| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 160 - 220 °C | 320 - 428 °F | Average value: 193 °C Grade Count:6 |
|
Overview of materials for Polyphenylene Sulfide (PPS) Coating Resin
This property data is a summary of similar materials in the MatWeb database for the category "PPS Coating Resin". Each property range of values reported is minimum and maximum values of appropriate ..
|
|||
| Maximum Service Temperature, Air | 80.0 - 220 °C | 176 - 428 °F | Average value: 136 °C Grade Count:5 |
|
Overview of materials for Nylon 66, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu..
|
|||
| Maximum Service Temperature, Air | 200 - 220 °C | 392 - 428 °F | UL Temperature Rating |
|
Solvay Specialty Polymers Ryton® R-4 Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4 and R-4-02 40% glass fiber reinforced polyphenylene sulfide compounds provide a good combination of mechanical and electrical properties with outstanding chemical resistance, even at e..
|
|||
| Maximum Service Temperature, Air | 200 - 220 °C | 392 - 428 °F | UL Temperature Rating |
|
Solvay Specialty Polymers Ryton® R-4-02 Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4 and R-4-02 40% glass fiber reinforced polyphenylene sulfide compounds provide a good combination of mechanical and electrical properties with outstanding chemical resistance, even at e..
|
|||
| Maximum Service Temperature, Air | 200 - 220 °C | 392 - 428 °F | UL Temperature Rating |
|
Solvay Specialty Polymers Ryton® R-4-02XT Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4XT and R-4-02XT 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength with good electrical properties and outstanding chemical resistance, even..
|
|||
| Maximum Service Temperature, Air | 200 - 220 °C | 392 - 428 °F | UL Temperature Rating |
|
Solvay Specialty Polymers Ryton® R-4-200BL Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-200NA and R-4-200BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and low maintenance molding using conventional molding equipmentFeat..
|
|||
| Maximum Service Temperature, Air | 200 - 220 °C | 392 - 428 °F | UL Temperature Rating |
|
Solvay Specialty Polymers Ryton® R-4-200NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-200NA and R-4-200BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and low maintenance molding using conventional molding equipmentFeat..
|
|||
| Maximum Service Temperature, Air | 200 - 220 °C | 392 - 428 °F | UL Temperature Rating |
|
Solvay Specialty Polymers Ryton® R-4-220BL Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-220NA and R-4-220BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength after constant or repeated exposure to high temperature water.Featur..
|
|||
| Maximum Service Temperature, Air | 200 - 220 °C | 392 - 428 °F | UL Temperature Rating |
|
Solvay Specialty Polymers Ryton® R-4-230BL Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-230NA and R-4-230BL 40% glass fiber reinforced polyphenylene sulfide compounds provide reduced flash and improved processability compared to other polyphenylene sulfide injection moldi..
|
|||
| Maximum Service Temperature, Air | 200 - 220 °C | 392 - 428 °F | UL Temperature Rating |
|
Solvay Specialty Polymers Ryton® R-4-230NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-230NA and R-4-230BL 40% glass fiber reinforced polyphenylene sulfide compounds provide reduced flash and improved processability compared to other polyphenylene sulfide injection moldi..
|
|||
| Maximum Service Temperature, Air | 200 - 220 °C | 392 - 428 °F | UL Temperature Rating |
|
Solvay Specialty Polymers Ryton® R-4-232NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-232NA 40% glass fiber reinforced polyphenylene sulfide compound complies with United States Food and Drug Administration (FDA) and European Union (EU 10/2011 and 1183/2012) regulations..
|
|||
| Maximum Service Temperature, Air | 200 - 220 °C | 392 - 428 °F | UL Temperature Rating |
|
Solvay Specialty Polymers Ryton® R-4-240BL Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-240NA and R-4-240BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and toughness compared to other polyphenylene sulfide compounds.Feat..
|
|||
| Maximum Service Temperature, Air | 200 - 220 °C | 392 - 428 °F | UL Temperature Rating |
|
Solvay Specialty Polymers Ryton® R-4-240NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-240NA and R-4-240BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and toughness compared to other polyphenylene sulfide compounds.Feat..
|
|||
| Maximum Service Temperature, Air | 200 - 220 °C | 392 - 428 °F | UL Temperature Rating |
|
Solvay Specialty Polymers Ryton® R-4XT Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4XT and R-4-02XT 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength with good electrical properties and outstanding chemical resistance, even..
|
|||
| Maximum Service Temperature, Air | 160 - 220 °C | 320 - 428 °F | |
|
Sichuan Deyang Haton® hp12370 Polyphenylene Sulfide Coating
Powder; anti-corrosionInformation provided by Sichuan Deyang Chemical Co., LTD
|
|||
| Maximum Service Temperature, Air | 160 - 220 °C | 320 - 428 °F | |
|
Sichuan Deyang Haton® hp23310 Polyphenylene Sulfide Coating
Powder; anti-corrosion, wear resistantInformation provided by Sichuan Deyang Chemical Co., LTD
|
|||
| Maximum Service Temperature, Air | 160 - 220 °C | 320 - 428 °F | |
|
Sichuan Deyang Haton® hs12370 Polyphenylene Sulfide Coating
Suspension; anti-corrosionInformation provided by Sichuan Deyang Chemical Co., LTD
|
|||
| Maximum Service Temperature, Air | 180 - 220 °C | 356 - 428 °F | |
|
Sichuan Deyang Haton® hs1237B Polyphenylene Sulfide Coating
Suspension; anti-corrosionInformation provided by Sichuan Deyang Chemical Co., LTD
|
|||
| Maximum Service Temperature, Air | 160 - 220 °C | 320 - 428 °F | |
|
Sichuan Deyang Haton® hs23310 Polyphenylene Sulfide Coating
Suspension; anti-corrosion, wear resistantInformation provided by Sichuan Deyang Chemical Co., LTD
|
|||
| Maximum Service Temperature, Air | 180 - 220 °C | 356 - 428 °F | |
|
Sichuan Deyang Haton® hs2331B Polyphenylene Sulfide Coating
Suspension; anti-corrosion, wear resistantInformation provided by Sichuan Deyang Chemical Co., LTD
|
|||
| Maximum Service Temperature, Air | 200 - 220 °C | 392 - 428 °F | UL Temperature Rating |
|
Solvay Specialty Polymers Ryton® R-4-220NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-220NA and R-4-220BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength after constant or repeated exposure to high temperature water.Featur..
|
|||
| Maximum Service Temperature, Air | 80.0 - 220 °C | 176 - 428 °F | Average value: 149 °C Grade Count:5 |
|
Overview of materials for Nylon 66/6, Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, Mineral Reinforced". Each property range of values reported is minimum and maximum values of..
|
|||
| Maximum Service Temperature, Air | 80.0 - 220 °C | 176 - 428 °F | Average value: 140 °C Grade Count:3 |
|
Overview of materials for Nylon 66, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu..
|
|||
| Maximum Service Temperature, Air | 180 - 220 °C | 356 - 428 °F | Average value: 199 °C Grade Count:4 |
|
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m..
|
|||
| Maximum Service Temperature, Air | 185 - 220 °C | 365 - 428 °F | Average value: 203 °C Grade Count:3 |
|
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% ..
|
|||