| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 105 °C | 221 °F | Maximum operating temperature continuously for 5000 hours based on a tensile stress of 50% at 23° C. (dry sample) |
|
Omnia Plastica Rilsan® PA6 GF - Akulon GF - at 50% RH
Polyamide 6 reinforced with the addition of 30% glass fibre and graphite. The glass charge makes the material highly resistant to abrasion, compression and flexing. Akulon GF is particularly suitabl..
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | Cured State |
|
Palm Labs Adhesives TURBO FUSE SERIES 190-HT (4000 cp HIGH TEMPERATURE) Rapid Bonding Adhesive
Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 190-HT advanced formula is designed to polymerize instantly by absorbing surface moisture and is recommended for..
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous; FRISETTA Test Method |
|
Nilit FRIANYL A63 HS-GV10 Nylon 6.6 for injection molding, 10% glass fiber reinforced
Nylon 6.6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous; FRISETTA Test Method |
|
Nilit FRIANYL B63 CV10 Nylon 6.6 for injection molding, 10% carbon fiber reinforced
Nylon 6.6 for injection molding, good conductive and electrostatic properties.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous; FRISETTA Test Method |
|
Nilit FRIANYL B63 SG40 Nylon 6 for injection molding, 40% mineral filled
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous; 5,000 h |
|
Quadrant EPP Ertalon® 6 PLA PA 6, cast (ISO Data)
Unmodified cast nylon 6 grade exhibiting characteristics which come very close to those of Ertalon 66 SA. It combines high strength, stiffness and hardness with good creep and wear resistance, heat ..
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous; FRISETTA Test Method |
|
Nilit FRIANYL B63 GV15 Nylon 6 for injection molding, 15% glass fiber reinforced
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Maximum Service Temperature, Air | 105 - 130 °C | 221 - 266 °F | Average value: 124 °C Grade Count:5 |
|
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in..
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | |
|
Manifattura Cattaneo PA 6 G Nylon
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | UL temperature rating; UL 1581 |
|
SABIC Innovative Plastics NORYL WCA871A PPE
Flame retardant performance and mechanical properties capable of meeting UL VW-1 requirement and 105C temperature rating as defined UL1581. UL1581 tests conducted on 1.0mmD wire with AWG28 conductor..
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous Use; ASTM D794 |
|
Teknor Apex APEX® 77-W115-B Polyvinyl Chloride, Flexible
Notes: 105°C General Purpose; RoHS Compliant Uses: Connects; Grommets; Plugs; Strain ReliefsForms: Pellets Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molded Components Additional Information: T..
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous Use; ASTM D794 |
|
Teknor Apex APEX® 84459 Polyvinyl Chloride, Flexible
Notes: 105°C Insulation; RoHS Compliant Features: Flame Retardant; Low to no Migration; Oil ResistantUses: Insulation Agency Ratings: UL 1063; UL 62; UL 1581 Forms: Pellets Wire Types: AWMInforma..
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous Use; ASTM D794 |
|
Teknor Apex APEX® 84842-B Polyvinyl Chloride, Flexible
Notes: 105°C Jacket; RoHS Compliant Features: High Heat Resistance; Sunlight Resistant (720 hours) Uses: Wire and Cable Applications; Wire JacketingAgency Ratings: UL 62; UL QMTT2 .E73402 Forms: ..
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous Use; ASTM D794 |
|
Teknor Apex APEX® 01-A0383A-85 Polyvinyl Chloride, Flexible
Notes: 105°C Insulation; RoHS Compliant Uses: Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous; ASTM D794 |
|
Teknor Apex APEX® 02-A0033A-65 NT1 Polyvinyl Chloride, Flexible
Notes: RoHS Compliant Forms: PelletsInformation Provided by Teknor Apex
|
|||
| Maximum Service Temperature, Air | <= 105 °C | <= 221 °F | |
|
Sylvin Technologies 5042N PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.
|
|||
| Maximum Service Temperature, Air | <= 105 °C | <= 221 °F | |
|
Sylvin Technologies 6140-90 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous Use |
|
Teknor Apex Telcar® TL-8451 Thermoplastic Elastomer
Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou..
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous Use |
|
Teknor Apex Telcar® TL-8732R Thermoplastic Elastomer
Notes: RoHS Compliant Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstri..
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous use |
|
Polyram PlusTek PD1002NT Nylon 12 for Extrusion
Medium viscosity Nylon 12 for extrusion application.Information provided by Polyram.
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | |
|
Cytec (Conap) RN-1000 / EA-028 Conapoxy® Resin / Conacure® Hardener
Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an..
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | 20000 h; VDE 0304/P2-1, IEC 216 |
|
EPICHEM Epinyl PA 6 GF 30 Polyamide 6, 30% Glass
Characteristics: medium viscosity, 30% glass fibre, excellent mechanical properties
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | |
|
Colorite Polymers CS1533UL Wire and Cable Jacket Vinyl Compound
Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai..
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | |
|
Colorite Polymers Weatherflex™ CS1522WX (NTL01B) Wire and Cable Vinyl Compound
Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai..
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | Service |
|
3M 8087 Construction Seaming Tape
3M™ Construction Seaming Tape 8087 is designed to seal seams on housewrap and insulated sheathing products. It can also be used to seam polyethylene vapor barrier products as well as to repair hole..
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | Service |
|
3M FM041909 White Polyester Label Products
3M™ White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ Adhesive P1480, which ..
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous Use; ASTM D794 |
|
Teknor Apex APEX® 7500-85 Polyvinyl Chloride, Flexible
Notes: 105°C General Purpose; RoHS Compliant Features: High Heat Resistance Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL Q..
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous Use; ASTM D794 |
|
Teknor Apex APEX® 80851-B Polyvinyl Chloride, Flexible
Notes: 105°C Insulation; RoHS Compliant Forms: Pellets Uses: Wire and Cable Applications Wire Types: THW; TW; THHN; THWN Agency Ratings: UL QMTT2 .E73402Information Provided by Teknor Apex
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous Use; ASTM D794 |
|
Teknor Apex APEX® 832-NL Polyvinyl Chloride, Flexible
Notes: 105°C Jacket; RoHS Compliant Uses: Wire and Cable ApplicationsForms: PelletsInformation Provided by Teknor Apex
|
|||
| Maximum Service Temperature, Air | 105 °C | 221 °F | |
|
3M Scotch® Super 33+™ Vinyl Electrical Tape
Scotch® Super 33+™ Vinyl Electrical Tape is a premium grade, 7 mil thick, all-weather vinyl-insulating tape. It is designed to perform continuously in ambient temperatures up to 105°C. The tape i..
|
|||