| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 100 °C | 212 °F | Recommended |
|
Nye Lubricants 730F (NG) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Maximum Service Temperature, Air | 100 °C | 212 °F | Maximum operating temperature continuously for 5000 hours based on a tensile stress of 50% at 23° C. (dry sample) |
|
Omnia Plastica Akulon® PA6 G.Oil - Omniamid Oil - at 50% RH
Cast Nylon 6 with the addition of 6% of special lubricating oil which remains in solution in the material. The unique method of production results in a micro distribution of oil particles with a hom..
|
|||
| Maximum Service Temperature, Air | 100 °C | 212 °F | short period, no load |
|
Omnia Plastica PE 1000 - Polyethylene 1000
Polyethylene with a molecular weight of ± 1000,000 with excellent impact strength. PE 1000 is less rigid and has a higher shock resistance than the low molecular weight polyethylene and it is there..
|
|||
| Maximum Service Temperature, Air | 100 °C | 212 °F | Deflection Temp.; ASTM D648 |
|
NCMT NanoPAC™ N10 High Performance Polypropylene Nanocomposite
Characteristics: Less shrinkage Solved distortion problem Good balance in impact and stiffness High gloss Reduce production cycleApplications: Household Industry Electrical Appliances Toys IndustryI..
|
|||
| Maximum Service Temperature, Air | 100 °C | 212 °F | |
|
Precision Polymer Engineering Q90Y Polyurethane Rubber
Peroxide cured, yellow Polyurethane Rubber, 85-95 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG910, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasio..
|
|||
| Maximum Service Temperature, Air | 100 °C | 212 °F | |
|
Precision Polymer Engineering R50D Natural Rubber
Natural Rubber, 45-55 °IRHD. Formulated to Defence Standard 93-30, Type QX, Grade 50 (NRQX50).Applications: Natural rubber offers low compression set, high tensile strength, high resilience and ex..
|
|||
| Maximum Service Temperature, Air | 100 °C | 212 °F | |
|
Parker Chomerics CHO-BOND 360-208 Conductive Epoxy
Low cost, electrically conductive epoxy adhesive that combines the good adhesive characteristics as epoxy, and the superior electrical conductivity of silver. It is recommended as a thermo-setting E..
|
|||
| Maximum Service Temperature, Air | 100 - 230 °C | 212 - 446 °F | Average value: 172 °C Grade Count:5 |
|
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl..
|
|||
| Maximum Service Temperature, Air | 100 °C | 212 °F | |
|
Lehmann & Voss LUVOCOM® 80-7353/NAT Polyacetal-copolymer, with aramid reinforcement and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
|
|||
| Maximum Service Temperature, Air | 100 °C | 212 °F | |
|
Lehmann & Voss LUVOCOM® 80-7555 Polyacetal-copolymer, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
|
|||
| Maximum Service Temperature, Air | 100 °C | 212 °F | |
|
Lehmann & Voss LUVOCOM® 80-7752 Polyacetal-copolymer, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita..
|
|||
| Maximum Service Temperature, Air | 100 °C | 212 °F | Continuous; DIN 52612 |
|
Isoflon PP Polypropylene
Products with excellent friction, anti-stick, abrasion and chemical inertia characteristicsVery good impact resistanceNo moisture regainProduct for the food industryInformation provided by Isoflon.
|
|||
| Maximum Service Temperature, Air | 100 °C | 212 °F | |
|
Lehmann & Voss LUVOCOM® 80-8030 Polyacetal-copolymer, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically ..
|
|||
| Maximum Service Temperature, Air | 100 °C | 212 °F | |
|
Trelleborg B419 Nitrile Rubber
Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi..
|
|||
| Maximum Service Temperature, Air | 100 °C | 212 °F | |
|
Tra-Con Tra-Cast 3143 Fire Retardant Epoxy Casting Compound
TRA-CAST 3143 has a low viscosity and long pot life. It is certified to the requirements of UL 94 V-O, and is recommended for rigid potting, laminating, transformer encapsulating, filament winding a..
|
|||
| Maximum Service Temperature, Air | 100 °C | 212 °F | |
|
Elastron® TPO Elastomer
wide hardness rangedoes not require vulcanization-quite higher saving on the processing costsremains flexible at low temperatureshigh temperature resistanceelectrical insulator with very low conduct..
|
|||
| Maximum Service Temperature, Air | 100 °C | 212 °F | long term; EMS |
|
EMS-Grivory Grivory® XE 4116 nat PA1010-GF55
Product description: Grilamid XE 4116 natural is a 55% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is especially suitable for the manufacturing of thin-walled, painted ..
|
|||
| Maximum Service Temperature, Air | 100 °C | 212 °F | Continuous use |
|
Hippe PA 66 Nylon 66
The polyamide with high degree of hardness, stiffness, scuff strength and stability of shape under heat. Preferred polyamide for components subjected to high load and heat stress in electrical, mec..
|
|||
| Maximum Service Temperature, Air | 100 °C | 212 °F | Continuous use |
|
Hippe PMMA
Components made of PMMA are brilliantly transparent. Outstanding aging stability and weathering resistance. Good surface hardness. Abrasion-resistant. Physiologically safe. High strength. Easi..
|
|||
| Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
|
EMS-Grivory Grivory® EB 50 H DZ PA6
Product description: Grilon EB 50 H DZ is a high viscosity, unreinforced, heat stabilized, impact modified PA6 extrusion blow molding grade. Grilon EB 50 H DZ has the following important properties:..
|
|||
| Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
|
EMS-Grivory Grivory® GV-4H PA*-GF40
Product description: Grivory GV-4H natural is a 40% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyamide...
|
|||
| Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
|
EMS-Grivory Grivory® GVX-6 H nat PA*-GF60
Product description: Grivory GVX-6H natural is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamid..
|
|||
| Maximum Service Temperature, Air | 100 °C | 212 °F | |
|
Azoty Tarnow™ TARNOFORM 300 POM
Basic, fast cycling injection molding grade suitable for many applications.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
|
|||
| Maximum Service Temperature, Air | 100 °C | 212 °F | |
|
BASF Ultraform® W2320 U035 LEV POM
Description: Is a POM, UV-stabilized, very free-flowing, rapidly solidifying grade for injection molding, with reduced emission potential.Information provided by BASF
|
|||
| Maximum Service Temperature, Air | 100 °C | 212 °F | Long Term |
|
CENTROPLAST CENTRODAL LF Polyoxymethylene conductive
This material is electrically conductive, with high mechanical strength and dimensional stability. Applications include structural components in potentially explosive areas, components for divertin..
|
|||
| Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
|
EMS-Grivory Grivory® GV-6H EF nat PA*-GF60
Product description: Grivory GV-6H EF black 9915 is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol..
|
|||
| Maximum Service Temperature, Air | 100 °C | 212 °F | ASTM D 3575 |
|
Eurofoam Porocell POR 303/B CR-Neoprene/NBR Foam
Polychloroprene and acrylonitrile butadiene foam rubber. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam..
|
|||
| Maximum Service Temperature, Air | 100 - 345 °C | 212 - 653 °F | Average value: 234 °C Grade Count:11 |
|
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and..
|
|||
| Maximum Service Temperature, Air | 100 °C | 212 °F | |
|
Lehmann & Voss PLASLUBE NY-1/SI/2/NT Polyamide 66, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Isotropic shrinkage characteristics.Information provided by Lehmann ..
|
|||