|
|||
| Maximum Service Temperature, Air | 80.0 - 110 °C | 176 - 230 °F | long term; EMS |
|
EMS-Grivory Grivory® BG-15 HM PA6-GF15
Product description: Grilon BG-15 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 15% glass fibers. Grilon BG-15 HM has the following important prop..
|
|||
| Maximum Service Temperature, Air | 80.0 - 100 °C | 176 - 212 °F | long term; EMS |
|
EMS-Grivory Grivory® BT 40 Z PA6
Product description: Grilon BT 40 Z is an unreinforced, normal viscosity, impact modified polyamide blend with amorphous and semi-crystalline components. Grilon BT 40 Z has the following important p..
|
|||
| Maximum Service Temperature, Air | 80.0 - 110 °C | 176 - 230 °F | long term; EMS |
|
EMS-Grivory Grivory® BG-50 HM PA6-GF50
Product description: Grilon BG-50 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 50% glass fibers. Grilon BG-50 HM has the following important prop..
|
|||
| Maximum Service Temperature, Air | 80.0 °C | 176 °F | |
|
3M 1400 Economy Vinyl Electrical Tape
3M™ Economy Vinyl Electrical Tape 1400 is a black 7 mil thick, general use vinyl-insulating tape. It is designed to perform continuously in temperatures up to 80°C. This tape has a polyvinyl chlor..
|
|||
| Maximum Service Temperature, Air | 80.0 °C | 176 °F | |
|
BCC Products BC 100 Thin Cyanoacrylate Adhesive
BC100 Thin is a low viscosity material ideal for bonding larger areas. BC100 Thin has a 20 second fixture cure and able to fill gaps of .002” wide. BC100 Thin is perfectly designed for bonding plas..
|
|||
| Maximum Service Temperature, Air | 80.0 °C | 176 °F | Short Periods |
|
Hippe PS Polystyrene
Amorphous thermoplastic with brilliant surface. High hardness and stiffness, but brittle and susceptible to impact. Very good dielectric properties. Physiologically safe if it falls below a parti..
|
|||