| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 98.9 °C | 210 °F | |
|
ND Industries High Temperature SuperGlue 311
Very high viscosity with thermal cycling resistance
|
|||
| Maximum Service Temperature, Air | 98.9 °C | 210 °F | |
|
ND Industries High Temperature SuperGlue 362
Medium viscosity with thermal cycling resistance
|
|||
| Maximum Service Temperature, Air | 99.0 °C | 210 °F | |
|
Parker Chomerics CHO-BOND 584-208 Conductive Adhesive
Two-component, highly conductive adhesive system that combines the good adhesive characteristics of epoxy with the superior conductivity of silver. In addition to being available in bulk form, the m..
|
|||
| Maximum Service Temperature, Air | 99.0 °C | 210 °F | |
|
Parker Chomerics CHO-BOND 592 Conductive Epoxy
Highly conductive silver-filled epoxy adhesive which combines the best properties of metals and organics. This two-component system is unique in that it combines long pot life, good electrical condu..
|
|||
| Maximum Service Temperature, Air | 99.0 °C | 210 °F | |
|
Parker Chomerics CHO-BOND® 592 Conductive Adhesive
Description: CHO-BOND® 500 Series Adhesive/Sealant Compounds; These pure silver-filled materials are used where tight tolerances require thin bond lines. Various cure cycles are available, and the ..
|
|||
| Maximum Service Temperature, Air | 98.9 °C | 210 °F | Long Term |
|
Quadrant EPP Ertalyte® PET-P, Polyester-semi-crystalline thermoplastic, extruded (ASTM Product Data Sheet) |
|||
| Maximum Service Temperature, Air | 98.9 °C | 210 °F | Long Term |
|
Quadrant EPP Ertalyte® TX Internally Lubricated Semi-Crystalline Polyester (ASTM Product Data Sheet) |
|||
| Maximum Service Temperature, Air | 98.9 °C | 210 °F | Long Term |
|
Quadrant EPP Quadrant Nylon 101 Extruded, Unfilled, Type 66 Natural and Black (ASTM Product Data Sheet) |
|||
| Maximum Service Temperature, Air | 98.9 °C | 210 °F | |
|
Technetics Group Amicon™ PET-P
(Unverified Data**)
Information provided by Technetics Group (formerly Plastomer Technologies)
|
|||
| Maximum Service Temperature, Air | 98.9 °C | 210 °F | Continuous |
|
Quadrant EPP Semitron® CMP LL5 Polyester (ASTM Product Data Sheet)
Enhanced semi-crystalline polyester product for extended service in CMP retaining rings. Superior performance, especially in oxide processes, and cost effective relative to standard ring materials. ..
|
|||
| Maximum Service Temperature, Air | 98.9 °C | 210 °F | |
|
Technetics Group Amicon™ Nylon 6/66
(Unverified Data**)
Information provided by Technetics Group (formerly Plastomer Technologies)
|
|||
| Maximum Service Temperature, Air | 99.0 °C | 210 °F | Long Term |
|
Ensinger ENSILON® 6/6 Extruded Nylon 6/6 (PA66)
(discontinued **)
ENSILON materials have high mechanical strength and superior resistance to wear and organic chemicals.Ensilon grades have been replaced by Tecamid.Information supplied by Ensinger, Inc.
|
|||
| Maximum Service Temperature, Air | 98.9 °C | 210 °F | Continuous Use |
|
Westlake Plastics Ultra Ethylux® HDPE
Ultra Ethylux is made from high density polyethylene resin. This material is a cost effective alternative for a variety of end uses including mild chemical and wear applications. Information provid..
|
|||
| Maximum Service Temperature, Air | 98.9 °C | 210 °F | Heat Distortion, Annealed; ASTM D648 |
|
Total PSC 536 Polystyrene
Polystyrene 536 is a high melt flow; high heat crystal polystyrene. Designed for fast cycle injection molding and for high output, direct injection profile extrusion for foam applications.Informatio..
|
|||
| Maximum Service Temperature, Air | 98.9 °C | 210 °F | Short Term |
|
TriStar TriSteel AC Metal Backed PTFE Bearing System
Ultraflon 601 (AC) POM lined metal backed bearing system, boundary lubrication required, high PV. Ultraflon 601 POM Liner is a lubricant enhanced acetal material for use in lubricated or unlubricate..
|
|||
| Maximum Service Temperature, Air | 98.9 °C | 210 °F | Short Term |
|
TriStar TriSteel AT Metal Backed PTFE Bearing System
Ultraflon 601T (AT) POM bronze with PTFE, lined metal back bearing system, high PV, self lube, high speed. This liner will run with zero lubrication required. Most commonly used in clip bearings, li..
|
|||
| Maximum Service Temperature, Air | 98.9 °C | 210 °F | |
|
Loctite® 426 Toughened Ethyl Cyanoacrylate Bonding Adhesive
Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-..
|
|||
| Maximum Service Temperature, Air | 98.9 °C | 210 °F | |
|
Loctite® PRISM® 411 Clear Instant Adhesive
Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-..
|
|||
| Maximum Service Temperature, Air | 99.0 °C | 210 °F | |
|
ChevronTexaco Delo® NLGI 0 Grease EP
FeaturesChevron Delo Greases EP are technically advanced, extreme pressure greases for a wide variety of on- and off-road applications.They are formulated with ISOSYN® base stocks, a lithium comple..
|
|||
| Maximum Service Temperature, Air | 99.0 °C | 210 °F | |
|
ChevronTexaco Dura-Lith® NLGI 0 Grease EP
FeaturesChevron Dura-Lith Greases EP are multipurpose extreme pressure greases.They are manufactured using selected highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thic..
|
|||
| Maximum Service Temperature, Air | 98.9 °C | 210 °F | Continuous |
|
Cast Nylons Nycast® CP Caprolactam/Laurinlactum Copolymer Cast Nylon
Highly resilient, with higher tensile elongation and impact strength than standard grades, NYCAST® CP is used applications requiring an extra degree of toughness. A copolymer of caprolactam and lau..
|
|||
| Maximum Service Temperature, Air | 99.0 °C | 210 °F | Deflection Temp; Load not specified |
|
Fibre Glast 88 / 87 General Purpose Epoxy Resin and Hardener
(discontinued **)
Description:#88 Epoxy Resin is a 100% reactive low viscosity liquid bisphenol-A based epoxy resin diluted with Alkyl glycidyl ether. This resin is specially designed for applications requiring low v..
|
|||
| Maximum Service Temperature, Air | 98.9 °C | 210 °F | |
|
Loctite® 480 Toughened Ethyl Cyanoacrylate Bonding Adhesive
Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-..
|
|||