Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Maximum Service Temperature, Air = 221 °F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 95.0 - 105 °C
203 - 221 °F
Softening Range
Huntsman Araldite GT 6084 Bisphenol A Epoxy Solid Resin
Weight per Epoxide (EEW, g/eq) 875 to 1025. Max color is 1.Comments/Applications: Unmodified bis A "Type 4" epoxy. Specifically designed for esterification reactions to produce epoxy esters for hi..
Maximum Service Temperature, Air 95.0 - 105 °C
203 - 221 °F
Softening Range
Huntsman Araldite GT 9545 Bisphenol A Epoxy Solid Resin
Weight per Epoxide (EEW, g/eq) 875 to 1025. Max color is 1.Comments/Applications: Unmodified bis A "Type 4" epoxy resin. Powder coating version of GT 6084; moderate flow.Data provided by Ciba Spec..
Maximum Service Temperature, Air 95.0 - 105 °C
203 - 221 °F
Softening point
Mitsui MILEXâ„¢ RN-2830MB Acrylic Rubber Modified Phenolic Resin
The MILEXâ„¢ Family of products is widely featured in brake systems of automobiles made by automakers through Mitsui Chemicals'. The phenolic material is primarily used as binders in brake pad..
Maximum Service Temperature, Air 95.0 - 105 °C
203 - 221 °F
Softening point
Mitsui MILEXâ„¢ RN-2830MR Acrylic Rubber Modified Phenolic Resin
The MILEXâ„¢ Family of products is widely featured in brake systems of automobiles made by automakers through Mitsui Chemicals'. The phenolic material is primarily used as binders in brake pad..
Maximum Service Temperature, Air 80.0 - 105 °C
176 - 221 °F
Softening point
Mitsui MILEXâ„¢ XL-225MB Phenol Aralkyl Resin, Standard Grade
The MILEXâ„¢ Family of products is widely featured in brake systems of automobiles made by automakers through Mitsui Chemicals'. The phenolic material is primarily used as binders in brake pad..
Maximum Service Temperature, Air 80.0 - 105 °C
176 - 221 °F
Sylvin Technologies 7056 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.
Maximum Service Temperature, Air 90.0 - 105 °C
194 - 221 °F
Sylvin Technologies 50423 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.
Maximum Service Temperature, Air 90.0 - 105 °C
194 - 221 °F
Sylvin Technologies 5108 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.
Maximum Service Temperature, Air 90.0 - 105 °C
194 - 221 °F
Sylvin Technologies 574 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.
Maximum Service Temperature, Air 90.0 - 105 °C
194 - 221 °F
Sylvin Technologies 578 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.
Maximum Service Temperature, Air 90.0 - 105 °C
194 - 221 °F
Sylvin Technologies 5120 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.
Maximum Service Temperature, Air 90.0 - 105 °C
194 - 221 °F
Sylvin Technologies 6134-80 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.
Maximum Service Temperature, Air 90.0 - 105 °C
194 - 221 °F
Softening point
Mitsui MILEX™ XL-1210MB Phenol Aralkyl Resin, Silicone Rubber Modified  (discontinued **)
The MILEX™ Family of products is widely featured in brake systems of automobiles made by the top automakers through Mitsui Chemicals' affiliation with leading brake manufacturers. The phenolic ..
Copyright © lookpolymers.com All Rights Reserved