Polymer Property : Maximum Service Temperature, Air = 180 °C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 - 180 °C
300 - 356 °F
Average value: 161 °C Grade Count:6
Overview of materials for Fluorocarbon ETFE/ECTFE, Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE/ECTFE, Molded/Extruded". Each property range of values reported is minimum and maximum..
Maximum Service Temperature, Air 65.0 - 180 °C
149 - 356 °F
Average value: 129 °C Grade Count:18
Overview of materials for Nylon 6, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ..
Maximum Service Temperature, Air 80.0 - 180 °C
176 - 356 °F
Average value: 126 °C Grade Count:4
Overview of materials for Nylon 66, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..
Maximum Service Temperature, Air 90.0 - 180 °C
194 - 356 °F
Average value: 139 °C Grade Count:8
Overview of materials for Nylon 612, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of ..
Maximum Service Temperature, Air 177 - 180 °C
351 - 356 °F
Softening Range
Huntsman DT 3357 Matting Agent
Color: WhiteComments/Applications: Non-yellowing reactive matting agent for very low gloss epoxy and epoxy/polyester hybrid powder systems. No effect on mechanical properties.Data provided by Ciba ..
Maximum Service Temperature, Air 170 - 180 °C
338 - 356 °F
UL 746B
Sumitomo Bakelite North America RX® 1366FR-P Short-Glass Reinforced Diallyl Phthalate
Short glass fiber reinforced, flame retardant, diallyl ortho-phthalate molding compound which meets the requirements of ASTM D5948 Type SDG-F.Information provided by Vyncolit, a Sumitomo Bak Group
Maximum Service Temperature, Air 150 - 180 °C
302 - 356 °F
Continuous
Asahi Glass F-Clean® Film for Greenhouses
F-CLEAN®, produced by Asahi Glass Company, Ltd., is a Ethylene-Tetrafluoroethylene copolymer (ETFE) film used as the preferred covering material for horticultural greenhouses. High ten..
Maximum Service Temperature, Air 150 - 180 °C
302 - 356 °F
Continuous
Asahi Glass Fluon® ETFE Film
Applications: Electronics, Energy Saving, Wallpaper, Sound Suppression Walls, Aviation and SpaceInformation provided by Asahi Glass Company, Inc.
Maximum Service Temperature, Air 90.0 - 180 °C
194 - 356 °F
Average value: 117 °C Grade Count:6
Overview of materials for Nylon 6, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v..
Maximum Service Temperature, Air 65.0 - 180 °C
149 - 356 °F
Average value: 98.9 °C Grade Count:10
Overview of materials for Acrylic, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Maximum Service Temperature, Air 130 - 180 °C
266 - 356 °F
Average value: 155 °C Grade Count:7
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is ..
Maximum Service Temperature, Air 60.0 - 180 °C
140 - 356 °F
Average value: 131 °C Grade Count:61
Overview of materials for Nylon 6, Cast
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW..
Maximum Service Temperature, Air 160 - 180 °C
320 - 356 °F
Average value: 166 °C Grade Count:4
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc..
Maximum Service Temperature, Air 65.0 - 180 °C
149 - 356 °F
Average value: 115 °C Grade Count:5
Overview of materials for Polypropylene with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i..
Maximum Service Temperature, Air 120 - 180 °C
248 - 356 °F
Average value: 150 °C Grade Count:15
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu..
Copyright © lookpolymers.com All Rights Reserved