| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 85.0 °C | 185 °F | 20,000 hr; IEC 216 |
|
Nilit Nilamon A3 H K8 40% Mineral Reinforced PA66
Description: Nilamon A3 H K8 combines good stiffness with low warpage. It is used for applications which need a degree of rigidity, particularly at higher temperatures, but which need to stay flat a..
|
|||
| Maximum Service Temperature, Air | 85.0 °C | 185 °F | Continuous; FRISETTA Test Method |
|
Nilit FRIANYL B63 K Nylon 6 for injection molding
Nylon 6 for injection molding, specially formulated for knobs.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
|
Parker Chomerics CHO-FORM 5526 EMI Shielding Material
Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material..
|
|||
| Maximum Service Temperature, Air | 85.0 °C | 185 °F | Glass |
|
Parker Chomerics Tecknit ECTC™ Windows Electrically Conductive Transparent Coating
Description: ECTC WINDOWS are custom designed optical display panels produced by depositing a very thin electrically conductive transparent coating directly onto the surface of various optical subst..
|
|||
| Maximum Service Temperature, Air | 85.0 °C | 185 °F | Continuous (GTP 50% Tensile); IEC 60216 |
|
PolyOne Bergamid™ B700 UF black Polyamide 6 (Nylon 6)
Information provided by PolyOne
|
|||
| Maximum Service Temperature, Air | 85.0 °C | 185 °F | UL-746 ABC |
|
Plaskolite West Optix® CP - 51 General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
|
|||
| Maximum Service Temperature, Air | 85.0 °C | 185 °F | Continuous; FRISETTA Test Method |
|
Nilit FRIANYL B63 EO Raw extruded nylon 6 for injection molding
Raw extruded nylon 6 for injection molding, lubricated in surface.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Maximum Service Temperature, Air | 85.0 - 93.0 °C | 185 - 199 °F | Softening Range |
|
Huntsman Araldite GT 6704 US Bisphenol A Epoxy Solid Resin
Weight per Epoxide (EEW, g/eq) 675 to 775. Max color is 1.Comments/Applications: "Type 2 1/2" epoxy resin with extremely good flow and very good powder stability.Data provided by Ciba Specialty Che..
|
|||
| Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
|
Fujipoly Industries FG-S Fine Connector
Fujipoly FG-S connectors have anisotropic conduction properties. The fine metal wires are embedded in a vertical orientation within the silicone rubber width of 0.40mm. Low resistance and high curre..
|
|||
| Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
|
LATI Latamid 6 BH PA 6, Heat Stabilized
Polyamide 6 (PA6). High fluidity. Heat stabilized. Very high fluidity.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Ter..
|
|||
| Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
|
LATI Latan 13 K/30 POM, 30% Carbon Fiber Reinforced
Polyoxymethylene (POM) based compound. Carbon fiber. Medium viscosity. Good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation ..
|
|||
| Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
|
Styrolution Luran® 388 S SAN
Description: Specialty grade with highest mechanical strength and chemical resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
|
|||
| Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
|
Styrolution Luran® S 757 G UV White 37019 ASA
Description: Particularly easy flowing injection molding grade for difficult moldings with large flow path/wall thickness ratios.Information provided by STYROLUTION, which is a joint venture between..
|
|||
| Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
|
Styrolution Novodur® HH-106 ABS
Novodur HH-106 is a high heat injection molding grade providing a balanced property profile.Information provided by Styrolution
|
|||
| Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
|
Master Bond MB297FL Cyanoacrylate Adhesive System
Vibration & shock resistant, fills gap to 0.007Information provided by Master Bond Inc.
|
|||
| Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
|
Trelleborg R350 Natural Rubber Polyisoprene
All information provided by Trelleborg
|
|||
| Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
|
Trelleborg R492 Commercial Natural Rubber Polyisoprene
All information provided by Trelleborg
|
|||
| Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
|
Trelleborg R496 Commercial Natural Rubber Polyisoprene
All information provided by Trelleborg
|
|||
| Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
|
Trelleborg R583 Commercial Natural Rubber Polyisoprene
All information provided by Trelleborg
|
|||
| Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
|
Von Roll Isola IMI E-Solder® 3026 Electrically Conductive Adhesive
Data provided by Von Roll Isola USA.E-SOLDER® epoxy based resin systems can be used at room temperature on heat sensitive materials, can bond dissimilar materials, and do not have flux or residue t..
|
|||
| Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
|
Trelleborg R698 Commercial Natural Rubber Polyisoprene
All information provided by Trelleborg
|
|||
| Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
|
Trelleborg R798 Commercial Natural Rubber Polyisoprene
All information provided by Trelleborg
|
|||
| Maximum Service Temperature, Air | 85.0 °C | 185 °F | ASTM D 3575 |
|
Eurofoam Porocell POR 445 CDN CR-Neoprene Foam
Polychloroprene foam rubber. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
|
|||
| Maximum Service Temperature, Air | 85.0 °C | 185 °F | Long Term |
|
Ensinger Tecaform™ HPV 13 Acetal Homopolymer - Extruded Products (POM)
Tecaform™ HPV 13 is a brown homopolymer acetal with an internal PTFE lubricant. Its low coefficient of friction, excellent PV values, toughness, wear resistance, and machinability make it an excep..
|
|||
| Maximum Service Temperature, Air | 85.0 °C | 185 °F | Long Term |
|
CENTROPLAST CENTROMID 6 E Polyamide 6 extruded
This tough and impact resistant material has good chemical resistance and can be bonded and welded. It is used for sealing rings, flanges, etc. Information provided by CENTROPLAST Engineering Plast..
|
|||
| Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
|
Parker Chomerics CHO-SHIELD® 2001 Conductive Coating
Electrically conductive coatings provide corrosion protection for enclosure flanges which mate with EMI shielding gaskets. They can also provide a corrosion resistant conductive surface coating on a..
|
|||
| Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
|
Abatron AboCast 10-5/AboCure 3-4 Epoxy
AboCast 10-5 is a filled, high-viscosity epoxy resin. It is blended with AboCure 3-4 to make a structural adhesive and casting compound for the optic and electric industry. AboCure 3-4 is a tan room..
|
|||
| Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
|
Abatron AboCast 10-5/AboCure 50-3 Epoxy
AboCast 10-5 is a filled, high-viscosity epoxy resin. It is blended with AboCure 50-3 to make a structural adhesive and casting compound for the optic and electric industry. AboCure 50-3 is a clear ..
|
|||
| Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
|
Quantum Acetal-Homopolymer
Information provided by Quantum Advanced Engineering Plastics
|
|||